JPS5429979B2 - - Google Patents
Info
- Publication number
- JPS5429979B2 JPS5429979B2 JP2058974A JP2058974A JPS5429979B2 JP S5429979 B2 JPS5429979 B2 JP S5429979B2 JP 2058974 A JP2058974 A JP 2058974A JP 2058974 A JP2058974 A JP 2058974A JP S5429979 B2 JPS5429979 B2 JP S5429979B2
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C25—ELECTROLYTIC OR ELECTROPHORETIC PROCESSES; APPARATUS THEREFOR
- C25D—PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C25D11/00—Electrolytic coating by surface reaction, i.e. forming conversion layers
- C25D11/36—Phosphatising
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Chemical Treatment Of Metals (AREA)
- Electroplating Methods And Accessories (AREA)
- Electrochemical Coating By Surface Reaction (AREA)
Priority Applications (3)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2058974A JPS5429979B2 (fr) | 1974-02-22 | 1974-02-22 | |
DE19752505836 DE2505836A1 (de) | 1974-02-22 | 1975-02-12 | Verfahren zur oberflaechenbehandlung von rostfreien legierten staehlen |
FR7505638A FR2262134A1 (en) | 1974-02-22 | 1975-02-24 | Electrolytic treatment of stainless steel surfaces - with an acid phosphating solution contg. a chelating cpd. |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2058974A JPS5429979B2 (fr) | 1974-02-22 | 1974-02-22 |
Related Child Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP7385880A Division JPS55161073A (en) | 1980-06-02 | 1980-06-02 | Surface treatment of corrosion resistant alloy steel |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS50115138A JPS50115138A (fr) | 1975-09-09 |
JPS5429979B2 true JPS5429979B2 (fr) | 1979-09-27 |
Family
ID=12031410
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP2058974A Expired JPS5429979B2 (fr) | 1974-02-22 | 1974-02-22 |
Country Status (3)
Country | Link |
---|---|
JP (1) | JPS5429979B2 (fr) |
DE (1) | DE2505836A1 (fr) |
FR (1) | FR2262134A1 (fr) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2011231408A (ja) * | 2007-02-27 | 2011-11-17 | Kos Ltd | 燐酸塩皮膜冷間圧造用のステンレス鋼線及びそれを利用した直結ネジ |
Families Citing this family (11)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH01100281A (ja) * | 1987-10-13 | 1989-04-18 | Nippon Parkerizing Co Ltd | 金属表面の皮膜化成処理液 |
JPH0778280B2 (ja) * | 1988-07-28 | 1995-08-23 | 株式会社日立製作所 | 金属の防食表面処理方法 |
JPH0768638B2 (ja) * | 1988-11-02 | 1995-07-26 | 株式会社日立製作所 | 金属の防食表面処理方法 |
US5205921A (en) * | 1991-02-04 | 1993-04-27 | Queen's University At Kingston | Method for depositing bioactive coatings on conductive substrates |
DE4111186A1 (de) * | 1991-04-06 | 1992-10-08 | Henkel Kgaa | Verfahren zum phosphatieren von metalloberflaechen |
DK173338B1 (da) * | 1996-08-29 | 2000-07-31 | Danfoss As | Fremgangsmåde til elektrokemisk phosphatering af metaloverflader, især af rustfrit stål, med CaZnPO4 ved koldflydning af me |
JP2000144494A (ja) * | 1998-09-11 | 2000-05-26 | Nippon Parkerizing Co Ltd | 冷間圧造用の潤滑皮膜を形成する方法 |
DE102005023023B4 (de) | 2005-05-19 | 2017-02-09 | Chemetall Gmbh | Verfahren zur Vorbereitung von metallischen Werkstücken zum Kaltumformen, mit dem Verfahren beschichtete Werkstücke und ihre Verwendung |
WO2016120669A1 (fr) | 2015-01-30 | 2016-08-04 | Arcelormittal | Procédé de préparation d'une tôle revêtue comprenant l'application d'une solution aqueuse comprenant un aminoacide et utilisation associée pour améliorer la résistance à la corrosion |
WO2016120670A1 (fr) | 2015-01-30 | 2016-08-04 | Arcelormittal | Procédé de préparation d'une tôle revêtue comprenant l'application d'une solution aqueuse comprenant un aminoacide et utilisation associée pour améliorer la compatibilité avec un adhésif |
WO2016120671A1 (fr) | 2015-01-30 | 2016-08-04 | Arcelormittal | Procédé de préparation d'une tôle revêtue comprenant l'application d'une solution aqueuse comprenant un aminoacide et utilisation associée pour améliorer les propriétés tribologiques |
Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US1041761A (en) * | 1911-11-02 | 1912-10-22 | William W Evans | Means for feeding air to furnaces. |
US1856261A (en) * | 1929-01-26 | 1932-05-03 | Gen Motors Corp | Coating surfaces of iron or steel |
JPS4884746A (fr) * | 1972-02-15 | 1973-11-10 |
-
1974
- 1974-02-22 JP JP2058974A patent/JPS5429979B2/ja not_active Expired
-
1975
- 1975-02-12 DE DE19752505836 patent/DE2505836A1/de active Pending
- 1975-02-24 FR FR7505638A patent/FR2262134A1/fr active Granted
Patent Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US1041761A (en) * | 1911-11-02 | 1912-10-22 | William W Evans | Means for feeding air to furnaces. |
US1856261A (en) * | 1929-01-26 | 1932-05-03 | Gen Motors Corp | Coating surfaces of iron or steel |
JPS4884746A (fr) * | 1972-02-15 | 1973-11-10 |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2011231408A (ja) * | 2007-02-27 | 2011-11-17 | Kos Ltd | 燐酸塩皮膜冷間圧造用のステンレス鋼線及びそれを利用した直結ネジ |
Also Published As
Publication number | Publication date |
---|---|
FR2262134A1 (en) | 1975-09-19 |
DE2505836A1 (de) | 1975-09-04 |
JPS50115138A (fr) | 1975-09-09 |
FR2262134B1 (fr) | 1979-03-16 |