JPS60258855A - ペ−スト式カドミウム負極の製造法 - Google Patents
ペ−スト式カドミウム負極の製造法Info
- Publication number
- JPS60258855A JPS60258855A JP59115943A JP11594384A JPS60258855A JP S60258855 A JPS60258855 A JP S60258855A JP 59115943 A JP59115943 A JP 59115943A JP 11594384 A JP11594384 A JP 11594384A JP S60258855 A JPS60258855 A JP S60258855A
- Authority
- JP
- Japan
- Prior art keywords
- cadmium
- metal
- plate
- metal cadmium
- nickel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/24—Electrodes for alkaline accumulators
- H01M4/26—Processes of manufacture
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP59115943A JPS60258855A (ja) | 1984-06-06 | 1984-06-06 | ペ−スト式カドミウム負極の製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP59115943A JPS60258855A (ja) | 1984-06-06 | 1984-06-06 | ペ−スト式カドミウム負極の製造法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS60258855A true JPS60258855A (ja) | 1985-12-20 |
| JPH03746B2 JPH03746B2 (forum.php) | 1991-01-08 |
Family
ID=14675010
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP59115943A Granted JPS60258855A (ja) | 1984-06-06 | 1984-06-06 | ペ−スト式カドミウム負極の製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS60258855A (forum.php) |
-
1984
- 1984-06-06 JP JP59115943A patent/JPS60258855A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPH03746B2 (forum.php) | 1991-01-08 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS60258855A (ja) | ペ−スト式カドミウム負極の製造法 | |
| JP2797554B2 (ja) | ニッケルカドミウム蓄電池 | |
| JPS60258854A (ja) | ペ−スト式カドミウム負極の製造法 | |
| JP2734149B2 (ja) | ペースト式カドミウム負極の製造法 | |
| JP2773253B2 (ja) | アルカリ蓄電池用カドミウム負極の製造法 | |
| JP2762730B2 (ja) | ニッケル―カドミウム蓄電池 | |
| JPS62136764A (ja) | ペ−スト式カドミウム負極の製造法 | |
| JPS63310565A (ja) | ペ−スト式カドミウム負極の製造方法 | |
| JPS617566A (ja) | ペ−スト式カドミウム負極の製造法 | |
| JP2529308B2 (ja) | アルカリ蓄電池用カドミウム負極の製造法 | |
| JP2754800B2 (ja) | ニッケルカドミウム蓄電池 | |
| JPH1064531A (ja) | アルカリ蓄電池用カドミウム負極およびその製造方法 | |
| JP3196234B2 (ja) | アルカリ蓄電池用カドミウム負極板とその製造方法 | |
| JP2771584B2 (ja) | 非焼結式密閉アルカリ蓄電池の製造方法 | |
| JP2773308B2 (ja) | ペースト式カドミウム負極の製造法 | |
| JPS617565A (ja) | ペ−スト式カドミウム負極 | |
| JPS60216449A (ja) | ペ−スト式カドミウム陰極板の製造方法 | |
| JPS61124057A (ja) | ペ−スト式カドミウム負極の製造法 | |
| JPH0668871A (ja) | 鉛蓄電池及びその製造方法 | |
| JPH09245827A (ja) | アルカリ蓄電池の製造法 | |
| JPS58158867A (ja) | 亜鉛極 | |
| JPS58137964A (ja) | アルカリ亜鉛蓄電池 | |
| JPH06124706A (ja) | 密閉形ニッケル−亜鉛蓄電池 | |
| JPS62136763A (ja) | ペ−スト式カドミウム負極の製造法 | |
| JPS63308870A (ja) | ペ−スト式カドミウム負極の製造法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| EXPY | Cancellation because of completion of term |