JPH0693467A5 - - Google Patents
Info
- Publication number
- JPH0693467A5 JPH0693467A5 JP4-244796A JP24479692A JPH0693467A5 JP H0693467 A5 JPH0693467 A5 JP H0693467A5 JP 24479692 A JP24479692 A JP 24479692A JP H0693467 A5 JPH0693467 A5 JP H0693467A5
- Authority
- JP
- Japan
- Prior art keywords
- document
- procedural amendment
- rust
- correction
- amended
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP4244796A JP2884941B2 (ja) | 1992-07-27 | 1992-09-14 | 耐候性に優れた鋼材および錆層の形成方法 |
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP19970192 | 1992-07-27 | ||
| JP4-199701 | 1992-07-27 | ||
| JP4244796A JP2884941B2 (ja) | 1992-07-27 | 1992-09-14 | 耐候性に優れた鋼材および錆層の形成方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH0693467A JPH0693467A (ja) | 1994-04-05 |
| JPH0693467A5 true JPH0693467A5 (enExample) | 1997-02-04 |
| JP2884941B2 JP2884941B2 (ja) | 1999-04-19 |
Family
ID=26511700
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP4244796A Expired - Lifetime JP2884941B2 (ja) | 1992-07-27 | 1992-09-14 | 耐候性に優れた鋼材および錆層の形成方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP2884941B2 (enExample) |
Families Citing this family (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE3783368T2 (de) * | 1987-05-29 | 1993-07-08 | Minolta Camera Kk | Automatisiertes bildvervielfaeltigungsgeraet. |
| KR100319302B1 (ko) | 1999-02-25 | 2002-01-04 | 구마모토 마사히로 | 내식성(耐食性)이 우수한 강재 및 이 강재를 이용한 구조물 |
| JP4513178B2 (ja) * | 1999-10-05 | 2010-07-28 | Jfeスチール株式会社 | 耐候性鋼材の製造方法 |
| JP5655280B2 (ja) * | 2009-06-03 | 2015-01-21 | 新日鐵住金株式会社 | 早期錆熟成耐候性鋼材及びその製造方法 |
| CN104060273B (zh) * | 2014-06-12 | 2017-12-19 | 江苏金陵特种涂料有限公司 | 一种钢结构用长效耐蚀涂料及其制备方法 |
| CN113930753B (zh) * | 2021-09-17 | 2023-09-05 | 武汉钢铁有限公司 | 热轧耐候钢锈层稳定化处理剂及处理方法 |
Family Cites Families (8)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4911739A (enExample) * | 1972-05-16 | 1974-02-01 | ||
| JPS5322530B2 (enExample) * | 1973-11-12 | 1978-07-10 | ||
| JPS5576078A (en) * | 1978-12-01 | 1980-06-07 | Nippon Paint Co Ltd | Pretreatment of iron or steel surface having iron oxide coating prior to painting |
| JPS5817833B2 (ja) * | 1979-01-19 | 1983-04-09 | 新日本製鐵株式会社 | 耐候性鋼の表面処理法 |
| JPS62103373A (ja) * | 1985-10-28 | 1987-05-13 | Nippon Fuerumaito Soushiya:Kk | 鉄鋼材の防錆処理方法 |
| JPH0621273B2 (ja) * | 1986-05-07 | 1994-03-23 | 神東塗料株式会社 | 耐候性鋼の錆安定化表面処理法 |
| JPH0733582B2 (ja) * | 1987-08-26 | 1995-04-12 | 石川島播磨重工業株式会社 | 炭素鋼の表面処理方法 |
| JPH01142088A (ja) * | 1987-11-30 | 1989-06-02 | Nippon Parkerizing Co Ltd | 耐候性鋼の表面処理方法 |
-
1992
- 1992-09-14 JP JP4244796A patent/JP2884941B2/ja not_active Expired - Lifetime
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPH09279229A5 (enExample) | ||
| Hirth | Theories of Hydrogen-induced cracking of steels | |
| NO942278D0 (no) | Forbedringer vedrörende behandling av betong | |
| CA2148160A1 (en) | Method for treating continuous extended lengths of tubular member interiors | |
| DE69509174D1 (de) | Verfahren zur Herstellung eines korrosions- und hitzebeständigen Körpers | |
| ATE338937T1 (de) | Oberflächengehärtetes präzisiongewicht und verfahren zu dessen herstellung | |
| JPH0586496A5 (enExample) | ||
| JPH0641333A5 (enExample) | ||
| JP2699733B2 (ja) | 鋼の錆安定化促進方法 | |
| KR900017922A (ko) | 바나듐-아렌의 제조방법 | |
| JPH0693467A (ja) | 耐候性に優れた鋼材および錆層の形成方法 | |
| JPS5872426A (ja) | 廃物発泡スチロ−ルの処理と再利用 | |
| ATE215616T1 (de) | Verfahren zum herstellen einer bc(n):h schicht | |
| CN85106667B (zh) | 双相超高强度时效不锈钢 | |
| JPS56112459A (en) | Cr-al coating method | |
| JPH083643A5 (enExample) | ||
| JPH11279644A5 (enExample) | ||
| EP0193575A1 (en) | Electrode for reducing oxygen | |
| Reick et al. | Development of ferritic-austenitic stainless steels with duplex microstructures | |
| SU1049564A1 (ru) | Состав дл хромомеднени предварительно никелированных стальных изделий | |
| JPH06262943A5 (enExample) | ||
| JPH0673354A5 (enExample) | ||
| AU636643B2 (en) | Method for soldering aluminum materials and apparatus used therein | |
| Kaluba et al. | On the Formation of Complex Chromium Diffusion Layers on Carbon Steel | |
| SU901351A1 (ru) | Состав дл жидкостного борохромировани стальных изделий |