JPS61272323A - 連続焼鈍による表面処理用原板の製造方法 - Google Patents
連続焼鈍による表面処理用原板の製造方法Info
- Publication number
- JPS61272323A JPS61272323A JP11458185A JP11458185A JPS61272323A JP S61272323 A JPS61272323 A JP S61272323A JP 11458185 A JP11458185 A JP 11458185A JP 11458185 A JP11458185 A JP 11458185A JP S61272323 A JPS61272323 A JP S61272323A
- Authority
- JP
- Japan
- Prior art keywords
- temper
- rolling
- cooling rate
- degree
- continuous annealing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 238000000137 annealing Methods 0.000 title claims abstract description 38
- 238000004519 manufacturing process Methods 0.000 title claims abstract description 16
- 238000004381 surface treatment Methods 0.000 title claims description 15
- 238000005096 rolling process Methods 0.000 claims abstract description 78
- 238000001816 cooling Methods 0.000 claims abstract description 69
- 238000000034 method Methods 0.000 claims abstract description 59
- 229910000831 Steel Inorganic materials 0.000 claims abstract description 37
- 239000010959 steel Substances 0.000 claims abstract description 37
- 230000008569 process Effects 0.000 claims abstract description 29
- 238000001953 recrystallisation Methods 0.000 claims abstract description 4
- 230000009466 transformation Effects 0.000 claims abstract description 3
- 230000009467 reduction Effects 0.000 claims description 28
- 238000002791 soaking Methods 0.000 claims description 13
- 239000012535 impurity Substances 0.000 claims description 4
- 238000005098 hot rolling Methods 0.000 abstract description 8
- 229910052799 carbon Inorganic materials 0.000 abstract description 5
- 238000005097 cold rolling Methods 0.000 abstract description 3
- 229910001209 Low-carbon steel Inorganic materials 0.000 abstract description 2
- 230000008859 change Effects 0.000 description 39
- 235000019589 hardness Nutrition 0.000 description 31
- 238000010438 heat treatment Methods 0.000 description 19
- 239000000463 material Substances 0.000 description 18
- 239000000203 mixture Substances 0.000 description 14
- 239000006104 solid solution Substances 0.000 description 14
- 238000005496 tempering Methods 0.000 description 13
- 239000000126 substance Substances 0.000 description 11
- 239000005028 tinplate Substances 0.000 description 11
- 239000007787 solid Substances 0.000 description 10
- 230000000694 effects Effects 0.000 description 6
- 238000002474 experimental method Methods 0.000 description 5
- 230000007423 decrease Effects 0.000 description 4
- 238000010586 diagram Methods 0.000 description 3
- 230000037311 normal skin Effects 0.000 description 3
- 238000012545 processing Methods 0.000 description 3
- 239000005029 tin-free steel Substances 0.000 description 3
- OKTJSMMVPCPJKN-UHFFFAOYSA-N Carbon Chemical compound [C] OKTJSMMVPCPJKN-UHFFFAOYSA-N 0.000 description 2
- ATJFFYVFTNAWJD-UHFFFAOYSA-N Tin Chemical compound [Sn] ATJFFYVFTNAWJD-UHFFFAOYSA-N 0.000 description 2
- 238000007796 conventional method Methods 0.000 description 2
- 238000005336 cracking Methods 0.000 description 2
- 239000013078 crystal Substances 0.000 description 2
- 238000007747 plating Methods 0.000 description 2
- 238000007670 refining Methods 0.000 description 2
- 238000010583 slow cooling Methods 0.000 description 2
- 238000005482 strain hardening Methods 0.000 description 2
- 229910000655 Killed steel Inorganic materials 0.000 description 1
- 229910001327 Rimmed steel Inorganic materials 0.000 description 1
- 230000002411 adverse Effects 0.000 description 1
- 239000010953 base metal Substances 0.000 description 1
- 239000010960 cold rolled steel Substances 0.000 description 1
- 230000006866 deterioration Effects 0.000 description 1
- 239000012530 fluid Substances 0.000 description 1
- 239000003205 fragrance Substances 0.000 description 1
- 238000007429 general method Methods 0.000 description 1
- 230000009931 harmful effect Effects 0.000 description 1
- 238000002844 melting Methods 0.000 description 1
- 230000008018 melting Effects 0.000 description 1
- 239000002184 metal Substances 0.000 description 1
- 229910052751 metal Inorganic materials 0.000 description 1
- 230000035515 penetration Effects 0.000 description 1
- 239000002304 perfume Substances 0.000 description 1
- 238000001556 precipitation Methods 0.000 description 1
- 238000004886 process control Methods 0.000 description 1
- 230000035945 sensitivity Effects 0.000 description 1
- 238000009987 spinning Methods 0.000 description 1
- 238000004804 winding Methods 0.000 description 1
Landscapes
- Heat Treatment Of Steel (AREA)
- Heat Treatment Of Sheet Steel (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11458185A JPS61272323A (ja) | 1985-05-28 | 1985-05-28 | 連続焼鈍による表面処理用原板の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11458185A JPS61272323A (ja) | 1985-05-28 | 1985-05-28 | 連続焼鈍による表面処理用原板の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS61272323A true JPS61272323A (ja) | 1986-12-02 |
JPH0545653B2 JPH0545653B2 (enrdf_load_stackoverflow) | 1993-07-09 |
Family
ID=14641425
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP11458185A Granted JPS61272323A (ja) | 1985-05-28 | 1985-05-28 | 連続焼鈍による表面処理用原板の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS61272323A (enrdf_load_stackoverflow) |
Cited By (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US6702904B2 (en) | 2000-02-29 | 2004-03-09 | Jfe Steel Corporation | High tensile cold-rolled steel sheet having excellent strain aging hardening properties |
EP1291447A4 (en) * | 2000-05-31 | 2004-05-19 | Jfe Steel Corp | COLD ROLLED STEEL SHEET WITH EXCELLENT RECOLD AGING PROPERTIES AND PRODUCTION METHOD FOR SUCH A STEEL SHEET |
EP1291448A4 (en) * | 2000-05-26 | 2004-06-30 | Jfe Steel Corp | COLD ROLLED STEEL SHEET AND GALVANIZED STEEL SHEET WITH GOOD RECOLD AGING PROPERTIES AND MANUFACTURING METHOD THEREFOR |
US7067023B2 (en) | 2000-05-26 | 2006-06-27 | Jfe Steel Corporation | Cold rolled steel sheet and galvanized steel sheet having strain age hardenability and method of producing the same |
KR100946132B1 (ko) * | 2002-09-30 | 2010-03-10 | 주식회사 포스코 | 주석도금 원판의 제조방법 |
JP2011063881A (ja) * | 2009-08-21 | 2011-03-31 | Jfe Steel Corp | 高張力冷延鋼板およびその製造方法 |
Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS50121118A (enrdf_load_stackoverflow) * | 1974-03-12 | 1975-09-22 | ||
JPS50139013A (enrdf_load_stackoverflow) * | 1974-04-27 | 1975-11-06 | ||
JPS5141623A (en) * | 1974-10-05 | 1976-04-08 | Nippon Steel Corp | Renzokushodonnyoru nanshitsunahyomenshoryokohanno seizoho |
JPS5857490A (ja) * | 1981-10-02 | 1983-04-05 | Toa Gurauto Kogyo Kk | 掘削面安定化用泥水液組成物 |
-
1985
- 1985-05-28 JP JP11458185A patent/JPS61272323A/ja active Granted
Patent Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS50121118A (enrdf_load_stackoverflow) * | 1974-03-12 | 1975-09-22 | ||
JPS50139013A (enrdf_load_stackoverflow) * | 1974-04-27 | 1975-11-06 | ||
JPS5141623A (en) * | 1974-10-05 | 1976-04-08 | Nippon Steel Corp | Renzokushodonnyoru nanshitsunahyomenshoryokohanno seizoho |
JPS5857490A (ja) * | 1981-10-02 | 1983-04-05 | Toa Gurauto Kogyo Kk | 掘削面安定化用泥水液組成物 |
Cited By (12)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US6702904B2 (en) | 2000-02-29 | 2004-03-09 | Jfe Steel Corporation | High tensile cold-rolled steel sheet having excellent strain aging hardening properties |
EP1193322A4 (en) * | 2000-02-29 | 2004-06-30 | Jfe Steel Corp | HIGH-STRENGTH HOT ROLLED STEEL SHEET WITH EXCELLENT RECALDERING PROPERTIES |
US6899771B2 (en) | 2000-02-29 | 2005-05-31 | Jfe Steel Corporation | High tensile strength cold rolled steel sheet having excellent strain age hardening characteristics and the production thereof |
US6902632B2 (en) | 2000-02-29 | 2005-06-07 | Jfe Steel Corporation | High tensile strength cold rolled steel sheet having excellent strain age hardening characteristics and the production thereof |
EP1571230A1 (en) * | 2000-02-29 | 2005-09-07 | JFE Steel Corporation | High tensile strength cold rolled steel sheet having excellent strain age hardening characteristics and the production thereof |
EP1571229A1 (en) * | 2000-02-29 | 2005-09-07 | JFE Steel Corporation | High tensile strength cold rolled steel sheet having excellent strain age hardening characteristics and the production thereof |
EP1291448A4 (en) * | 2000-05-26 | 2004-06-30 | Jfe Steel Corp | COLD ROLLED STEEL SHEET AND GALVANIZED STEEL SHEET WITH GOOD RECOLD AGING PROPERTIES AND MANUFACTURING METHOD THEREFOR |
US7067023B2 (en) | 2000-05-26 | 2006-06-27 | Jfe Steel Corporation | Cold rolled steel sheet and galvanized steel sheet having strain age hardenability and method of producing the same |
US7101445B2 (en) | 2000-05-26 | 2006-09-05 | Jfe Steel Corporation | Cold rolled steel sheet and galvanized steel sheet having strain age hardenability and method of producing the same |
EP1291447A4 (en) * | 2000-05-31 | 2004-05-19 | Jfe Steel Corp | COLD ROLLED STEEL SHEET WITH EXCELLENT RECOLD AGING PROPERTIES AND PRODUCTION METHOD FOR SUCH A STEEL SHEET |
KR100946132B1 (ko) * | 2002-09-30 | 2010-03-10 | 주식회사 포스코 | 주석도금 원판의 제조방법 |
JP2011063881A (ja) * | 2009-08-21 | 2011-03-31 | Jfe Steel Corp | 高張力冷延鋼板およびその製造方法 |
Also Published As
Publication number | Publication date |
---|---|
JPH0545653B2 (enrdf_load_stackoverflow) | 1993-07-09 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP7118972B2 (ja) | 非常に良好な成形性を有する焼戻しされた被覆鋼板及びこの鋼板を製造する方法 | |
JP5283504B2 (ja) | 優れた延性を有する高強度鋼板を製造する方法およびこれにより製造された鋼板 | |
JP6992070B2 (ja) | 非常に良好な成形性を有する焼戻しされた被覆鋼板及びこの鋼板を製造する方法 | |
JPS6014097B2 (ja) | 2つの相から成る熱間圧延鋼ストリップ | |
JPS6111291B2 (enrdf_load_stackoverflow) | ||
CN105063511B (zh) | 中厚板轧机轧制超低碳贝氏体类薄规格钢板及其生产方法 | |
JP2008138234A (ja) | 高強度高延性缶用鋼板およびその製造方法 | |
JPS61272323A (ja) | 連続焼鈍による表面処理用原板の製造方法 | |
JPS6169928A (ja) | 連続焼鈍によるしごき加工用鋼板の製造方法 | |
JPS5842725A (ja) | 加工性のすぐれた高強度熱延鋼板の製造法 | |
KR20210079720A (ko) | 합금화용융아연도금 강판 및 그 제조방법 | |
JPS63223125A (ja) | 高靭性高張力鋼板の製造方法 | |
EP1022347A1 (en) | Method for producing raw plate for surface treatment plate for can using continuous annealing | |
US4662950A (en) | Method of making a steel plate for construction applications | |
JPH02129319A (ja) | 表面処理鋼板用原板の製造方法 | |
JPS6263619A (ja) | 軟質な非時効性薄鋼板の製造方法 | |
JPH03150316A (ja) | 深絞り用冷延鋼板の製造方法 | |
JPS61207520A (ja) | 軟質の非時効性表面処理用鋼板の製造方法 | |
JPH02213415A (ja) | 高強度、高靭性棒鋼の製造方法 | |
JP2674388B2 (ja) | 高成形性溶融亜鉛メッキ鋼板の製造方法 | |
JP3324074B2 (ja) | 高強度高延性容器用鋼板およびその製造方法 | |
JPH0394020A (ja) | 耐2次加工脆性に優れた深絞り用冷延鋼板の製造方法 | |
JPS6142766B2 (enrdf_load_stackoverflow) | ||
JPS62139823A (ja) | 深絞り用冷延鋼板の製造方法 | |
JPS6354048B2 (enrdf_load_stackoverflow) |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
LAPS | Cancellation because of no payment of annual fees |