JPS6345322A - ホ−ロ−用鋼板の製造方法 - Google Patents
ホ−ロ−用鋼板の製造方法Info
- Publication number
- JPS6345322A JPS6345322A JP18614386A JP18614386A JPS6345322A JP S6345322 A JPS6345322 A JP S6345322A JP 18614386 A JP18614386 A JP 18614386A JP 18614386 A JP18614386 A JP 18614386A JP S6345322 A JPS6345322 A JP S6345322A
- Authority
- JP
- Japan
- Prior art keywords
- enamel
- content
- steel
- cold
- less
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Heat Treatment Of Steel (AREA)
- Heat Treatment Of Sheet Steel (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP18614386A JPS6345322A (ja) | 1986-08-09 | 1986-08-09 | ホ−ロ−用鋼板の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP18614386A JPS6345322A (ja) | 1986-08-09 | 1986-08-09 | ホ−ロ−用鋼板の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6345322A true JPS6345322A (ja) | 1988-02-26 |
JPH0559969B2 JPH0559969B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1993-09-01 |
Family
ID=16183131
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP18614386A Granted JPS6345322A (ja) | 1986-08-09 | 1986-08-09 | ホ−ロ−用鋼板の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6345322A (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) |
Cited By (9)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0230738A (ja) * | 1988-07-20 | 1990-02-01 | Kawasaki Steel Corp | 耐泡・黒点欠陥に優れた直接一回掛けほうろう用鋼板 |
JPH0293047A (ja) * | 1988-09-28 | 1990-04-03 | Sumitomo Metal Ind Ltd | ほうろう用鋼板およびその製造方法 |
JPH02104640A (ja) * | 1988-10-12 | 1990-04-17 | Kawasaki Steel Corp | プレス成形性と耐泡・黒点欠陥に優れた直接一回掛けほうろう用鋼板 |
JPH02133543A (ja) * | 1988-07-29 | 1990-05-22 | Nkk Corp | 耐泡性の優れたホーロー用冷延鋼板およびその製造方法 |
JPH0413849A (ja) * | 1990-05-02 | 1992-01-17 | Sumitomo Metal Ind Ltd | ほうろう用冷延鋼板およびその製造法 |
JPH0559444A (ja) * | 1991-06-18 | 1993-03-09 | Sumitomo Metal Ind Ltd | ほうろう用冷延鋼板の製造方法 |
WO1995011320A1 (fr) * | 1993-10-18 | 1995-04-27 | Nippon Steel Corporation | Tole d'acier laminee a froid d'une excellente aptitude au façonnage, et son procede de production |
KR100347570B1 (ko) * | 1997-08-29 | 2002-09-18 | 주식회사 포스코 | 성형성 및 표면품질이 우수한 법랑용 강판의제조방법 |
JP4747843B2 (ja) * | 2003-10-21 | 2011-08-17 | セイコーエプソン株式会社 | 逆止弁、逆止弁を備えるポンプ |
-
1986
- 1986-08-09 JP JP18614386A patent/JPS6345322A/ja active Granted
Cited By (13)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0230738A (ja) * | 1988-07-20 | 1990-02-01 | Kawasaki Steel Corp | 耐泡・黒点欠陥に優れた直接一回掛けほうろう用鋼板 |
JPH02133543A (ja) * | 1988-07-29 | 1990-05-22 | Nkk Corp | 耐泡性の優れたホーロー用冷延鋼板およびその製造方法 |
JPH0293047A (ja) * | 1988-09-28 | 1990-04-03 | Sumitomo Metal Ind Ltd | ほうろう用鋼板およびその製造方法 |
JPH02104640A (ja) * | 1988-10-12 | 1990-04-17 | Kawasaki Steel Corp | プレス成形性と耐泡・黒点欠陥に優れた直接一回掛けほうろう用鋼板 |
JPH0413849A (ja) * | 1990-05-02 | 1992-01-17 | Sumitomo Metal Ind Ltd | ほうろう用冷延鋼板およびその製造法 |
JPH0559444A (ja) * | 1991-06-18 | 1993-03-09 | Sumitomo Metal Ind Ltd | ほうろう用冷延鋼板の製造方法 |
WO1995011320A1 (fr) * | 1993-10-18 | 1995-04-27 | Nippon Steel Corporation | Tole d'acier laminee a froid d'une excellente aptitude au façonnage, et son procede de production |
GB2289057A (en) * | 1993-10-18 | 1995-11-08 | Nippon Steel Corp | Cold-rolled steel sheet having excellent workability and process for producing the same |
US5558726A (en) * | 1993-10-18 | 1996-09-24 | Nippon Steel Corporation | Cold rolled steel having excellent machinability and production thereof |
GB2289057B (en) * | 1993-10-18 | 1997-04-09 | Nippon Steel Corp | Cold rolled steel sheet having excellent machinability and production method thereof. |
CN1040776C (zh) * | 1993-10-18 | 1998-11-18 | 新日本制铁株式会社 | 加工性优良的冷轧钢板及其生产方法 |
KR100347570B1 (ko) * | 1997-08-29 | 2002-09-18 | 주식회사 포스코 | 성형성 및 표면품질이 우수한 법랑용 강판의제조방법 |
JP4747843B2 (ja) * | 2003-10-21 | 2011-08-17 | セイコーエプソン株式会社 | 逆止弁、逆止弁を備えるポンプ |
Also Published As
Publication number | Publication date |
---|---|
JPH0559969B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1993-09-01 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US3239390A (en) | Method of producing non-ageing special low carbon iron sheets | |
CN107058881B (zh) | 适于彩涂的低成本冷轧镀锌钢带及其制备方法 | |
CN1045813A (zh) | 搪瓷用钢板及其制造方法 | |
JPS6345322A (ja) | ホ−ロ−用鋼板の製造方法 | |
JPS6043431A (ja) | 連続焼鈍による耐フル−チイング性のすぐれた軟質表面処理用鋼板の製造法 | |
JPH02285057A (ja) | 溶融亜鉛めっき用鋼板の連続焼鈍方法 | |
JPS5818973B2 (ja) | プレス成形性の優れた高張力冷延鋼板の製造方法 | |
JP2550552B2 (ja) | 耐爪とび性の優れたホ−ロ−用冷延鋼板の製造方法 | |
GB2066290A (en) | Processes for producing high strength cold rolled steel sheets | |
JPS63420A (ja) | 一回掛けホ−ロ−用鋼板の製造方法 | |
JPS6046167B2 (ja) | 連続焼鈍による非時効性で塗装焼付硬化能の優れた深紋り用高強度冷延鋼板の製造方法 | |
JPH03191047A (ja) | プレス成形性に優れた合金化溶融Znめっき鋼板の製造方法 | |
JPH0459984B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
JPS5913030A (ja) | 深絞り性の優れたAlキルド冷延鋼板の製造法 | |
JP2003096542A (ja) | ほうろう用鋼板とその製造方法 | |
JPH01180916A (ja) | 密着性および耐泡性の優れたほうろう用鋼板の製造方法 | |
JPH05202420A (ja) | ほうろう用冷延鋼板の製造方法 | |
JPH0653914B2 (ja) | ほうろう用鋼板及びその製造方法 | |
JPH0633187A (ja) | ほうろう焼成後高強度化するほうろう用冷延鋼板およびその製造方法 | |
JPS5989723A (ja) | 連続鋳造−直接熱延による加工用薄鋼板の製造方法 | |
JPH0543983A (ja) | 深絞り性、耐時効性の良好なほうろう用鋼板およびその製造方法 | |
CN117960829A (zh) | Al-Si镀层钢板的制备方法、热冲压构件及其制备方法 | |
JP2517500B2 (ja) | 耐泡、耐黒点性の優れた直接1回掛ほうろう用冷延鋼板の製造方法 | |
JP2002194493A (ja) | ほうろう用鋼板、その製造方法、ほうろう製品、およびその製造方法 | |
JPH0830244B2 (ja) | ホ−ロ−用鋼板及びその製造方法 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
EXPY | Cancellation because of completion of term |