JPS61253357A - 溶射被膜の硬度回復方法 - Google Patents

溶射被膜の硬度回復方法

Info

Publication number
JPS61253357A
JPS61253357A JP9651785A JP9651785A JPS61253357A JP S61253357 A JPS61253357 A JP S61253357A JP 9651785 A JP9651785 A JP 9651785A JP 9651785 A JP9651785 A JP 9651785A JP S61253357 A JPS61253357 A JP S61253357A
Authority
JP
Japan
Prior art keywords
film
hardness
laser
iron
thermally sprayed
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP9651785A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0243821B2 (enrdf_load_stackoverflow
Inventor
Katsutoshi Okano
岡野 勝敏
Fumiaki Otsubo
文明 大坪
Hiroshi Nojima
野島 宏
Takashi Shigematsu
孝 重松
Suguru Nakamura
英 中村
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yoshikawa Kogyo Co Ltd
Toshiba Corp
Original Assignee
Yoshikawa Kogyo Co Ltd
Toshiba Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yoshikawa Kogyo Co Ltd, Toshiba Corp filed Critical Yoshikawa Kogyo Co Ltd
Priority to JP9651785A priority Critical patent/JPS61253357A/ja
Publication of JPS61253357A publication Critical patent/JPS61253357A/ja
Publication of JPH0243821B2 publication Critical patent/JPH0243821B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Coating By Spraying Or Casting (AREA)
JP9651785A 1985-05-07 1985-05-07 溶射被膜の硬度回復方法 Granted JPS61253357A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP9651785A JPS61253357A (ja) 1985-05-07 1985-05-07 溶射被膜の硬度回復方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP9651785A JPS61253357A (ja) 1985-05-07 1985-05-07 溶射被膜の硬度回復方法

Publications (2)

Publication Number Publication Date
JPS61253357A true JPS61253357A (ja) 1986-11-11
JPH0243821B2 JPH0243821B2 (enrdf_load_stackoverflow) 1990-10-01

Family

ID=14167329

Family Applications (1)

Application Number Title Priority Date Filing Date
JP9651785A Granted JPS61253357A (ja) 1985-05-07 1985-05-07 溶射被膜の硬度回復方法

Country Status (1)

Country Link
JP (1) JPS61253357A (enrdf_load_stackoverflow)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2007154261A (ja) * 2005-12-06 2007-06-21 Kyushu Institute Of Technology 溶射皮膜を形成した素材の改質方法
JP2009537701A (ja) * 2006-05-24 2009-10-29 ブルースコープ・スティール・リミテッド Al/Znベースの合金被覆製品の処理

Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5518575A (en) * 1978-07-28 1980-02-08 Komatsu Ltd Surface treating method

Patent Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5518575A (en) * 1978-07-28 1980-02-08 Komatsu Ltd Surface treating method

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2007154261A (ja) * 2005-12-06 2007-06-21 Kyushu Institute Of Technology 溶射皮膜を形成した素材の改質方法
JP2009537701A (ja) * 2006-05-24 2009-10-29 ブルースコープ・スティール・リミテッド Al/Znベースの合金被覆製品の処理

Also Published As

Publication number Publication date
JPH0243821B2 (enrdf_load_stackoverflow) 1990-10-01

Similar Documents

Publication Publication Date Title
CN101519778B (zh) 一种穿孔顶头表面强化的激光熔覆方法
JP3065674B2 (ja) 基体の保護層および保護層形成方法
JP2003531731A (ja) ろう付け方法およびそれから製造された製品
CN101519704A (zh) 一种高炉风口激光熔覆钴基合金涂层的方法
JPS5942070B2 (ja) テツ コウ オヨビ ソノセイヒン ノ ヒヨウメンヒメヒンフホウホウ
CN113699521B (zh) 一种高性能钛合金表面涂层及其制备方法
US2496971A (en) Thermite coating process
JPH0778273B2 (ja) 翼部材の表面処理方法
JPS61253357A (ja) 溶射被膜の硬度回復方法
JPS591678A (ja) 複合熱間工具鋼の製造法
JPS6010826B2 (ja) 金属連続鋳造機械用鋳造ベルト
JPS61113757A (ja) 金属基体面に形成した異種金属被膜のレ−ザ−処理方法
JP2736525B2 (ja) 溶射方法
James A review of experimental findings in surface preparation for thermal spraying
JPS62116784A (ja) 粉体形成被膜の硬度回復方法
JP2638327B2 (ja) 高耐摩耗チタン合金製部品
CA3163982A1 (en) Pre-coated steel sheet comprising an additional coating for increasing the mechanical strength of the weld metal zone of a welded steel part prepared from said pre-coated sheet
JPS58153731A (ja) 溶接残留応力の低減方法
Dubrovskii et al. Electric resistance surfacing with a wire and with melting of the metals to be joined
Amuda et al. Wear and corrosion characteristics of silicon carbide surface modified mild steel
JP2785139B2 (ja) 圧延用複合ロール及びその製造法
RU2007107551A (ru) Способ восстановления изношенных поверхностей деталей машин
JPS6360270A (ja) 鋳鉄の耐摩耗性向上方法
SU975284A2 (ru) Способ сварки давлением
RU2499077C1 (ru) Способ нанесения износостойких покрытий на стальные изделия

Legal Events

Date Code Title Description
R250 Receipt of annual fees

Free format text: JAPANESE INTERMEDIATE CODE: R250

EXPY Cancellation because of completion of term