JPS5782404A - Manufacture of sintered mo body - Google Patents

Manufacture of sintered mo body

Info

Publication number
JPS5782404A
JPS5782404A JP55158838A JP15883880A JPS5782404A JP S5782404 A JPS5782404 A JP S5782404A JP 55158838 A JP55158838 A JP 55158838A JP 15883880 A JP15883880 A JP 15883880A JP S5782404 A JPS5782404 A JP S5782404A
Authority
JP
Japan
Prior art keywords
particle size
powder
average particle
sintered
green compact
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP55158838A
Other languages
Japanese (ja)
Inventor
Koji Ishige
Tadashi Hayashi
Tadashi Morita
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toshiba Corp
Original Assignee
Toshiba Corp
Tokyo Shibaura Electric Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toshiba Corp, Tokyo Shibaura Electric Co Ltd filed Critical Toshiba Corp
Priority to JP55158838A priority Critical patent/JPS5782404A/en
Publication of JPS5782404A publication Critical patent/JPS5782404A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To obtain a sintered Mo body with superior machinability by compacting Mo powder having specified average particle size and sintering the green compact at a specified temp.
CONSTITUTION: Mo powder having 3W3.5μm average particle size is compacted into a prescribed shape after adding an org. binder as required. This green compact is sintered at 1800W1900°C in a reducing atmosphere for a prescribed time. The reason why the particle size of the Mo powder is restricted as mentioned above is that the machinability of the resulting sintered body is deteriorated in case of ≤3μm average particle size, and Mo powder having ≥3.5μm average particle size is difficultly freed of air during compacting, whereby the green compact is apt to crack.
COPYRIGHT: (C)1982,JPO&Japio
JP55158838A 1980-11-13 1980-11-13 Manufacture of sintered mo body Pending JPS5782404A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP55158838A JPS5782404A (en) 1980-11-13 1980-11-13 Manufacture of sintered mo body

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP55158838A JPS5782404A (en) 1980-11-13 1980-11-13 Manufacture of sintered mo body

Publications (1)

Publication Number Publication Date
JPS5782404A true JPS5782404A (en) 1982-05-22

Family

ID=15680497

Family Applications (1)

Application Number Title Priority Date Filing Date
JP55158838A Pending JPS5782404A (en) 1980-11-13 1980-11-13 Manufacture of sintered mo body

Country Status (1)

Country Link
JP (1) JPS5782404A (en)

Similar Documents

Publication Publication Date Title
JPS5681603A (en) Sintering method for green material of aluminum powder
JPS5782404A (en) Manufacture of sintered mo body
JPS57164958A (en) Manufacture of sintered high-alloy steel
JPS5712607A (en) Metallic mold for resin
JPS572861A (en) Manufacture of sintered product of cast iron powder
JPS552762A (en) Reducing-sintering method for high speed steel powder
JPS55164048A (en) Production of intermetallic compound ferromagnetic body
JPS55113862A (en) Horseshoe
JPS5690951A (en) Iron-base metal sintering method
JPS56139603A (en) Production of ferrosilicon sintered sheet material
JPS57108232A (en) Electrical contact material and its manufacture
JPS5782403A (en) Manufacture of sintered mo body
JPS5763658A (en) Manufacture of sintered machine parts with superior specific strength
ES460045A1 (en) Method of manufacturing sintered components
JPS5596616A (en) Method of manufacturing copper-substituted rare earth cobalt permanent magnet
JPS574341A (en) Hot forging method of powder
Tengzelius et al. Means to improve the dimensional tolerances of PM steel components
JPS54103708A (en) Method of sintering molybdenum
JPS6475604A (en) Method for molding aluminum alloy powder
JPS57187271A (en) Dot needle for writing
JPS5471004A (en) Method of producing sintered mineral excellent in strength to reduction
JPS57158351A (en) Composite sintered aluminum material and its manufacture
JPS5641301A (en) Manufacture of sintered body of tungsten
JPS5735601A (en) Sintering and forging method
JPS5333906A (en) Sintering method by compression molding