JPS5770061A - Continuous casting method for steel ingot - Google Patents

Continuous casting method for steel ingot

Info

Publication number
JPS5770061A
JPS5770061A JP14682080A JP14682080A JPS5770061A JP S5770061 A JPS5770061 A JP S5770061A JP 14682080 A JP14682080 A JP 14682080A JP 14682080 A JP14682080 A JP 14682080A JP S5770061 A JPS5770061 A JP S5770061A
Authority
JP
Japan
Prior art keywords
mold
bar
shell
outlet
heating elements
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP14682080A
Other languages
Japanese (ja)
Inventor
Atsumi Ono
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to JP14682080A priority Critical patent/JPS5770061A/en
Publication of JPS5770061A publication Critical patent/JPS5770061A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To obtain an ingot having smooth surfaces free from any surface defect by incorporating heating elements in the outlet side wall of a mold.
CONSTITUTION: A mold 1 has heating elements 2. In starting melting and casting, a dummy bar 5 is located at the bottom end of the mold 1, after which metallic granules 4 are supplied with a continuous supply device 3 for the same into the mold 1, where they are heated to melt. Under cooling with the cooling water 7 injected from spray nozzles 6, the bar 5 is lowered by pinch rolls 8. The solidified shell 10 of cast metal is formed by controlling the height of the molten metal 9 in the mold, the inside wall surface temp. at the outlet of the mold, the descending speed of the bar 5, and the supply rate of the granules 4. As the bar 5 descends, the shell 10 grows to form an ingot 11. At this time, it is important to control these in such a way that the molten metal 9 does not form the shell 10 along the side walls in the mold and forms the shell quickly in the outside of the mold outlet. To this end, the inside wall surface temp. at the mold outlet is maintained at above the solidifying temp. of the cast metal by the heating elements 2.
COPYRIGHT: (C)1982,JPO&Japio
JP14682080A 1980-10-22 1980-10-22 Continuous casting method for steel ingot Pending JPS5770061A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP14682080A JPS5770061A (en) 1980-10-22 1980-10-22 Continuous casting method for steel ingot

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP14682080A JPS5770061A (en) 1980-10-22 1980-10-22 Continuous casting method for steel ingot

Publications (1)

Publication Number Publication Date
JPS5770061A true JPS5770061A (en) 1982-04-30

Family

ID=15416263

Family Applications (1)

Application Number Title Priority Date Filing Date
JP14682080A Pending JPS5770061A (en) 1980-10-22 1980-10-22 Continuous casting method for steel ingot

Country Status (1)

Country Link
JP (1) JPS5770061A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH0259145A (en) * 1988-10-21 1990-02-28 O C C Co Ltd Method for continuously casting metal by heating mold

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH0259145A (en) * 1988-10-21 1990-02-28 O C C Co Ltd Method for continuously casting metal by heating mold

Similar Documents

Publication Publication Date Title
US3713479A (en) Direct chill casting of ingots
JPH0688106B2 (en) Horizontal continuous casting method for strip-shaped metal ingot and its equipment
FR2342112A1 (en) Continuously casting metals, esp. aluminium and its alloys at high spe - by partial heat extn. from melt before it enters mould (NL 26.8.77)
RU1819188C (en) Method and apparatus for cooling steel ingots at continuous casting
ES2001920A6 (en) Method for controlling early casting stage in continuous casting process.
JPS5770061A (en) Continuous casting method for steel ingot
JPS56109144A (en) Pour-casting method
US2747245A (en) Process for continuous casting of metal billets
WO1989003738A1 (en) A method and apparatus for the direct casting of metals to form elongated bodies
US4355680A (en) Method and apparatus for continuous casting of hollow articles
SU373087A1 (en) LIQUID CAST IRON CRYSTALLIZATION METHOD
JPS5592260A (en) Steel manufactured by continuous casting method and production thereof
JPS5581061A (en) Production of composite material for abrasion resistance through casting
US3422881A (en) Device for feeding molten metal into the peripheral groove of a continuous casting wheel for the production of metal bars or ingots
JPS5775261A (en) Continuous casting method for homogeneous alloy cast ingot
JPS5684157A (en) Horizontal continuous casting method of molten metal
JPS6153143B2 (en)
SU921671A1 (en) Apparatus for horisontal continuous casting
GB1313008A (en) Method of casting metals
JPS57160567A (en) Purifying method for metal
JPS5639163A (en) Production of steel ingot
JPS5797854A (en) Method for prevention of breakout of ingot in continuous casting
JPS5770059A (en) Direct cooling casting device for hollow casting
JPS5725278A (en) Manufacture of sound steel ingot and mold to be used for said purpose
JPS60115351A (en) Continuous casting method