JPS612738A - 合成樹脂成形品の表面処理方法 - Google Patents
合成樹脂成形品の表面処理方法Info
- Publication number
- JPS612738A JPS612738A JP59122686A JP12268684A JPS612738A JP S612738 A JPS612738 A JP S612738A JP 59122686 A JP59122686 A JP 59122686A JP 12268684 A JP12268684 A JP 12268684A JP S612738 A JPS612738 A JP S612738A
- Authority
- JP
- Japan
- Prior art keywords
- treatment
- synthetic resin
- resin molded
- molded article
- low
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Coating Of Shaped Articles Made Of Macromolecular Substances (AREA)
- Manufacture Of Macromolecular Shaped Articles (AREA)
- Treatments Of Macromolecular Shaped Articles (AREA)
- Application Of Or Painting With Fluid Materials (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP59122686A JPS612738A (ja) | 1984-06-13 | 1984-06-13 | 合成樹脂成形品の表面処理方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP59122686A JPS612738A (ja) | 1984-06-13 | 1984-06-13 | 合成樹脂成形品の表面処理方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS612738A true JPS612738A (ja) | 1986-01-08 |
JPH0526815B2 JPH0526815B2 (ko) | 1993-04-19 |
Family
ID=14842110
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP59122686A Granted JPS612738A (ja) | 1984-06-13 | 1984-06-13 | 合成樹脂成形品の表面処理方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS612738A (ko) |
Cited By (9)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS62179536A (ja) * | 1986-02-03 | 1987-08-06 | Mazda Motor Corp | ポリエチレン製ガソリンタンクの製造方法 |
JPS6470536A (en) * | 1987-08-03 | 1989-03-16 | Becton Dickinson Co | Method of preparing lubricating surface |
EP0590467A1 (de) * | 1992-09-26 | 1994-04-06 | Röhm Gmbh | Verfahren zum Erzeugen von siliciumoxidischen kratzfesten Schichten auf Kunststoffen durch Plasmabeschichtung |
JPH10500637A (ja) * | 1994-12-05 | 1998-01-20 | インテグレイテッド ライナー テクノロジーズ,インコーポレイテッド | 硬化エラストマーのプラスチック及び金属との結合 |
JP2002082223A (ja) * | 2000-09-08 | 2002-03-22 | Konica Corp | 偏光板用保護フィルム、光学用フィルムおよび画像表示材料 |
JP2006253398A (ja) * | 2005-03-10 | 2006-09-21 | Shin Etsu Chem Co Ltd | 半導体装置の製造方法 |
WO2007119552A1 (ja) * | 2006-03-29 | 2007-10-25 | Zeon Corporation | 樹脂複合成形体の製造方法 |
WO2017002973A1 (ja) * | 2015-07-02 | 2017-01-05 | コニカミノルタ株式会社 | 接合体及び接合体の製造方法 |
WO2017002974A1 (ja) * | 2015-07-02 | 2017-01-05 | コニカミノルタ株式会社 | 接合体及び接合体の製造方法 |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2003111843A (ja) * | 2001-10-05 | 2003-04-15 | Awi Mach:Kk | 注射器用キャップ、注射器、および注射器用キャップの製造方法 |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS57202323A (en) * | 1981-06-08 | 1982-12-11 | Shin Etsu Chem Co Ltd | Antistatic fluorine-contained resin molded article |
JPS5930832A (ja) * | 1982-08-13 | 1984-02-18 | Shin Etsu Chem Co Ltd | 表面特性の改質されたフツ素系樹脂成形品 |
-
1984
- 1984-06-13 JP JP59122686A patent/JPS612738A/ja active Granted
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS57202323A (en) * | 1981-06-08 | 1982-12-11 | Shin Etsu Chem Co Ltd | Antistatic fluorine-contained resin molded article |
JPS5930832A (ja) * | 1982-08-13 | 1984-02-18 | Shin Etsu Chem Co Ltd | 表面特性の改質されたフツ素系樹脂成形品 |
Cited By (15)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS62179536A (ja) * | 1986-02-03 | 1987-08-06 | Mazda Motor Corp | ポリエチレン製ガソリンタンクの製造方法 |
JPS6470536A (en) * | 1987-08-03 | 1989-03-16 | Becton Dickinson Co | Method of preparing lubricating surface |
EP0590467A1 (de) * | 1992-09-26 | 1994-04-06 | Röhm Gmbh | Verfahren zum Erzeugen von siliciumoxidischen kratzfesten Schichten auf Kunststoffen durch Plasmabeschichtung |
JPH10500637A (ja) * | 1994-12-05 | 1998-01-20 | インテグレイテッド ライナー テクノロジーズ,インコーポレイテッド | 硬化エラストマーのプラスチック及び金属との結合 |
US6234335B1 (en) | 1994-12-05 | 2001-05-22 | Integrated Liner Technologies Inc. | Sealable container and open top cap with directly bonded elastomer septum |
JP2002082223A (ja) * | 2000-09-08 | 2002-03-22 | Konica Corp | 偏光板用保護フィルム、光学用フィルムおよび画像表示材料 |
JP2006253398A (ja) * | 2005-03-10 | 2006-09-21 | Shin Etsu Chem Co Ltd | 半導体装置の製造方法 |
JP4623282B2 (ja) * | 2005-03-10 | 2011-02-02 | 信越化学工業株式会社 | 半導体装置の製造方法 |
KR101243533B1 (ko) * | 2005-03-10 | 2013-03-20 | 신에쓰 가가꾸 고교 가부시끼가이샤 | 반도체 장치의 제조 방법 |
TWI413219B (zh) * | 2005-03-10 | 2013-10-21 | Shinetsu Chemical Co | Semiconductor device manufacturing method |
WO2007119552A1 (ja) * | 2006-03-29 | 2007-10-25 | Zeon Corporation | 樹脂複合成形体の製造方法 |
JP4998462B2 (ja) * | 2006-03-29 | 2012-08-15 | 日本ゼオン株式会社 | 樹脂複合成形体の製造方法 |
US8287682B2 (en) | 2006-03-29 | 2012-10-16 | Zeon Corporation | Process for production of resin composite molded article |
WO2017002973A1 (ja) * | 2015-07-02 | 2017-01-05 | コニカミノルタ株式会社 | 接合体及び接合体の製造方法 |
WO2017002974A1 (ja) * | 2015-07-02 | 2017-01-05 | コニカミノルタ株式会社 | 接合体及び接合体の製造方法 |
Also Published As
Publication number | Publication date |
---|---|
JPH0526815B2 (ko) | 1993-04-19 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
RU2137603C1 (ru) | Способ усиления эффекта отделения от формы | |
Hegemann et al. | Plasma treatment of polymers to generate stable, hydrophobic surfaces | |
US4649071A (en) | Composite material and process for producing the same | |
US5879757A (en) | Surface treatment of polymers | |
EP0118527B1 (en) | A method of making an abrasion resistant coating on a solid substrate and articles produced thereby | |
US5569497A (en) | Protective coating of plastic substrates via plasma-polymerization | |
Friedrich et al. | Formation of plasma polymer layers with functional groups of different type and density at polymer surfaces and their interaction with Al atoms | |
JP2005531654A5 (ko) | ||
EP1242515B1 (en) | Surface treatment of an organic polymeric material | |
JPH0848543A (ja) | 種々の基板上への防曇及び耐引掻性コーティングのプラズマ強化化学蒸着法 | |
AU779530B2 (en) | A method of coating the surface of an inorganic substrate with an organic material and the product obtained | |
JP2003504438A5 (ko) | ||
JPS612738A (ja) | 合成樹脂成形品の表面処理方法 | |
KR20070072899A (ko) | 향상된 증착 속도의 플라즈마 강화 화학 기상 방법 | |
GB2053026A (en) | Microwave plasma modification of surface properties in organic polymers | |
JPS63124521A (ja) | X線リソグラフイ−用マスク表面の処理方法 | |
Chen et al. | Preliminary experiment of surface hardening of polymers by glow discharge polymerization | |
Bhat et al. | Adhesion aspects of plasma polymerized acetonitrile and acrylonitrile on polypropylene surface | |
Yu et al. | Surface passivation of epoxy resin with a covalently adhered poly (tetrafluoroethylene) layer | |
JPS62132940A (ja) | 高分子基材へのプラズマ重合薄膜形成方法 | |
EP0543634A1 (en) | Improvements in coating processes | |
Costantino et al. | Improvement of the adhesion of silicone to aluminum using plasma polymerization | |
KR0149054B1 (ko) | 소수성 고분자 표면의 친수화방법 | |
Schalken et al. | μPlasma Printing Deposition of Amine-Containing Organo-Silane Polymers by Means of 3-Aminopropyl Trimethoxysilane | |
JP3261452B2 (ja) | 生分解性プラスチック積層体及び生分解性プラスチック成型体の表面加工方法 |