JPS5738346A - Tempered glass container - Google Patents
Tempered glass containerInfo
- Publication number
- JPS5738346A JPS5738346A JP11011980A JP11011980A JPS5738346A JP S5738346 A JPS5738346 A JP S5738346A JP 11011980 A JP11011980 A JP 11011980A JP 11011980 A JP11011980 A JP 11011980A JP S5738346 A JPS5738346 A JP S5738346A
- Authority
- JP
- Japan
- Prior art keywords
- container
- org
- compressive stress
- stress layer
- glass container
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03C—CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03C17/00—Surface treatment of glass, not in the form of fibres or filaments, by coating
- C03C17/28—Surface treatment of glass, not in the form of fibres or filaments, by coating with organic material
- C03C17/32—Surface treatment of glass, not in the form of fibres or filaments, by coating with organic material with synthetic or natural resins
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11011980A JPS5738346A (en) | 1980-08-11 | 1980-08-11 | Tempered glass container |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11011980A JPS5738346A (en) | 1980-08-11 | 1980-08-11 | Tempered glass container |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5738346A true JPS5738346A (en) | 1982-03-03 |
Family
ID=14527510
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP11011980A Pending JPS5738346A (en) | 1980-08-11 | 1980-08-11 | Tempered glass container |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5738346A (ja) |
Cited By (9)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH06298549A (ja) * | 1993-04-08 | 1994-10-25 | Nitto Denzai Kk | ガラスの固定方法 |
JP2016500045A (ja) * | 2012-11-30 | 2016-01-07 | コーニング インコーポレイテッド | 向上した強度および向上した損傷耐久性を有するガラス製容器 |
US10117806B2 (en) | 2012-11-30 | 2018-11-06 | Corning Incorporated | Strengthened glass containers resistant to delamination and damage |
US10273049B2 (en) | 2012-06-28 | 2019-04-30 | Corning Incorporated | Delamination resistant glass containers with heat-tolerant coatings |
US10737973B2 (en) | 2012-02-28 | 2020-08-11 | Corning Incorporated | Pharmaceutical glass coating for achieving particle reduction |
US10899659B2 (en) | 2014-09-05 | 2021-01-26 | Corning Incorporated | Glass articles and methods for improving the reliability of glass articles |
US11007117B2 (en) | 2012-02-28 | 2021-05-18 | Corning Incorporated | Glass articles with low-friction coatings |
US11208348B2 (en) | 2015-09-30 | 2021-12-28 | Corning Incorporated | Halogenated polyimide siloxane chemical compositions and glass articles with halogenated polyimide siloxane low-friction coatings |
US11497681B2 (en) | 2012-02-28 | 2022-11-15 | Corning Incorporated | Glass articles with low-friction coatings |
Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS49101405A (ja) * | 1972-12-18 | 1974-09-25 | ||
JPS5141718A (en) * | 1974-10-08 | 1976-04-08 | Ishizuka Glass | Garasuseihinno kyokashorihoho |
JPS5556042A (en) * | 1978-10-20 | 1980-04-24 | Ishizuka Glass Ltd | Production of light-weight bottle having stable chemical durability and mechanical strength |
JPS5570510A (en) * | 1978-11-15 | 1980-05-28 | Kubota Ltd | Machining device |
-
1980
- 1980-08-11 JP JP11011980A patent/JPS5738346A/ja active Pending
Patent Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS49101405A (ja) * | 1972-12-18 | 1974-09-25 | ||
JPS5141718A (en) * | 1974-10-08 | 1976-04-08 | Ishizuka Glass | Garasuseihinno kyokashorihoho |
JPS5556042A (en) * | 1978-10-20 | 1980-04-24 | Ishizuka Glass Ltd | Production of light-weight bottle having stable chemical durability and mechanical strength |
JPS5570510A (en) * | 1978-11-15 | 1980-05-28 | Kubota Ltd | Machining device |
Cited By (28)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH06298549A (ja) * | 1993-04-08 | 1994-10-25 | Nitto Denzai Kk | ガラスの固定方法 |
US10737973B2 (en) | 2012-02-28 | 2020-08-11 | Corning Incorporated | Pharmaceutical glass coating for achieving particle reduction |
US11872189B2 (en) | 2012-02-28 | 2024-01-16 | Corning Incorporated | Glass articles with low-friction coatings |
US11786441B2 (en) | 2012-02-28 | 2023-10-17 | Corning Incorporated | Glass articles with low-friction coatings |
US11737951B2 (en) | 2012-02-28 | 2023-08-29 | Corning Incorporated | Glass articles with low-friction coatings |
US11939259B2 (en) | 2012-02-28 | 2024-03-26 | Corning Incorporated | Pharmaceutical glass coating for achieving particle reduction |
US11007117B2 (en) | 2012-02-28 | 2021-05-18 | Corning Incorporated | Glass articles with low-friction coatings |
US11497681B2 (en) | 2012-02-28 | 2022-11-15 | Corning Incorporated | Glass articles with low-friction coatings |
US11071689B2 (en) | 2012-02-28 | 2021-07-27 | Corning Incorporated | Glass articles with low-friction coatings |
US11020317B2 (en) | 2012-02-28 | 2021-06-01 | Corning Incorporated | Glass articles with low-friction coatings |
US10273048B2 (en) | 2012-06-07 | 2019-04-30 | Corning Incorporated | Delamination resistant glass containers with heat-tolerant coatings |
US10273049B2 (en) | 2012-06-28 | 2019-04-30 | Corning Incorporated | Delamination resistant glass containers with heat-tolerant coatings |
US11608290B2 (en) | 2012-06-28 | 2023-03-21 | Corning Incorporated | Delamination resistant glass containers with heat-tolerant coatings |
US10787292B2 (en) | 2012-06-28 | 2020-09-29 | Corning Incorporated | Delamination resistant glass containers with heat-tolerant coatings |
JP2019151551A (ja) * | 2012-11-30 | 2019-09-12 | コーニング インコーポレイテッド | 向上した強度および向上した損傷耐久性を有するガラス製容器 |
US10117806B2 (en) | 2012-11-30 | 2018-11-06 | Corning Incorporated | Strengthened glass containers resistant to delamination and damage |
US10813835B2 (en) | 2012-11-30 | 2020-10-27 | Corning Incorporated | Glass containers with improved strength and improved damage tolerance |
JP2020164418A (ja) * | 2012-11-30 | 2020-10-08 | コーニング インコーポレイテッド | 向上した強度および向上した損傷耐久性を有するガラス製容器 |
US11963927B2 (en) | 2012-11-30 | 2024-04-23 | Corning Incorporated | Glass containers with delamination resistance and improved damage tolerance |
JP2022063326A (ja) * | 2012-11-30 | 2022-04-21 | コーニング インコーポレイテッド | 向上した強度および向上した損傷耐久性を有するガラス製容器 |
US10786431B2 (en) | 2012-11-30 | 2020-09-29 | Corning Incorporated | Glass containers with delamination resistance and improved damage tolerance |
US10507164B2 (en) | 2012-11-30 | 2019-12-17 | Corning Incorporated | Glass containers with improved strength and improved damage tolerance |
US10307333B2 (en) | 2012-11-30 | 2019-06-04 | Corning Incorporated | Glass containers with delamination resistance and improved damage tolerance |
US10307334B2 (en) | 2012-11-30 | 2019-06-04 | Corning Incorporated | Glass containers with delamination resistance and improved damage tolerance |
US11951072B2 (en) | 2012-11-30 | 2024-04-09 | Corning Incorporated | Glass containers with improved strength and improved damage tolerance |
JP2016500045A (ja) * | 2012-11-30 | 2016-01-07 | コーニング インコーポレイテッド | 向上した強度および向上した損傷耐久性を有するガラス製容器 |
US10899659B2 (en) | 2014-09-05 | 2021-01-26 | Corning Incorporated | Glass articles and methods for improving the reliability of glass articles |
US11208348B2 (en) | 2015-09-30 | 2021-12-28 | Corning Incorporated | Halogenated polyimide siloxane chemical compositions and glass articles with halogenated polyimide siloxane low-friction coatings |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US3825142A (en) | Thermoplastic shielded glass bottle | |
EP0135635A1 (en) | Exercise dumb-bell | |
JPS55144544A (en) | Silica column for chromatograph | |
JPS5738346A (en) | Tempered glass container | |
JPS52109531A (en) | Titanium dioxide pigment composition and method of manufacturing same | |
JPS5765751A (en) | Highly electrically conductive resin composition and electrically conductive resin molded product therefrom | |
JPS5767036A (en) | Tempered glass container | |
JPS53115781A (en) | Manufacture of thermoplastic resin film of improved anti-fogging and non- blocking properties | |
JPS52104062A (en) | Production of surface protection film of electronic parts | |
JPS5738345A (en) | Tempered glass container | |
JPS56155031A (en) | Quenched tempered glass container | |
JPS55100501A (en) | Mirror plate | |
JPS5326877A (en) | Composite film for packaging | |
JPS51135593A (en) | Plastic squirt manufacturing process | |
JPS5573875A (en) | Excellently workable mn-plated steel material having pretreatment layer for painting | |
JPS5287427A (en) | Thermosetting powder form acrylic resin, manufacturing method thereof, and paint containg same | |
JPS56127637A (en) | Coating pretreating method of polyolefinic resin product | |
JPS5647565A (en) | Reflector | |
JPS5778466A (en) | Corrosionproof paint composition | |
JPS5718738A (en) | Surface-activated polyester molded article and its preparation | |
JPS5288813A (en) | Protective coating metallic tube | |
JPS54150078A (en) | Semiconductor device | |
JPS5513749A (en) | Foamable coating powder composition | |
JPS5512136A (en) | Coating composition | |
JPS5734137A (en) | Preparation of plastic film having excellent surface characteristics |