JPS6167753A - 鉄損が低く、かつ磁束密度の優れた無方向性電磁鋼板 - Google Patents
鉄損が低く、かつ磁束密度の優れた無方向性電磁鋼板Info
- Publication number
- JPS6167753A JPS6167753A JP59188547A JP18854784A JPS6167753A JP S6167753 A JPS6167753 A JP S6167753A JP 59188547 A JP59188547 A JP 59188547A JP 18854784 A JP18854784 A JP 18854784A JP S6167753 A JPS6167753 A JP S6167753A
- Authority
- JP
- Japan
- Prior art keywords
- flux density
- magnetic flux
- iron loss
- electrical steel
- oriented electrical
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Soft Magnetic Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP59188547A JPS6167753A (ja) | 1984-09-08 | 1984-09-08 | 鉄損が低く、かつ磁束密度の優れた無方向性電磁鋼板 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP59188547A JPS6167753A (ja) | 1984-09-08 | 1984-09-08 | 鉄損が低く、かつ磁束密度の優れた無方向性電磁鋼板 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6167753A true JPS6167753A (ja) | 1986-04-07 |
| JPH0419295B2 JPH0419295B2 (enExample) | 1992-03-30 |
Family
ID=16225606
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP59188547A Granted JPS6167753A (ja) | 1984-09-08 | 1984-09-08 | 鉄損が低く、かつ磁束密度の優れた無方向性電磁鋼板 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6167753A (enExample) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH02179856A (ja) * | 1988-12-28 | 1990-07-12 | Nippon Steel Corp | 磁性焼鈍後の溶接性の優れた無方向性電磁鋼板 |
| US4946519A (en) * | 1987-06-18 | 1990-08-07 | Kawasaki Steel Corporation | Semi-processed non-oriented electromagnetic steel strip having low core loss and high magnetic permeability, and method of making |
| US5013372A (en) * | 1987-06-18 | 1991-05-07 | Kawasaki Steel Corporation | Semi-process non-oriented electromagnetic steel strip having low core loss and high magnetic permeability, and method of making |
| US5186763A (en) * | 1991-04-25 | 1993-02-16 | Nippon Steel Corporation | Process for production of non-oriented electrical steel sheet having excellent magnetic properties |
-
1984
- 1984-09-08 JP JP59188547A patent/JPS6167753A/ja active Granted
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4946519A (en) * | 1987-06-18 | 1990-08-07 | Kawasaki Steel Corporation | Semi-processed non-oriented electromagnetic steel strip having low core loss and high magnetic permeability, and method of making |
| US5013372A (en) * | 1987-06-18 | 1991-05-07 | Kawasaki Steel Corporation | Semi-process non-oriented electromagnetic steel strip having low core loss and high magnetic permeability, and method of making |
| JPH02179856A (ja) * | 1988-12-28 | 1990-07-12 | Nippon Steel Corp | 磁性焼鈍後の溶接性の優れた無方向性電磁鋼板 |
| US5186763A (en) * | 1991-04-25 | 1993-02-16 | Nippon Steel Corporation | Process for production of non-oriented electrical steel sheet having excellent magnetic properties |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0419295B2 (enExample) | 1992-03-30 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPH0469223B2 (enExample) | ||
| JP2022545793A (ja) | 無方向性電磁鋼板及びその製造方法 | |
| JP3888033B2 (ja) | 無方向性電磁鋼板の製造方法 | |
| JPS62180014A (ja) | 鉄損が低くかつ磁束密度の優れた無方向性電磁鋼板およびその製造方法 | |
| JPS6167753A (ja) | 鉄損が低く、かつ磁束密度の優れた無方向性電磁鋼板 | |
| JP4422220B2 (ja) | 磁束密度が高く鉄損の低い無方向性電磁鋼板及びその製造方法 | |
| JPH03229820A (ja) | 無方向性電磁鋼板の製造方法 | |
| JPH02258927A (ja) | 一方向性高磁束密度電磁鋼板の製造方法 | |
| JP3056970B2 (ja) | 磁気特性が優れた一方向性電磁鋼板の製造方法 | |
| JPH0625747A (ja) | 薄手高磁束密度一方向性電磁鋼板の製造方法 | |
| JPH03211258A (ja) | 磁気特性および表面性状の優れた無方向性電磁鋼板およびその製造方法 | |
| JPS59157259A (ja) | 鉄損が低くかつ磁束密度がすぐれた無方向性電磁鋼板およびその製造法 | |
| JPH0266138A (ja) | 磁気特性の優れた無方向性電磁鋼板およびその製造方法 | |
| JP2898793B2 (ja) | 高磁束密度、低鉄損を有する無方向性電磁鋼板の製造方法 | |
| JPH02104619A (ja) | 優れた鉄損特性を有する無方向性電磁鋼板の製造方法 | |
| JPS6333518A (ja) | 鉄損が低くかつ磁束密度がすぐれた無方向性電磁鋼板およびその製造法 | |
| JPH02104620A (ja) | 低鉄損の無方向性電磁鋼板の製造方法 | |
| JPH01139721A (ja) | 鉄損が低くかつ透磁率が高いセミプロセス無方向性電磁鋼板の製造方法 | |
| JP4320794B2 (ja) | 圧延方向の磁気特性に優れた電磁鋼板の製造方法 | |
| JPH0261031A (ja) | 磁気特性の優れた無方向性電磁鋼板およびその製造方法 | |
| JP3324044B2 (ja) | 超高磁束密度一方向性電磁鋼板の製造方法 | |
| JPH0331420A (ja) | 磁気特性の優れたフルプロセス無方向性電磁鋼板の製造方法 | |
| JP4163773B2 (ja) | 方向性電磁鋼板の製造方法 | |
| JPH06279859A (ja) | 鉄損および磁束密度が極めて優れた無方向性電磁鋼板の製造方法 | |
| JPH03294422A (ja) | 磁気特性の優れた無方向性電磁鋼板の製造方法 |