JPS6114227B2 - - Google Patents
Info
- Publication number
- JPS6114227B2 JPS6114227B2 JP56191825A JP19182581A JPS6114227B2 JP S6114227 B2 JPS6114227 B2 JP S6114227B2 JP 56191825 A JP56191825 A JP 56191825A JP 19182581 A JP19182581 A JP 19182581A JP S6114227 B2 JPS6114227 B2 JP S6114227B2
- Authority
- JP
- Japan
- Prior art keywords
- surface treatment
- inorganic
- sprayed layer
- substance
- glassy
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
- 238000004381 surface treatment Methods 0.000 claims description 20
- 239000000126 substance Substances 0.000 claims description 16
- 229910010272 inorganic material Inorganic materials 0.000 claims description 13
- 239000011147 inorganic material Substances 0.000 claims description 13
- 239000000463 material Substances 0.000 claims description 13
- 238000000034 method Methods 0.000 claims description 12
- 229910018072 Al 2 O 3 Inorganic materials 0.000 claims description 10
- 229910004298 SiO 2 Inorganic materials 0.000 claims description 5
- 239000000203 mixture Substances 0.000 claims description 2
- 239000011248 coating agent Substances 0.000 description 17
- 238000000576 coating method Methods 0.000 description 17
- 230000000873 masking effect Effects 0.000 description 14
- 239000000843 powder Substances 0.000 description 8
- 238000011282 treatment Methods 0.000 description 6
- 239000011521 glass Substances 0.000 description 5
- 238000005255 carburizing Methods 0.000 description 4
- 230000035939 shock Effects 0.000 description 4
- 238000005507 spraying Methods 0.000 description 4
- 238000009792 diffusion process Methods 0.000 description 3
- 238000002844 melting Methods 0.000 description 3
- 230000008018 melting Effects 0.000 description 3
- 230000035515 penetration Effects 0.000 description 3
- 238000007751 thermal spraying Methods 0.000 description 3
- 238000007796 conventional method Methods 0.000 description 2
- 238000005336 cracking Methods 0.000 description 2
- 238000005121 nitriding Methods 0.000 description 2
- 230000002265 prevention Effects 0.000 description 2
- 239000007921 spray Substances 0.000 description 2
- 239000000758 substrate Substances 0.000 description 2
- OKTJSMMVPCPJKN-UHFFFAOYSA-N Carbon Chemical compound [C] OKTJSMMVPCPJKN-UHFFFAOYSA-N 0.000 description 1
- 238000005299 abrasion Methods 0.000 description 1
- XAGFODPZIPBFFR-UHFFFAOYSA-N aluminium Chemical compound [Al] XAGFODPZIPBFFR-UHFFFAOYSA-N 0.000 description 1
- 229910052782 aluminium Inorganic materials 0.000 description 1
- 230000015572 biosynthetic process Effects 0.000 description 1
- 238000005422 blasting Methods 0.000 description 1
- 229910052799 carbon Inorganic materials 0.000 description 1
- 239000000919 ceramic Substances 0.000 description 1
- 238000005260 corrosion Methods 0.000 description 1
- 230000007797 corrosion Effects 0.000 description 1
- 238000005516 engineering process Methods 0.000 description 1
- 239000000155 melt Substances 0.000 description 1
- 238000007750 plasma spraying Methods 0.000 description 1
- 238000007747 plating Methods 0.000 description 1
- 239000011148 porous material Substances 0.000 description 1
- 229920005989 resin Polymers 0.000 description 1
- 239000011347 resin Substances 0.000 description 1
- 239000011800 void material Substances 0.000 description 1
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C10/00—Solid state diffusion of only metal elements or silicon into metallic material surfaces
- C23C10/04—Diffusion into selected surface areas, e.g. using masks
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C4/00—Coating by spraying the coating material in the molten state, e.g. by flame, plasma or electric discharge
- C23C4/01—Selective coating, e.g. pattern coating, without pre-treatment of the material to be coated
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Physics & Mathematics (AREA)
- Plasma & Fusion (AREA)
- Coating By Spraying Or Casting (AREA)
- Other Surface Treatments For Metallic Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56191825A JPS5893865A (ja) | 1981-12-01 | 1981-12-01 | 表面処理防止方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56191825A JPS5893865A (ja) | 1981-12-01 | 1981-12-01 | 表面処理防止方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5893865A JPS5893865A (ja) | 1983-06-03 |
| JPS6114227B2 true JPS6114227B2 (enExample) | 1986-04-17 |
Family
ID=16281141
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP56191825A Granted JPS5893865A (ja) | 1981-12-01 | 1981-12-01 | 表面処理防止方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5893865A (enExample) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2017098854A1 (ja) * | 2015-12-09 | 2017-06-15 | 日本電気硝子株式会社 | 封孔剤、封孔剤塗布液、耐食性被膜、高温部材及び高温部材の製造方法 |
Families Citing this family (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS59169347U (ja) * | 1983-04-27 | 1984-11-13 | 光洋精工株式会社 | キ−溝を備えた軸 |
| JPH02217482A (ja) * | 1989-12-16 | 1990-08-30 | Yoshikawa Kogyo Co Ltd | ガラス質皮膜成形物 |
| JPH02298249A (ja) * | 1990-04-14 | 1990-12-10 | Koyo Seiko Co Ltd | キー溝を備えた軸の浸炭方法 |
| WO2018159195A1 (ja) * | 2017-02-28 | 2018-09-07 | 日本電気硝子株式会社 | 封孔剤、封孔剤塗布液、耐食性被膜、高温部材及びこれらの製造方法 |
-
1981
- 1981-12-01 JP JP56191825A patent/JPS5893865A/ja active Granted
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2017098854A1 (ja) * | 2015-12-09 | 2017-06-15 | 日本電気硝子株式会社 | 封孔剤、封孔剤塗布液、耐食性被膜、高温部材及び高温部材の製造方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5893865A (ja) | 1983-06-03 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US2310239A (en) | Corrosion resistant coating for metal surfaces | |
| EP0911422A3 (en) | Method of forming a bond coat for a thermal barrier coating | |
| CN101707942A (zh) | 产生和去除针对阴极涂层的临时性保护层的方法 | |
| JP4395359B2 (ja) | 高温適用のための、低温硬化セラミックコーティングを形成するためのシステム及び方法 | |
| JPH07268594A (ja) | 溶融金属めっき浴浸漬部材とその製造方法 | |
| RU2008118511A (ru) | Ролики с покрытием, нанесенным методом термического напыления | |
| US6284320B1 (en) | Method for producing member for molten metal bath having coating film excellent in resistance to corrosion by molten metal | |
| JPH03180457A (ja) | ガラス被膜形成方法 | |
| JPS6045704B2 (ja) | 表面処理防止方法 | |
| JPH10306362A (ja) | 溶融金属に対する耐食性および耐剥離性が優れた複合溶射皮膜を形成した溶融金属浴用部材 | |
| JPS5893865A (ja) | 表面処理防止方法 | |
| JPS5852462B2 (ja) | カナガタエンシンチユウゾウニオケル チルカボウシヨウバンド | |
| JPS6349744B2 (enExample) | ||
| JPS5754282A (ja) | Tainetsugokinnohyomenshorihoho | |
| JPS6220672A (ja) | 内燃機関の燃料弁アトマイザ | |
| US3446655A (en) | Method of producing refractory metal articles | |
| US3475141A (en) | Porcelain-enamel on galvanized steels by means of an aluminum coat | |
| EP0600471B1 (en) | An aluminum phosphate/silicon dioxide-based sealing material | |
| JP2567137B2 (ja) | 耐摩耗性ならびに耐溶融金属性に優れる複合皮膜被覆部材とその製造方法 | |
| JP2585548B2 (ja) | 気密性セラミック塗膜及びその製造方法 | |
| JP4863181B2 (ja) | 水素同位体透過防止用複合酸化物皮膜被覆部材及びその製造方法 | |
| JP2003041383A (ja) | 半導体製造装置用部材およびその製造方法 | |
| JPH0258347B2 (enExample) | ||
| JPS6028903B2 (ja) | 金属材料の表面処理方法 | |
| EP0602680A1 (en) | Potassium silicate-containing sealant |