JPS59136338A - 熱可塑性合成樹脂成形用組成物 - Google Patents
熱可塑性合成樹脂成形用組成物Info
- Publication number
- JPS59136338A JPS59136338A JP1026583A JP1026583A JPS59136338A JP S59136338 A JPS59136338 A JP S59136338A JP 1026583 A JP1026583 A JP 1026583A JP 1026583 A JP1026583 A JP 1026583A JP S59136338 A JPS59136338 A JP S59136338A
- Authority
- JP
- Japan
- Prior art keywords
- fiber
- synthetic resin
- thermoplastic synthetic
- rock wool
- potassium titanate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Compositions Of Macromolecular Compounds (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1026583A JPS59136338A (ja) | 1983-01-25 | 1983-01-25 | 熱可塑性合成樹脂成形用組成物 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1026583A JPS59136338A (ja) | 1983-01-25 | 1983-01-25 | 熱可塑性合成樹脂成形用組成物 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS59136338A true JPS59136338A (ja) | 1984-08-04 |
| JPH0242104B2 JPH0242104B2 (enExample) | 1990-09-20 |
Family
ID=11745478
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1026583A Granted JPS59136338A (ja) | 1983-01-25 | 1983-01-25 | 熱可塑性合成樹脂成形用組成物 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS59136338A (enExample) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6281448A (ja) * | 1985-10-04 | 1987-04-14 | Mitsubishi Monsanto Chem Co | サ−モトロピツク液晶ポリマ−組成物およびその製造方法 |
-
1983
- 1983-01-25 JP JP1026583A patent/JPS59136338A/ja active Granted
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6281448A (ja) * | 1985-10-04 | 1987-04-14 | Mitsubishi Monsanto Chem Co | サ−モトロピツク液晶ポリマ−組成物およびその製造方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0242104B2 (enExample) | 1990-09-20 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN103740082B (zh) | 一种ul94-5va级的高性能阻燃增强pc/abs共混材料及其制备方法 | |
| CN102108206A (zh) | 高性能尼龙树脂/硫酸钙晶须复合材料及其制备方法 | |
| JPH0132855B2 (enExample) | ||
| CN111154248A (zh) | 一种高刚性增韧阻燃pc/abs材料及其制备方法 | |
| JPWO1999020446A1 (ja) | 繊維含有熱可塑性樹脂組成物の製造法 | |
| KR20210119701A (ko) | 자동차 부품용 재생 폴리프로필렌 복합소재의 제조방법 | |
| CN114045043B (zh) | 一种高抗冲木塑头盔复合材料及制备方法 | |
| JPS59136338A (ja) | 熱可塑性合成樹脂成形用組成物 | |
| JP2777690B2 (ja) | 樹脂組成物 | |
| JP5604114B2 (ja) | 成形品の製造方法、成形品および熱可塑性樹脂組成物 | |
| JPH0365311A (ja) | 炭素繊維チョップ | |
| JP3352121B2 (ja) | 長繊維強化ポリアミド樹脂組成物及びその成形品 | |
| CN111320869A (zh) | 一种3d打印耐高温环保无卤波纤增强尼龙6t耗材及其制备方法 | |
| CN117659545A (zh) | 一种高分子材料组合物及其制备和使用方法 | |
| CN112454721B (zh) | 一种圆柱状八溴醚颗粒的制备方法 | |
| CN111303650B (zh) | 利用回收渔网丝生产的汽车发动机罩盖专用材料 | |
| JPS59227936A (ja) | 複合強化ポリプロピレン組成物 | |
| JP2000336264A (ja) | リサイクル熱可塑性樹脂組成物 | |
| JP4514531B2 (ja) | 長繊維強化ポリアミド樹脂成形用組成物及び成形体の製造方法。 | |
| JPH0140061B2 (enExample) | ||
| JPH09296053A (ja) | 繊維強化熱可塑性樹脂成形品 | |
| JPH0517631A (ja) | 長繊維強化ポリオレフイン樹脂組成物 | |
| JPH10139927A (ja) | リサイクル樹脂組成物 | |
| JP2002241510A (ja) | 熱可塑性樹脂成形品及びその製造方法 | |
| JPH04225034A (ja) | ポリアミド樹脂薄物成形品の製造方法 |