JPS56150459A - Continuous manufacture of coated soft small-size tube - Google Patents
Continuous manufacture of coated soft small-size tubeInfo
- Publication number
- JPS56150459A JPS56150459A JP5292380A JP5292380A JPS56150459A JP S56150459 A JPS56150459 A JP S56150459A JP 5292380 A JP5292380 A JP 5292380A JP 5292380 A JP5292380 A JP 5292380A JP S56150459 A JPS56150459 A JP S56150459A
- Authority
- JP
- Japan
- Prior art keywords
- small
- size tube
- tube
- size
- gas
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To continuously manufacture a coated soft small-size tube with excellent productivity by performing automatically annealing and the formation of cupper alloy film on the surface of the small-size tube molded of strip steel while transferring it in the direction of axis.
CONSTITUTION: A small-size tube 1 molded of a strip steel is passed through a strainer 3 and a guide roll 4, and then copper or a copper alloy wire 15 is melted and sprayed onto the surface of the small-size tube 1 through a flame-coating nozzle 17. The small-size tube 1 so treated is then passed through core tubes 10, 10', and 10", through a high-frequency induction heater 6a consisting of high-frequency heating coils 11a, 11b, and 11c, and further through a heating surface 6b provided with a resistance heating body 12 in such a way as to melt the powdery metal (e.g. Cu) adhered to the surface of the small-size tube in order to form a thin metal film on the whole surface of the tube. And, the small-size tube is sent to a cooling zone 7 where a nonoxidative protective gas, e.g., a modified heavy hydrocarbon gas, hydrogen gas, ammonia-decomposed gas, etc., is blown into the core tube 10" through an inlet 14 to cool the small-size tube.
COPYRIGHT: (C)1981,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP5292380A JPS56150459A (en) | 1980-04-23 | 1980-04-23 | Continuous manufacture of coated soft small-size tube |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP5292380A JPS56150459A (en) | 1980-04-23 | 1980-04-23 | Continuous manufacture of coated soft small-size tube |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS56150459A true JPS56150459A (en) | 1981-11-20 |
Family
ID=12928346
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP5292380A Pending JPS56150459A (en) | 1980-04-23 | 1980-04-23 | Continuous manufacture of coated soft small-size tube |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS56150459A (en) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH10251798A (en) * | 1997-03-12 | 1998-09-22 | Nisshin Steel Co Ltd | Copper plated steel sheet for double rolled pipe, excellent in copper penetration resistance and so on, and its production |
JPH11230481A (en) * | 1998-02-16 | 1999-08-27 | Mitsubishi Materials Corp | Manufacture of inner surface plated copper tube |
JP2017508872A (en) * | 2013-12-19 | 2017-03-30 | サンドヴィック マテリアルズ テクノロジー ドイチュラント ゲーエムベーハー | Annealing furnace and method for annealing steel strands |
-
1980
- 1980-04-23 JP JP5292380A patent/JPS56150459A/en active Pending
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH10251798A (en) * | 1997-03-12 | 1998-09-22 | Nisshin Steel Co Ltd | Copper plated steel sheet for double rolled pipe, excellent in copper penetration resistance and so on, and its production |
JPH11230481A (en) * | 1998-02-16 | 1999-08-27 | Mitsubishi Materials Corp | Manufacture of inner surface plated copper tube |
JP2017508872A (en) * | 2013-12-19 | 2017-03-30 | サンドヴィック マテリアルズ テクノロジー ドイチュラント ゲーエムベーハー | Annealing furnace and method for annealing steel strands |
US10400302B2 (en) | 2013-12-19 | 2019-09-03 | Sandvik Materials Technology Deutschland Gmbh | Annealing furnace and method for annealing a steel strand |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS57149462A (en) | High-speed hot-dip coating methode of wire material and apparatus therefor | |
GB1304616A (en) | ||
JPS55122820A (en) | Manufacture of alloyed zinc-plated high tensile steel sheet with superior workability | |
JPS56150459A (en) | Continuous manufacture of coated soft small-size tube | |
US3354864A (en) | Apparatus for coating metallic strands | |
US4551354A (en) | Method for metalizing metal bodies | |
JPS5579848A (en) | Copper alloy with superior strength, electric conductivity and softening resistance and manufacture thereof | |
US3511686A (en) | Method for annealing and coating metal strip | |
JPS6117351A (en) | Production of composite wire rod | |
JP2633363B2 (en) | Method and apparatus for melting and brightening steel strip with electric tin | |
US3526529A (en) | Method of producing high tensile strength aluminum coated ferrous strands | |
JPS5554522A (en) | Manufacture of hot dipped steel sheet with superior workability | |
Creps | Method for Galvanizing and Plastic Coating Steel | |
JPS5625951A (en) | High permeability alloy sheet | |
JPS57100846A (en) | Manufacture of alloy thin plate having high magnetic permeability of iron-cobalt-silicon compound | |
JPS5527410A (en) | Metal thin strip producing apparatus | |
ES436789A1 (en) | Continuous hot dip coating of small diameter strand | |
JPS5636318A (en) | Manufacture of steel pipe plated with molten metal | |
JPS57165164A (en) | Production of roll for continuous casting installation | |
JPS55141559A (en) | Treatment of bead cut part of welded pipe made of surface treated steel plate | |
JPS55109547A (en) | Sheet production | |
JPS5719358A (en) | Amorphous alloy containing iron group element and hafnium | |
JPS57123998A (en) | Treatment of molten tin of tin electroplated steel plate | |
JPS57210964A (en) | Hot dipping method using zn-al-sn alloy | |
JPS57100922A (en) | Preparation of plate glass |