JPS58125373A - 高速潜弧溶接法 - Google Patents
高速潜弧溶接法Info
- Publication number
- JPS58125373A JPS58125373A JP592782A JP592782A JPS58125373A JP S58125373 A JPS58125373 A JP S58125373A JP 592782 A JP592782 A JP 592782A JP 592782 A JP592782 A JP 592782A JP S58125373 A JPS58125373 A JP S58125373A
- Authority
- JP
- Japan
- Prior art keywords
- welding
- electrode
- submerged arc
- electrodes
- speed
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K9/00—Arc welding or cutting
- B23K9/18—Submerged-arc welding
- B23K9/186—Submerged-arc welding making use of a consumable electrodes
- B23K9/188—Submerged-arc welding making use of a consumable electrodes making use of several electrodes
Landscapes
- Engineering & Computer Science (AREA)
- Physics & Mathematics (AREA)
- Plasma & Fusion (AREA)
- Mechanical Engineering (AREA)
- Arc Welding In General (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP592782A JPS58125373A (ja) | 1982-01-20 | 1982-01-20 | 高速潜弧溶接法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP592782A JPS58125373A (ja) | 1982-01-20 | 1982-01-20 | 高速潜弧溶接法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS58125373A true JPS58125373A (ja) | 1983-07-26 |
| JPH0150507B2 JPH0150507B2 (enExample) | 1989-10-30 |
Family
ID=11624519
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP592782A Granted JPS58125373A (ja) | 1982-01-20 | 1982-01-20 | 高速潜弧溶接法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS58125373A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH02258168A (ja) * | 1988-08-31 | 1990-10-18 | Kawasaki Steel Corp | アーク溶接方法及び装置、並びにフラックスコアードワイヤ |
| US5140140A (en) * | 1990-11-15 | 1992-08-18 | Pollack Alex J | Method and apparatus of submerged arc welding with electrodes in tandem |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4837348A (enExample) * | 1971-09-14 | 1973-06-01 |
-
1982
- 1982-01-20 JP JP592782A patent/JPS58125373A/ja active Granted
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4837348A (enExample) * | 1971-09-14 | 1973-06-01 |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH02258168A (ja) * | 1988-08-31 | 1990-10-18 | Kawasaki Steel Corp | アーク溶接方法及び装置、並びにフラックスコアードワイヤ |
| US5140140A (en) * | 1990-11-15 | 1992-08-18 | Pollack Alex J | Method and apparatus of submerged arc welding with electrodes in tandem |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0150507B2 (enExample) | 1989-10-30 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4214141A (en) | Multiple electrode submerged arc welding method | |
| US2620423A (en) | Method of electric welding | |
| JP2006075904A (ja) | 高いワイヤスピードでのレーザー/migハイブリッド溶接方法。 | |
| US3790354A (en) | Welding arrangement of explosive-plated metal sheets | |
| US3036205A (en) | Covered arc welding electrode | |
| JPS58125373A (ja) | 高速潜弧溶接法 | |
| JPH0453617B2 (enExample) | ||
| JPS59110474A (ja) | ア−ク溶接方法 | |
| JPH0221911B2 (enExample) | ||
| JPS6333941B2 (enExample) | ||
| JPH0429470B2 (enExample) | ||
| JPS5823189B2 (ja) | ダイデンリユウ mig ア−クヨウセツホウ | |
| SU889351A1 (ru) | Неплав щийс электрод | |
| JPS61266185A (ja) | 2電極ミグ溶接法 | |
| JPS6247110B2 (enExample) | ||
| JP3300193B2 (ja) | 片面サブマージアーク溶接方法 | |
| JPS5492536A (en) | Submerged arc welding method | |
| JPH07112635B2 (ja) | ソリッドワイヤ | |
| JPS6239078B2 (enExample) | ||
| JPH09314335A (ja) | タンデムサブマージアーク溶接方法 | |
| SU1712093A1 (ru) | Способ сварки трехфазной дугой | |
| JPS5913575A (ja) | 2電極mag溶接法 | |
| JPS60145275A (ja) | 初層溶接法 | |
| SU706208A1 (ru) | Способ сварки конструкций из толстолистового проката | |
| JPS6157112B2 (enExample) |