JPS5896671A - 感圧性接着テ−プの製造方法 - Google Patents
感圧性接着テ−プの製造方法Info
- Publication number
- JPS5896671A JPS5896671A JP19413881A JP19413881A JPS5896671A JP S5896671 A JPS5896671 A JP S5896671A JP 19413881 A JP19413881 A JP 19413881A JP 19413881 A JP19413881 A JP 19413881A JP S5896671 A JPS5896671 A JP S5896671A
- Authority
- JP
- Japan
- Prior art keywords
- water
- weight
- parts
- acrylic copolymer
- acidic group
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Adhesive Tapes (AREA)
- Adhesives Or Adhesive Processes (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP19413881A JPS5896671A (ja) | 1981-12-02 | 1981-12-02 | 感圧性接着テ−プの製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP19413881A JPS5896671A (ja) | 1981-12-02 | 1981-12-02 | 感圧性接着テ−プの製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5896671A true JPS5896671A (ja) | 1983-06-08 |
| JPS6210591B2 JPS6210591B2 (enExample) | 1987-03-06 |
Family
ID=16319535
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP19413881A Granted JPS5896671A (ja) | 1981-12-02 | 1981-12-02 | 感圧性接着テ−プの製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5896671A (enExample) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS61254678A (ja) * | 1985-05-07 | 1986-11-12 | Nitto Electric Ind Co Ltd | エアゾ−ル型感圧性接着剤組成物 |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5046742A (enExample) * | 1973-08-21 | 1975-04-25 |
-
1981
- 1981-12-02 JP JP19413881A patent/JPS5896671A/ja active Granted
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5046742A (enExample) * | 1973-08-21 | 1975-04-25 |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS61254678A (ja) * | 1985-05-07 | 1986-11-12 | Nitto Electric Ind Co Ltd | エアゾ−ル型感圧性接着剤組成物 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6210591B2 (enExample) | 1987-03-06 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPH10513212A (ja) | 剥離のための水性(メタ)アクリルラテックスポリマー | |
| EP3650513B1 (en) | Water-based acrylic pressure-sensitive adhesive for clothing, and preparation method thereof | |
| KR102262503B1 (ko) | 아크릴계 에멀젼 수지의 제조 방법 | |
| HUT67716A (en) | Multi-component adhesive polymer composition and process for producing thereof | |
| JPS5837348B2 (ja) | 水分散型感圧接着剤組成物 | |
| JP4509279B2 (ja) | アクリル系感圧性接着剤の製造方法 | |
| JPH0684490B2 (ja) | 再剥離性粘着剤組成物 | |
| JPS61264077A (ja) | 水分散型感圧性接着剤組成物の製造法 | |
| JP4803916B2 (ja) | アクリル系感圧性接着剤及びその製造方法 | |
| DE4007637A1 (de) | Waessrige polymerisatdispersionen | |
| EP1016680B1 (en) | Acrylic pressure-sensitive adhesive composition and process for producing the same | |
| JP2610616B2 (ja) | 水分散型感圧性接着剤組成物 | |
| JP3142865B2 (ja) | 強粘着性エマルジョン型感圧接着剤の製造法 | |
| JPS5896671A (ja) | 感圧性接着テ−プの製造方法 | |
| JP3944890B2 (ja) | 剥離紙用アンダーコート剤 | |
| JP2831749B2 (ja) | 水性樹脂分散液 | |
| JPS5933602B2 (ja) | 感圧接着剤の製造方法 | |
| JPS6150516B2 (enExample) | ||
| JPS6345430B2 (enExample) | ||
| JP4146556B2 (ja) | 水分散型感圧性接着剤組成物とその製造方法およびその接着シ―ト類 | |
| JP2006008831A (ja) | 水性粘着剤組成物 | |
| JPS58167667A (ja) | 感圧性接着テ−プの製造方法 | |
| JP3748274B2 (ja) | 水系再剥離型感圧接着剤 | |
| JPH0339522B2 (enExample) | ||
| JPS59179676A (ja) | 感圧性接着テ−プの製造方法 |