JPS58193303A - 軟鉄系焼結部品の製造法 - Google Patents
軟鉄系焼結部品の製造法Info
- Publication number
- JPS58193303A JPS58193303A JP7702282A JP7702282A JPS58193303A JP S58193303 A JPS58193303 A JP S58193303A JP 7702282 A JP7702282 A JP 7702282A JP 7702282 A JP7702282 A JP 7702282A JP S58193303 A JPS58193303 A JP S58193303A
- Authority
- JP
- Japan
- Prior art keywords
- ferrous sintered
- less
- soft ferrous
- sintered material
- subjected
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。
め要約のデータは記録されません。
Description
【発明の詳細な説明】
磁気特性を要する軟鉄系材料は、柔かさと同時にねばさ
を有するため、切削時にむしれを発生し難削で加工精度
を上げることが困難である。軟鉄系焼結材についても同
様で、特に薄肉材に対する精度のよい加工が困難である
。
を有するため、切削時にむしれを発生し難削で加工精度
を上げることが困難である。軟鉄系焼結材についても同
様で、特に薄肉材に対する精度のよい加工が困難である
。
本発明は軟鉄系焼結材について、水蒸気中で加熱処理し
て空孔内にFe O等の酸化鉄の皮膜を形 3 成すると、被削性を悪化させず剛性を増し硬くなって切
削の際むしれにくくなるため、また外力に対し歪みにく
くなり薄肉部を有する部品等も精度よく加工できること
を見出したものである。
て空孔内にFe O等の酸化鉄の皮膜を形 3 成すると、被削性を悪化させず剛性を増し硬くなって切
削の際むしれにくくなるため、また外力に対し歪みにく
くなり薄肉部を有する部品等も精度よく加工できること
を見出したものである。
即ち本発明は、21%以下、co、3%以下、Ouコ%
以下の密度6.グ〜7.!;g/rsの軟鉄系焼結部品
に水蒸気中で加熱処理を行なった後、切削加工を施すも
のである。
以下の密度6.グ〜7.!;g/rsの軟鉄系焼結部品
に水蒸気中で加熱処理を行なった後、切削加工を施すも
のである。
次に実施例について説明する。
外径3Qvsm、内径117mm、幅コ3關の密度g
、 s g7bm3の焼結部品(組成:純鉄)を水蒸気
中で3!rOcに30分加熱処理した後、内径11gm
mに旋削加工仕上げした。寸法精度はo、oymm以下
であった。
、 s g7bm3の焼結部品(組成:純鉄)を水蒸気
中で3!rOcに30分加熱処理した後、内径11gm
mに旋削加工仕上げした。寸法精度はo、oymm以下
であった。
、これに対し水蒸気加熱処理を行なわずに旋削仕上げ加
工を行なったものはQ、/lnm程度以下に精度を上げ
ることはできなかった。
工を行なったものはQ、/lnm程度以下に精度を上げ
ることはできなかった。
本発明法によれば、VTR用マグネットケース、ステッ
プモーター用部品等を焼結材を用いて精度のよいものを
安価に提供でき乞。
プモーター用部品等を焼結材を用いて精度のよいものを
安価に提供でき乞。
Claims (2)
- (1)軟鉄系焼結部品に水蒸気中で加熱処理を施し空孔
内に酸化鉄の皮膜を生成せしめた後、切削加工すること
を特徴とする軟鉄系焼結部品の製造法。 - (2)軟鉄系焼結部品が薄肉部を有することを特徴とす
る特許請求の範囲(11項記載の軟鉄系焼結部品の製造
法。