JPS63122787A - タ−ルピツチの精製法 - Google Patents
タ−ルピツチの精製法Info
- Publication number
- JPS63122787A JPS63122787A JP26862886A JP26862886A JPS63122787A JP S63122787 A JPS63122787 A JP S63122787A JP 26862886 A JP26862886 A JP 26862886A JP 26862886 A JP26862886 A JP 26862886A JP S63122787 A JPS63122787 A JP S63122787A
- Authority
- JP
- Japan
- Prior art keywords
- pitch
- solvent
- coal tar
- tar pitch
- content
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Working-Up Tar And Pitch (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP26862886A JPS63122787A (ja) | 1986-11-13 | 1986-11-13 | タ−ルピツチの精製法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP26862886A JPS63122787A (ja) | 1986-11-13 | 1986-11-13 | タ−ルピツチの精製法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS63122787A true JPS63122787A (ja) | 1988-05-26 |
JPH0430999B2 JPH0430999B2 (enrdf_load_stackoverflow) | 1992-05-25 |
Family
ID=17461188
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP26862886A Granted JPS63122787A (ja) | 1986-11-13 | 1986-11-13 | タ−ルピツチの精製法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS63122787A (enrdf_load_stackoverflow) |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US11434429B2 (en) * | 2019-03-18 | 2022-09-06 | Terrapower, Llc | Mesophase pitch for carbon fiber production using supercritical carbon dioxide |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS60170694A (ja) * | 1984-02-16 | 1985-09-04 | Kawasaki Steel Corp | 炭素繊維プリカ−サ−ピツチの製造方法 |
-
1986
- 1986-11-13 JP JP26862886A patent/JPS63122787A/ja active Granted
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS60170694A (ja) * | 1984-02-16 | 1985-09-04 | Kawasaki Steel Corp | 炭素繊維プリカ−サ−ピツチの製造方法 |
Also Published As
Publication number | Publication date |
---|---|
JPH0430999B2 (enrdf_load_stackoverflow) | 1992-05-25 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
TWI555834B (zh) | Preparation of mesophase pitch by high temperature coal tar hydrogenation | |
US5091072A (en) | Process for preparing pitches | |
US4789456A (en) | Process for preparing mesophase pitches | |
KR101423511B1 (ko) | 타르 또는 핏치의 불순물 정제 방법 및 장치 | |
US4820401A (en) | Process for the preparation of mesophase pitches | |
US4925547A (en) | Process for producing pitch for the manufacture of high-performance carbon fibers together with pitch for the manufacture of general-purpose carbon fibers | |
US4581124A (en) | Process for thermally cracking heavy hydrocarbon oil | |
CN86102643A (zh) | 重质渣油的处理过程 | |
US4663022A (en) | Process for the production of carbonaceous pitch | |
US5182011A (en) | Process for preparing pitches | |
JPS6149355B2 (enrdf_load_stackoverflow) | ||
JPS61197688A (ja) | 石炭系重質物の精製方法 | |
JPS63122787A (ja) | タ−ルピツチの精製法 | |
JP3051155B2 (ja) | メソフェーズピッチの単離方法 | |
JPH0458519B2 (enrdf_load_stackoverflow) | ||
JPS60106882A (ja) | 重質瀝青物の精製方法 | |
CN109370631B (zh) | 一种最大化利用煤焦油生产煤系针状焦的生产方法 | |
CN118360070A (zh) | 制备煤系针状焦原料和煤系针状焦的系统和方法 | |
CN109370630B (zh) | 一种制备煤系针状焦原料的方法 | |
JPS6049084A (ja) | ニードルコークスの製造方法 | |
JPS6051782A (ja) | ベ−タレジン量を調整したqiレスピッチの製造方法 | |
JPS5910717B2 (ja) | 高級炭素材原料用重質油の製造法 | |
JPH0430998B2 (enrdf_load_stackoverflow) | ||
JPH0699692B2 (ja) | カツトタ−ルの処理方法 | |
JPH0452315B2 (enrdf_load_stackoverflow) |