JPS62167822A - 鉄損の極めて低い一方向性珪素鋼板の製造方法 - Google Patents

鉄損の極めて低い一方向性珪素鋼板の製造方法

Info

Publication number
JPS62167822A
JPS62167822A JP20269186A JP20269186A JPS62167822A JP S62167822 A JPS62167822 A JP S62167822A JP 20269186 A JP20269186 A JP 20269186A JP 20269186 A JP20269186 A JP 20269186A JP S62167822 A JPS62167822 A JP S62167822A
Authority
JP
Japan
Prior art keywords
product
annealing
steel sheet
thickness
iron loss
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP20269186A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0258326B2 (enrdf_load_stackoverflow
Inventor
Hiroshi Shimizu
洋 清水
Hiroshi Shishido
宍戸 浩
Isao Ito
伊藤 庸
Hiroshi Shimanaka
嶋中 浩
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JFE Steel Corp
Original Assignee
Kawasaki Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kawasaki Steel Corp filed Critical Kawasaki Steel Corp
Priority to JP20269186A priority Critical patent/JPS62167822A/ja
Publication of JPS62167822A publication Critical patent/JPS62167822A/ja
Publication of JPH0258326B2 publication Critical patent/JPH0258326B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Manufacturing Of Steel Electrode Plates (AREA)
  • Chemical Treatment Of Metals (AREA)
JP20269186A 1986-08-30 1986-08-30 鉄損の極めて低い一方向性珪素鋼板の製造方法 Granted JPS62167822A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP20269186A JPS62167822A (ja) 1986-08-30 1986-08-30 鉄損の極めて低い一方向性珪素鋼板の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP20269186A JPS62167822A (ja) 1986-08-30 1986-08-30 鉄損の極めて低い一方向性珪素鋼板の製造方法

Related Parent Applications (1)

Application Number Title Priority Date Filing Date
JP55116927A Division JPS5920745B2 (ja) 1980-08-27 1980-08-27 鉄損の極めて低い一方向性珪素鋼板とその製造方法

Publications (2)

Publication Number Publication Date
JPS62167822A true JPS62167822A (ja) 1987-07-24
JPH0258326B2 JPH0258326B2 (enrdf_load_stackoverflow) 1990-12-07

Family

ID=16461556

Family Applications (1)

Application Number Title Priority Date Filing Date
JP20269186A Granted JPS62167822A (ja) 1986-08-30 1986-08-30 鉄損の極めて低い一方向性珪素鋼板の製造方法

Country Status (1)

Country Link
JP (1) JPS62167822A (enrdf_load_stackoverflow)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US5306353A (en) * 1990-04-13 1994-04-26 Kawasaki Steel Corporation Method of producing grain oriented silicon steel sheets having less iron loss
US6020036A (en) * 1996-08-19 2000-02-01 Citizen Watch Co., Ltd. Method of forming hard carbon film over the inner surface of guide bush
JP2012031519A (ja) * 2010-06-30 2012-02-16 Jfe Steel Corp 方向性電磁鋼板およびその製造方法

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US5306353A (en) * 1990-04-13 1994-04-26 Kawasaki Steel Corporation Method of producing grain oriented silicon steel sheets having less iron loss
US6020036A (en) * 1996-08-19 2000-02-01 Citizen Watch Co., Ltd. Method of forming hard carbon film over the inner surface of guide bush
JP2012031519A (ja) * 2010-06-30 2012-02-16 Jfe Steel Corp 方向性電磁鋼板およびその製造方法

Also Published As

Publication number Publication date
JPH0258326B2 (enrdf_load_stackoverflow) 1990-12-07

Similar Documents

Publication Publication Date Title
US6562473B1 (en) Electrical steel sheet suitable for compact iron core and manufacturing method therefor
JPS5920745B2 (ja) 鉄損の極めて低い一方向性珪素鋼板とその製造方法
JPS61117215A (ja) 鉄損の少ない一方向性電磁鋼板の製造方法
JPS60145382A (ja) 磁気特性、皮膜特性とも優れた方向性電磁鋼板の製造方法
JP2001158950A (ja) 小型電気機器用電磁鋼板およびその製造方法
KR940008933B1 (ko) 자기 특성이 뛰어나고 또한 표면외관이 좋은 무방향성 전자(電磁) 강판의 제조방법
JP2003171718A (ja) 圧延面内での平均磁気特性に優れた電磁鋼板の製造方法
JPS5835245B2 (ja) 磁束密度の高い一方向性珪素鋼板の製造方法
JPH0277524A (ja) 鉄損の優れた薄手高磁束密度一方向性電磁鋼板の製造方法
JPS58217630A (ja) 鉄損の優れた薄手高磁束密度一方向性電磁鋼板の製造方法
JPH02298219A (ja) 鉄損の優れた薄手高磁束密度一方向性電磁鋼板の製造方法
JPS62167822A (ja) 鉄損の極めて低い一方向性珪素鋼板の製造方法
JPS6332849B2 (enrdf_load_stackoverflow)
US5318639A (en) Method of manufacturing grain oriented silicon steel sheets
JP3994667B2 (ja) 方向性電磁鋼板の製造方法
JPS59126722A (ja) 鉄損の優れた薄手高磁束密度一方向性電磁鋼板の製造方法
JPS62167821A (ja) 鉄損の極めて低い一方向性珪素鋼板の製造方法
JPS62167820A (ja) 鉄損の極めて低い一方向性珪素鋼板の製造方法
JPS6253572B2 (enrdf_load_stackoverflow)
JPH06256847A (ja) 磁気特性の優れた一方向性電磁鋼板の製造方法
JPH04235221A (ja) 鉄損の低い方向性電磁鋼板の製造方法
KR970007162B1 (ko) 철손 특성이 우수한 저온 스라브 가열방식의 방향성 전기강판의 제조방법
JP2991613B2 (ja) 磁気特性の良好な方向性珪素鋼板の製造方法
JPS58107417A (ja) 鉄損のすぐれた一方向性けい素鋼板の製造方法
JPS63162814A (ja) 鉄損劣化の少ない薄手方向性けい素鋼板の製造方法