JPH0150507B2 - - Google Patents
Info
- Publication number
- JPH0150507B2 JPH0150507B2 JP57005927A JP592782A JPH0150507B2 JP H0150507 B2 JPH0150507 B2 JP H0150507B2 JP 57005927 A JP57005927 A JP 57005927A JP 592782 A JP592782 A JP 592782A JP H0150507 B2 JPH0150507 B2 JP H0150507B2
- Authority
- JP
- Japan
- Prior art keywords
- welding
- electrode
- wire
- speed
- arc
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K9/00—Arc welding or cutting
- B23K9/18—Submerged-arc welding
- B23K9/186—Submerged-arc welding making use of a consumable electrodes
- B23K9/188—Submerged-arc welding making use of a consumable electrodes making use of several electrodes
Landscapes
- Engineering & Computer Science (AREA)
- Physics & Mathematics (AREA)
- Plasma & Fusion (AREA)
- Mechanical Engineering (AREA)
- Arc Welding In General (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP592782A JPS58125373A (ja) | 1982-01-20 | 1982-01-20 | 高速潜弧溶接法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP592782A JPS58125373A (ja) | 1982-01-20 | 1982-01-20 | 高速潜弧溶接法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS58125373A JPS58125373A (ja) | 1983-07-26 |
| JPH0150507B2 true JPH0150507B2 (enExample) | 1989-10-30 |
Family
ID=11624519
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP592782A Granted JPS58125373A (ja) | 1982-01-20 | 1982-01-20 | 高速潜弧溶接法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS58125373A (enExample) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0712540B2 (ja) * | 1988-08-31 | 1995-02-15 | 川崎製鉄株式会社 | アーク溶接方法及び装置、並びにフラックスコアードワイヤ |
| US5140140A (en) * | 1990-11-15 | 1992-08-18 | Pollack Alex J | Method and apparatus of submerged arc welding with electrodes in tandem |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4837348A (enExample) * | 1971-09-14 | 1973-06-01 |
-
1982
- 1982-01-20 JP JP592782A patent/JPS58125373A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS58125373A (ja) | 1983-07-26 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP0077640A1 (en) | Four-electrode submerged arc welding process | |
| JPH0150507B2 (enExample) | ||
| JPH11138266A (ja) | タンデムサブマージアーク溶接方法 | |
| JP2002219571A (ja) | 3電極アーク溶接制御方法 | |
| JPH0221911B2 (enExample) | ||
| JPH0453617B2 (enExample) | ||
| JP4224196B2 (ja) | 溶接ビード形状に優れた多電極サブマージアーク溶接方法 | |
| JPS5966978A (ja) | 多電極潜弧溶接法 | |
| JPS6247110B2 (enExample) | ||
| JPS6239078B2 (enExample) | ||
| JPS61266185A (ja) | 2電極ミグ溶接法 | |
| JPS6317587Y2 (enExample) | ||
| JPS6331305B2 (enExample) | ||
| JP2534853B2 (ja) | 高速ティグドレッシング法 | |
| JPH09314335A (ja) | タンデムサブマージアーク溶接方法 | |
| JPH0471782A (ja) | 高速サブマージドアーク溶接法 | |
| JPS6149787A (ja) | 高速連続仮付溶接方法 | |
| JPS5823189B2 (ja) | ダイデンリユウ mig ア−クヨウセツホウ | |
| JP3300193B2 (ja) | 片面サブマージアーク溶接方法 | |
| JPS6317588Y2 (enExample) | ||
| SU1712093A1 (ru) | Способ сварки трехфазной дугой | |
| JPH0429469B2 (enExample) | ||
| JPH0155074B2 (enExample) | ||
| JPS5841946B2 (ja) | Mig溶接における厚板溶接法 | |
| SU889351A1 (ru) | Неплав щийс электрод |