JPS58108661A - アルカリ電池用ニツケル電極の製造法 - Google Patents
アルカリ電池用ニツケル電極の製造法Info
- Publication number
- JPS58108661A JPS58108661A JP56208541A JP20854181A JPS58108661A JP S58108661 A JPS58108661 A JP S58108661A JP 56208541 A JP56208541 A JP 56208541A JP 20854181 A JP20854181 A JP 20854181A JP S58108661 A JPS58108661 A JP S58108661A
- Authority
- JP
- Japan
- Prior art keywords
- nickel
- paste
- kneading
- active material
- alkaline battery
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/24—Electrodes for alkaline accumulators
- H01M4/32—Nickel oxide or hydroxide electrodes
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56208541A JPS58108661A (ja) | 1981-12-22 | 1981-12-22 | アルカリ電池用ニツケル電極の製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56208541A JPS58108661A (ja) | 1981-12-22 | 1981-12-22 | アルカリ電池用ニツケル電極の製造法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS58108661A true JPS58108661A (ja) | 1983-06-28 |
| JPH0252387B2 JPH0252387B2 (enrdf_load_stackoverflow) | 1990-11-13 |
Family
ID=16557892
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP56208541A Granted JPS58108661A (ja) | 1981-12-22 | 1981-12-22 | アルカリ電池用ニツケル電極の製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS58108661A (enrdf_load_stackoverflow) |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5463230A (en) * | 1977-10-28 | 1979-05-22 | Matsushita Electric Industrial Co Ltd | Preparation of electrode for battery |
-
1981
- 1981-12-22 JP JP56208541A patent/JPS58108661A/ja active Granted
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5463230A (en) * | 1977-10-28 | 1979-05-22 | Matsushita Electric Industrial Co Ltd | Preparation of electrode for battery |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0252387B2 (enrdf_load_stackoverflow) | 1990-11-13 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR100386519B1 (ko) | 알칼리축전지용비소결식니켈극 | |
| JPWO2006064979A1 (ja) | アルカリ二次電池用ニッケル電極及びその製造方法並びにアルカリ二次電池 | |
| JPS58108661A (ja) | アルカリ電池用ニツケル電極の製造法 | |
| JP3188000B2 (ja) | 非焼結式ニッケル正極 | |
| JP3249398B2 (ja) | アルカリ蓄電池用非焼結式ニッケル極 | |
| JP3268989B2 (ja) | アルカリ蓄電池用ニッケル極 | |
| JPS58198856A (ja) | アルカリ蓄電池用カドミウム負極板の製造方法 | |
| JPH0793138B2 (ja) | 電池用正極板およびその製造方法 | |
| JP3397216B2 (ja) | ニッケル極板とその製造方法およびこれを用いたアルカリ蓄電池 | |
| JP3097238B2 (ja) | アルカリ蓄電池用陽極板 | |
| JPH03145058A (ja) | ペースト式ニッケル正極及びアルカリ蓄電池 | |
| JPH0410181B2 (enrdf_load_stackoverflow) | ||
| JPH0232750B2 (enrdf_load_stackoverflow) | ||
| JP2564172B2 (ja) | カドミウム負極板およびその負極板を用いたアルカリ二次電池 | |
| JP2577954B2 (ja) | カドミウム負極板およびアルカリ二次電池 | |
| JP4479136B2 (ja) | ニッケル電極材料の製造方法 | |
| JPH10188971A (ja) | アルカリ蓄電池用非焼結式ニッケル極 | |
| JPH07272723A (ja) | アルカリ蓄電池用ニッケル正極 | |
| JPS59151758A (ja) | ニツケル電極の製造法 | |
| JPS63310565A (ja) | ペ−スト式カドミウム負極の製造方法 | |
| JPS60146453A (ja) | アルカリ電池用ニツケル電極の製造法 | |
| JPS63310564A (ja) | ペ−スト式カドミウム負極の製造方法 | |
| JPS59132563A (ja) | 電池用ニツケル電極の製造法 | |
| JPS60170160A (ja) | 非焼結式ニツケル電極の製造法 | |
| WO2001004974A1 (en) | Non-sintered nickel electrode for alkaline storage battery |