JPS5583165A - Manufacturing method of positive electrode plate for alkaline cell - Google Patents
Manufacturing method of positive electrode plate for alkaline cellInfo
- Publication number
- JPS5583165A JPS5583165A JP15716678A JP15716678A JPS5583165A JP S5583165 A JPS5583165 A JP S5583165A JP 15716678 A JP15716678 A JP 15716678A JP 15716678 A JP15716678 A JP 15716678A JP S5583165 A JPS5583165 A JP S5583165A
- Authority
- JP
- Japan
- Prior art keywords
- nickel
- electrode plate
- manufacturing
- positive electrode
- compound
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To scheme to improve working performance and life characteristic by pulverizing minutely nickel cobalt compound which is obtained by anode-oxydizing nickel in acid bath containing cobalt salt and mixing electric conductive material with said nickel cobalt compound to form electrode plate.
CONSTITUTION: Nickel cobalt compound is obtained by anode-oxydizing nickel in acid bath containing cobalt salt. After pulverizing minutely said compound, electric coductive materials such as black lead or nickel are mixed with and pressing- molded, and an electrode plate is obtained.
COPYRIGHT: (C)1980,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15716678A JPS5583165A (en) | 1978-12-19 | 1978-12-19 | Manufacturing method of positive electrode plate for alkaline cell |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15716678A JPS5583165A (en) | 1978-12-19 | 1978-12-19 | Manufacturing method of positive electrode plate for alkaline cell |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5583165A true JPS5583165A (en) | 1980-06-23 |
Family
ID=15643623
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP15716678A Pending JPS5583165A (en) | 1978-12-19 | 1978-12-19 | Manufacturing method of positive electrode plate for alkaline cell |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5583165A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS58121558A (en) * | 1982-01-13 | 1983-07-19 | Japan Storage Battery Co Ltd | Alkaline battery |
WO2006106624A1 (en) * | 2005-03-31 | 2006-10-12 | Mitsui Mining & Smelting Co., Ltd. | Composite oxide particle having black color |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6144380A (en) * | 1984-08-06 | 1986-03-04 | Mitsubishi Electric Corp | Radar equipment |
-
1978
- 1978-12-19 JP JP15716678A patent/JPS5583165A/en active Pending
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6144380A (en) * | 1984-08-06 | 1986-03-04 | Mitsubishi Electric Corp | Radar equipment |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS58121558A (en) * | 1982-01-13 | 1983-07-19 | Japan Storage Battery Co Ltd | Alkaline battery |
WO2006106624A1 (en) * | 2005-03-31 | 2006-10-12 | Mitsui Mining & Smelting Co., Ltd. | Composite oxide particle having black color |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
EP0008430A3 (en) | Mixed oxides for the electrodes of electrochemical high temperature cells with solid electrolyte, and process for their manufacture | |
Öjefors | Self-discharge of the alkaline iron electrode | |
JPS5583165A (en) | Manufacturing method of positive electrode plate for alkaline cell | |
JPS5553074A (en) | Solid electrolyte cell | |
JPS5524331A (en) | Nickel-cadmium alkaline cell | |
JPS5581466A (en) | Positive electrode plate for alkaline storage battery | |
JPS5678072A (en) | Positive plate for alkaline storage battery | |
JPS5740870A (en) | Solid electrolyte battery | |
JPS5576569A (en) | Cadmium cathode plate for enclosed type alkali battery | |
JPS57107568A (en) | Reversible copper electrode | |
IE57059B1 (en) | Process for the production of anode active materials for use in cells | |
KR880002217B1 (en) | Alkali battery pole infixed manufacture method | |
SU111360A1 (en) | Paste for the negative electrode of a lead starter battery | |
JPS5546288A (en) | Nonaqueous electrolytic cell | |
JPS57165961A (en) | Production of cadmium electrode for alkaline cell | |
JPS57101345A (en) | Alkaline battery | |
JPS57101346A (en) | Alkaline battery | |
JPS5279690A (en) | Electromic display cell | |
JPS55113278A (en) | Water-injecting type air battery | |
JPS5659463A (en) | Battery | |
JPS5686458A (en) | Manufacture of alkaline cell | |
JPS5595277A (en) | Lithium-bromine complex cell | |
JPS57212772A (en) | Manufacture of paste for lead storage battery electrode plate | |
JPS57170458A (en) | Manufacture of cadmium negative electrode for battery | |
JPS5750769A (en) | Oxygen electrode for battery |