JPS6293910A - 磁性流体の製造方法 - Google Patents
磁性流体の製造方法Info
- Publication number
- JPS6293910A JPS6293910A JP23346685A JP23346685A JPS6293910A JP S6293910 A JPS6293910 A JP S6293910A JP 23346685 A JP23346685 A JP 23346685A JP 23346685 A JP23346685 A JP 23346685A JP S6293910 A JPS6293910 A JP S6293910A
- Authority
- JP
- Japan
- Prior art keywords
- magnetic fluid
- magnetic
- liquid
- metal
- fine particles
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01F—MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H01F1/00—Magnets or magnetic bodies characterised by the magnetic materials therefor; Selection of materials for their magnetic properties
- H01F1/44—Magnets or magnetic bodies characterised by the magnetic materials therefor; Selection of materials for their magnetic properties of magnetic liquids, e.g. ferrofluids
- H01F1/442—Magnets or magnetic bodies characterised by the magnetic materials therefor; Selection of materials for their magnetic properties of magnetic liquids, e.g. ferrofluids the magnetic component being a metal or alloy, e.g. Fe
Landscapes
- Engineering & Computer Science (AREA)
- Power Engineering (AREA)
- Soft Magnetic Materials (AREA)
- Lubricants (AREA)
- Manufacture Of Metal Powder And Suspensions Thereof (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP23346685A JPS6293910A (ja) | 1985-10-21 | 1985-10-21 | 磁性流体の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP23346685A JPS6293910A (ja) | 1985-10-21 | 1985-10-21 | 磁性流体の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6293910A true JPS6293910A (ja) | 1987-04-30 |
| JPH0433122B2 JPH0433122B2 (enExample) | 1992-06-02 |
Family
ID=16955471
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP23346685A Granted JPS6293910A (ja) | 1985-10-21 | 1985-10-21 | 磁性流体の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6293910A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO1997032321A1 (de) * | 1996-02-27 | 1997-09-04 | Haehndel Thomas | Magnetofluid mit hoher sättigungsmagnetisierung |
| JP2009024246A (ja) * | 2007-07-23 | 2009-02-05 | Toyota Motor Corp | 金属ナノ粒子の製造方法 |
-
1985
- 1985-10-21 JP JP23346685A patent/JPS6293910A/ja active Granted
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO1997032321A1 (de) * | 1996-02-27 | 1997-09-04 | Haehndel Thomas | Magnetofluid mit hoher sättigungsmagnetisierung |
| JP2009024246A (ja) * | 2007-07-23 | 2009-02-05 | Toyota Motor Corp | 金属ナノ粒子の製造方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0433122B2 (enExample) | 1992-06-02 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Wojciechowski et al. | Iron nitride thin films: Growth, structure, and properties | |
| JP3463091B2 (ja) | カーボンナノチューブの製造方法 | |
| US4599184A (en) | Process for producing ferromagnetic liquid | |
| JPS6293910A (ja) | 磁性流体の製造方法 | |
| CN101345108B (zh) | 全致密纳米复合稀土永磁材料的制备方法 | |
| JPS6136200A (ja) | ダイヤモンドの気相合成法 | |
| JPS6320032A (ja) | 被膜を有する超微粒子の製造法 | |
| JPS6116793B2 (enExample) | ||
| JPS62232101A (ja) | 窒化鉄磁性体の製造方法 | |
| Nakatani et al. | Iron-nitride magnetic fluids prepared by plasma CVD technique and their magnetic properties | |
| JPS6211207A (ja) | 金属磁性流体 | |
| JPS6293911A (ja) | 磁性流体の製造装置 | |
| JP2008214743A (ja) | プラズマジェットを用いた金属ナノ粒子の合成及び表面処理 | |
| JPS63181305A (ja) | 酸化鉄垂直磁化薄膜の製造方法 | |
| Hoang Nam et al. | Magnetic properties of FePt nanoparticles prepared by sonoelectrodeposition | |
| Heng et al. | Plasma‐Assisted Material Preparation Strategies and Property Optimization | |
| CN104319053B (zh) | 大气压介质阻挡放电制备氮化铁磁性液体的装置与方法 | |
| JP3276390B2 (ja) | 窒化鉄粒子とその製造方法 | |
| JPS61112306A (ja) | 磁性流体の新磁性流体への転換改善方法 | |
| Jervis et al. | Formation of stable nanoscale iron carbide particles by laser breakdown chemical vapor deposition | |
| JPH06228739A (ja) | 大気圧プラズマによる粉体の表面処理方法とその装置 | |
| JP3255958B2 (ja) | 磁性流体乃至磁性粒子製造装置 | |
| JPH0410376B2 (enExample) | ||
| JPH0445503A (ja) | 磁性流体及びその製造方法 | |
| JPH07242404A (ja) | 窒化鉄磁性体の製造方法及び製造装置 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| EXPY | Cancellation because of completion of term |