JPH09213140A - 薄肉難燃性電線 - Google Patents

薄肉難燃性電線

Info

Publication number
JPH09213140A
JPH09213140A JP8003498A JP349896A JPH09213140A JP H09213140 A JPH09213140 A JP H09213140A JP 8003498 A JP8003498 A JP 8003498A JP 349896 A JP349896 A JP 349896A JP H09213140 A JPH09213140 A JP H09213140A
Authority
JP
Japan
Prior art keywords
flame
electric wire
coupling agent
retardant
heat resistance
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP8003498A
Other languages
English (en)
Inventor
Shigeru Kashiwazaki
茂 柏崎
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hitachi Cable Ltd
Original Assignee
Hitachi Cable Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hitachi Cable Ltd filed Critical Hitachi Cable Ltd
Priority to JP8003498A priority Critical patent/JPH09213140A/ja
Publication of JPH09213140A publication Critical patent/JPH09213140A/ja
Pending legal-status Critical Current

Abstract

(57)【要約】 【課題】耐電圧特性を大幅に改善した薄肉難撚性電線を
得ること。 【解決手段】耐熱性が300℃以上のシランカップリン
グ剤あるいはチタネートカップリング剤によって表面処
理したハロゲン系難燃剤および耐熱性が300℃以上の
シランカップリング剤あるいはチタネートカップリング
剤によって表面処理した無機系難燃助剤を含有せしめた
ポリエチレンコンパウンドを用い、被覆厚さが200μ
m以下となるように絶縁被覆して構成。

Description

【発明の詳細な説明】
【0001】
【発明の属する技術分野】本発明は、薄肉の難燃性電線
に関し、特に、耐電圧特性を改善した薄肉難燃性電線に
関するものである。
【0002】
【従来の技術】近年、電気機器や電子機器の小型化、省
スペース化の傾向が著しく、これらに使用される電線・
ケーブルに対する細径化への要請も益々強まってきてい
る。
【0003】電線を細径化するには、必然的に導体を細
くし、絶縁体厚さを薄くする必要がある。
【0004】一方、上記機器は小型化に伴う過密配線の
傾向にあり、そのように配線される電線・ケーブルの難
燃化が重要な課題として浮上している。
【0005】通常、1mm径以上の電線には、絶縁体材料
として誘電率が小さく電気特性の優れているポリエチレ
ンが使用されている。そして、上記電気機器、電子機器
に配線される難燃性電線としては、可撓性を付与して配
線作業を容易にするため、例えば低密度ポリエチレンに
ハロゲン系難燃剤と三酸化アンチモンを添加した難燃性
絶縁組成物を絶縁体として被覆したものが一般に使用さ
れてきた。
【0006】
【発明が解決しようとする課題】上記した電線の細径化
の要請から、電線の外形を1mm以下とし、被覆される絶
縁体厚さも200μm以下とする必要がある。
【0007】しかし、このような薄肉細径の電線に上記
従来組成の難燃性絶縁組成物を被覆したところ、絶縁破
壊を起す確立が極端に増加することが判明した。
【0008】本発明の目的は、上記したような実情に鑑
み、耐電圧特性を大幅に改善し得る新規な薄肉難燃性電
線を提供しようとするものである。
【0009】
【課題を解決するための手段】本発明は、被覆する絶縁
材料として、耐熱性が300℃以上のシランカップリン
グ剤あるいはチタネートカップリング剤によって表面処
理したハロゲン系難燃剤および耐熱性が300℃以上の
シランカップリング剤あるいはチタネートカップリング
剤によって表面処理した無機系難燃助剤を含有せしめた
ポリエチレンコンパウンドを用いたものである。
【0010】
【発明の実施の形態】本発明において、ハロゲン系難燃
剤としては臭素系難燃剤のヘキサブロモビフェニールエ
ーテル、デカブロモビフェニルエーテル、ヘキサブロモ
シクロドデカン、ビス(ブロモエチルエーテル)テトラ
ブロモビスフェノールA、ヘキサブロモベンゼン、ヘキ
サブロモビフェニル、テトラブロモビスフェノールS、
ピロガードSP103(第一工業製薬(株)製)、ピロ
ガードSR700(第一工業製薬(株)製)、ファイヤ
ガード3000(帝人化成(株)製)、サイテックスB
T93(サイテックス社製)等、また、塩素系難燃剤の
デクロランプラス315、デクロランプラス25、デク
ロランプラス2520、デクロラン603、デクロラン
604(いずれもフッカーケミカル社製)等があげられ
るが、これらに限るものではない。ただし、塩素化パラ
フィン、塩素化ポリエチレンは除かれる。無機系難燃助
剤としては三酸化アンチモン、五酸化アンチモン、シリ
カ、NaSbO3 、酸化スズ、水酸化スズ、酸化モリブ
テン、モリブテン酸アンモニウム、酸化ジルコニウム、
水酸化ジルコニウム等があげられる。
【0011】本発明に使用される耐熱性が300℃以上
のシランカップリング剤とは、空気中で熱天秤によって
5℃/分の速度で昇温したとき重量減少が25%になる
ときの温度が300℃以上であるものをいう。
【0012】このようなシランカップリング剤として
は、例えばPetrarch System社より入手可能なα(2−
アミノエチル)−アミノプロピルトリメトキシシラン
(商品名AAS−M)、α−クロロプロピルトリメトキ
シシシラン(商品名CPS−M)、α−メタクリルオキ
シプロピルトリメトキシシラン(商品名MOPS−
M)、N,N−ジメチルアミノフェニルトリエトキシシ
ラン(商品名D−5190)、トリル−トリメトキシシ
ラン、トリメトキシシリル安息香酸、クロロメチルフェ
ネチルトリメトキシシラン(商品名Tー2902)、2
−スチリルエチルトリメトキシシラン(商品名PSX0
83)、アミノエチルアミノメチルフェネチルトリメト
キシシラン(商品名PSX084)などをあげることが
できるが、これらに限定されるものではない。
【0013】一方、耐熱性が300℃以下のシランカッ
プリング剤は押出加工時に気泡を生じるために好ましく
ない。
【0014】本発明に使用されるチタネートカップリン
グ剤としては、例えば味の素(株)より入手可能なイソ
プロピルトリイソステアロイルチタネート(商品名TT
S)、イソプロピルトリドデシルベンゼンスルホニルチ
タネート(商品名9S)、イソプロピルトリス(ジオク
チルパイロホスフェート)チタネート(商品名38
S)、テトライソプロピルビス(ジオクチルホスファイ
ト)チタネート(商品名41B)、テトラオクチルビス
(ジトリデシルホスファイト)チタネート(商品名46
B)、テトラ(2,2−ジアリルオキシメチル−1−ブ
チル)ビス(ジ−トリデシル)ホスファイトチタネート
(商品名55)、ビス(ジオクチルパイロホスフェー
ト)オキシアセテートチタネート(商品名138S)お
よびトリス(ジオクチルパイロホスフェート)エチレン
チタネート(商品名238S)などをあげることができ
るが、これらに限るものではない。
【0015】ポリエチレンを難燃化するには、ハロゲン
系難燃剤と無機系難燃助剤を併用する必要があり、この
場合、これらを5〜70重量%、好ましくは15〜25
重量%含有させるのが一般的である。
【0016】シランカップリング剤あるいはチタネート
カップリング剤は、難燃剤(ハロゲン系難燃剤+無機系
難燃助剤)100重量部に対して0.1〜5重量部、好
ましくは0.2〜2重量部使用するのが一般的である。
【0017】シランカップリング剤あるいはチタネート
カップリング剤で処理した難燃剤を使用することによ
り、ポリマと難燃剤界面との間に生じる空隙が大幅に減
少し、耐電圧特性が改善されるものと考えられる。
【0018】
【実施例】以下に本発明の実施例および比較例を説明す
る。
【0019】外径0.12mmのスズメッキ銅線を7本撚
り合わせた導体上に40mm押出機を用いて表1及び表2
の実施例及び比較例に示す組成の難燃ポリエチレンコン
パウンドを、絶縁厚が100μmとなるように押出被覆
し、外径0.52mmの電線を作製し各供試試料とした。
なお、ポリエチレンは三井デュポンケミカル(株)のミ
ラソン3530〔融点111℃、降伏点応力(JISK
−6760に準拠)135kg/cm2 、メルトインデック
ス0.3〕を使用した。
【0020】各供試試料についての耐電圧試験結果を表
1及び表2に併記した。耐電圧試験は、電線押出時に2
kVの数珠玉高周波スパークテスタを用いて5000m当
たりのスパーク抜け回数を測定した。
【0021】
【表1】
【0022】
【表2】
【0023】表1および表2から明らかなように、実施
例は、シランカップリング剤またはチタネートカップリ
ング剤を添加したものであり、スパーク抜けがゼロであ
る。比較例1は、耐熱性が300℃に達しないシランカ
ップリング剤を使用したものであり、スパーク抜けが発
生している。比較例2、3はシランカップリング剤およ
びチタネートカップリング剤のいずれをも添加しなかっ
たものであり、スパーク抜けの発生数が極めて多くなっ
ている。
【0024】
【発明の効果】以上説明した通り、本発明によれば、薄
肉の難燃性細径電線において、従来特に問題となる欠点
であった耐電圧特性を大幅に向上させることができ、外
径1mm以下でかつ絶縁厚200μm以下の難燃性電線
を高信頼性をもって市場に供給することが可能になるも
のである。
───────────────────────────────────────────────────── フロントページの続き (51)Int.Cl.6 識別記号 庁内整理番号 FI 技術表示箇所 H01B 3/44 H01B 3/44 F

Claims (1)

    【特許請求の範囲】
  1. 【請求項1】耐熱性が300℃以上のシランカップリン
    グ剤あるいはチタネートカップリング剤によって表面処
    理したハロゲン系難燃剤および耐熱性が300℃以上の
    シランカップリング剤あるいはチタネートカップリング
    剤によって表面処理した無機系難燃助剤を含有せしめた
    ポリエチレンコンパウンドを用い、被覆厚さが200μ
    m以下となるように絶縁被覆してなる薄肉難燃性電線。
JP8003498A 1996-01-12 1996-01-12 薄肉難燃性電線 Pending JPH09213140A (ja)