JPS55119124A - Manufacture of low yield ratio nonheat-treated high tensile steel plate - Google Patents
Manufacture of low yield ratio nonheat-treated high tensile steel plateInfo
- Publication number
- JPS55119124A JPS55119124A JP2791179A JP2791179A JPS55119124A JP S55119124 A JPS55119124 A JP S55119124A JP 2791179 A JP2791179 A JP 2791179A JP 2791179 A JP2791179 A JP 2791179A JP S55119124 A JPS55119124 A JP S55119124A
- Authority
- JP
- Japan
- Prior art keywords
- steel plate
- yield ratio
- slab
- low yield
- manufacture
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To manufacture a high tensile steel plate with a low yield ratio stably at a low cost by a method wherein the heating temperature and rolling conditions of the slab of low alloy steel containing an extremely small quantity of boron are controlled when the slab is hot-rolled and worked to a steel plate. CONSTITUTION:The slab of low alloy steel containing one kind or two kinds or more among 0.11-0.35% C, 0.05-0.90% Si, 0.75-2.50% Mn, 0.05-0.80% Mo, 0.01-0.08% Nb, 0.03-0.15% sol.Al, 0.0002-0.0015% B, 0.10-2.00% Cu, 0.10-2.50% Ni, 0.10-2.50% Cr, 0.01-0.10% V is heated below 1,150 deg.C. The slab is formed in a steel plate with fixed thickness by applying the rolling of the quantity of distortion due to the working of the thickness decrease of at least 30% at the temperatures of 900 deg.C or less and cooled as it is. The steel plate is tempering-treated at 550 deg.C or less as necessary. The steel plate being obtained having low carbon equivalent, is excellent in strength and toughness and possesses a low yield ratio.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2791179A JPS55119124A (en) | 1979-03-09 | 1979-03-09 | Manufacture of low yield ratio nonheat-treated high tensile steel plate |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2791179A JPS55119124A (en) | 1979-03-09 | 1979-03-09 | Manufacture of low yield ratio nonheat-treated high tensile steel plate |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS55119124A true JPS55119124A (en) | 1980-09-12 |
JPH0112814B2 JPH0112814B2 (en) | 1989-03-02 |
Family
ID=12234056
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP2791179A Granted JPS55119124A (en) | 1979-03-09 | 1979-03-09 | Manufacture of low yield ratio nonheat-treated high tensile steel plate |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS55119124A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS58164760A (en) * | 1982-03-25 | 1983-09-29 | Sumitomo Metal Ind Ltd | Stainless clad steel plate for pressure vessel |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH05280110A (en) * | 1991-08-30 | 1993-10-26 | Kazuo Tsukada | Wall construction in two-by-four method housing |
-
1979
- 1979-03-09 JP JP2791179A patent/JPS55119124A/en active Granted
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS58164760A (en) * | 1982-03-25 | 1983-09-29 | Sumitomo Metal Ind Ltd | Stainless clad steel plate for pressure vessel |
Also Published As
Publication number | Publication date |
---|---|
JPH0112814B2 (en) | 1989-03-02 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
SE8307123D0 (en) | METHOD OF MANUFACTURING HIGH TENSILE STRENGTH STEEL PLATES | |
GB1009924A (en) | Steel alloys and methods of making same | |
JPS5597425A (en) | Preparation of high-tensile steel with low yield ratio, low carbon and low alloy | |
JPS55131125A (en) | Production of unmodified high-strength high-toughness steel | |
JPS5576020A (en) | Production of steel plate stable in strength and toughness by direct hardening and tempering | |
JPS5651532A (en) | Production of high-strength zinc hot dipped steel plate of superior workability | |
CN101812634A (en) | Low-carbon low-welding crack-sensitive high-strength steel and steel plate and manufacture method thereof | |
JPS6415320A (en) | Production of high tensile steel for low temperature use having excellent toughness of weld zone | |
JPS55119124A (en) | Manufacture of low yield ratio nonheat-treated high tensile steel plate | |
JPS6468422A (en) | Production of high tensile steel plate for building | |
JPS55131126A (en) | Production of modified by low alloy containing boron high tensile steel plate | |
JPS5442326A (en) | Production of high-ductile, high-tensile normalized steel plate having decreased rolling anisotropy | |
JPS57210915A (en) | Manufacture of refined high tensile steel with high toughness | |
JPS5589432A (en) | Preraration of high tensile wire material and bar steel with excellent strain and corrosion crack resistance | |
JPS6462415A (en) | Production of high-tensile unequal-sided unequal thickness steel shape | |
SE7704046L (en) | WAY TO PRODUCE HOGHALL FIXED STEEL PLATE WHICH HAS AN EXCELLENT LAYER TEMPERATURE STRENGTH AND A STRETCH LIMIT OF AT LEAST 40 KP / MMŸ2 | |
JPS5457418A (en) | Manufacture of high toughness, refined steel | |
JPS5538979A (en) | Manufacture of low yield point, high tensile hot rolled steel plate with superior workability | |
JPS6425915A (en) | Manufacture of ferritic structural member for fast reactor core | |
JPS55131130A (en) | Production of high strength steel material having low yield ratio | |
JPS55104427A (en) | Production of steel for low temperature | |
JPS6468421A (en) | Production of high-tensile steel plate for construction | |
JPS5465115A (en) | Boron-added high tensile steel with superior low temperature toughness | |
JPS5675520A (en) | Manufacture of high yield ratio type nonskin-pass hot rolled high tensile steel plate | |
JPS5779117A (en) | Production of ultrathick temper type high tensile steel |