JPS6152379A - 接水金属材料の防食方法及び装置 - Google Patents
接水金属材料の防食方法及び装置Info
- Publication number
- JPS6152379A JPS6152379A JP59173714A JP17371484A JPS6152379A JP S6152379 A JPS6152379 A JP S6152379A JP 59173714 A JP59173714 A JP 59173714A JP 17371484 A JP17371484 A JP 17371484A JP S6152379 A JPS6152379 A JP S6152379A
- Authority
- JP
- Japan
- Prior art keywords
- dissolved oxygen
- water
- oxygen concentration
- corrosion
- contact
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E30/00—Energy generation of nuclear origin
Landscapes
- Preventing Corrosion Or Incrustation Of Metals (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP59173714A JPS6152379A (ja) | 1984-08-21 | 1984-08-21 | 接水金属材料の防食方法及び装置 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP59173714A JPS6152379A (ja) | 1984-08-21 | 1984-08-21 | 接水金属材料の防食方法及び装置 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6152379A true JPS6152379A (ja) | 1986-03-15 |
JPH0438836B2 JPH0438836B2 (enrdf_load_stackoverflow) | 1992-06-25 |
Family
ID=15965768
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP59173714A Granted JPS6152379A (ja) | 1984-08-21 | 1984-08-21 | 接水金属材料の防食方法及び装置 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6152379A (enrdf_load_stackoverflow) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2015218968A (ja) * | 2014-05-19 | 2015-12-07 | パナソニックIpマネジメント株式会社 | 過熱水蒸気処理方法及び装置 |
CN106499659A (zh) * | 2016-11-28 | 2017-03-15 | 云南驰宏锌锗股份有限公司 | 一种离心风机停运状态下防锈蚀的保护装置及保护方法 |
-
1984
- 1984-08-21 JP JP59173714A patent/JPS6152379A/ja active Granted
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2015218968A (ja) * | 2014-05-19 | 2015-12-07 | パナソニックIpマネジメント株式会社 | 過熱水蒸気処理方法及び装置 |
CN106499659A (zh) * | 2016-11-28 | 2017-03-15 | 云南驰宏锌锗股份有限公司 | 一种离心风机停运状态下防锈蚀的保护装置及保护方法 |
CN106499659B (zh) * | 2016-11-28 | 2019-06-21 | 云南驰宏锌锗股份有限公司 | 一种离心风机停运状态下防锈蚀的保护装置及保护方法 |
Also Published As
Publication number | Publication date |
---|---|
JPH0438836B2 (enrdf_load_stackoverflow) | 1992-06-25 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US5130080A (en) | Method of providing extended life expectancy for components of boiling water reactors | |
US9758880B2 (en) | Method and system for controlling water chemistry in power generation plant | |
JP5637867B2 (ja) | プラントの運転方法及びシステム | |
US4820473A (en) | Method of reducing radioactivity in nuclear plant | |
CA2221002A1 (en) | In situ palladium doping or coating of stainless steel surfaces | |
US11170902B2 (en) | Nuclear power plant and method for operating a nuclear power plant | |
CA1188594A (en) | Method of scavenging dissolved oxygen in steam generating equipment using ammonia or amine neutralized erythorbic acid | |
JPS6152379A (ja) | 接水金属材料の防食方法及び装置 | |
Hiro et al. | Stagnations of increasing trends in negative pressure with repeated cavitation in water/metal Berthelot tubes as a result of mechanical sealing | |
JPS6230269B2 (enrdf_load_stackoverflow) | ||
US3415692A (en) | Method of passivating metal surfaces | |
JP2017218656A (ja) | ステンレス鋼の局部腐食抑制方法及び金属容器の保管方法 | |
JPS6151758B2 (enrdf_load_stackoverflow) | ||
JPH0566999B2 (enrdf_load_stackoverflow) | ||
Verma et al. | Corrosion inhibition in lithium bromide absorption fluid for advanced and current absorption cycle machines | |
JPS6296898A (ja) | 発電プラント | |
RU2271410C2 (ru) | Способ защиты от коррозии энергетического оборудования | |
US4587098A (en) | Method of stabilized operation of acid digestion kettle of tantalum | |
JPH0694209A (ja) | ボイラ給水処理方法 | |
JPS58185778A (ja) | 炭素鋼の防食 | |
KR20010108013A (ko) | 핵 발전소의 오염물질 제거방법 | |
JPH068913B2 (ja) | 原子力プラントの放射能低減方法 | |
JPS61149501A (ja) | 原子力タ−ビンロ−タデイスクの応力腐食割れ防止方法 | |
JPH02280890A (ja) | 火力発電プラントの水処理方法 | |
JPH0636066B2 (ja) | 原子力発電プラントの防蝕皮膜生成方法及びその装置 |