JPH06192343A5 - - Google Patents

Info

Publication number
JPH06192343A5
JPH06192343A5 JP4-344344A JP34434492A JPH06192343A5 JP H06192343 A5 JPH06192343 A5 JP H06192343A5 JP 34434492 A JP34434492 A JP 34434492A JP H06192343 A5 JPH06192343 A5 JP H06192343A5
Authority
JP
Japan
Prior art keywords
compound
aqueous solution
amount
mol
weight
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP4-344344A
Other languages
English (en)
Japanese (ja)
Other versions
JPH06192343A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP34434492A priority Critical patent/JPH06192343A/ja
Priority claimed from JP34434492A external-priority patent/JPH06192343A/ja
Publication of JPH06192343A publication Critical patent/JPH06192343A/ja
Publication of JPH06192343A5 publication Critical patent/JPH06192343A5/ja
Ceased legal-status Critical Current

Links

JP34434492A 1992-12-24 1992-12-24 共重合体水溶液の製造方法 Ceased JPH06192343A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP34434492A JPH06192343A (ja) 1992-12-24 1992-12-24 共重合体水溶液の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP34434492A JPH06192343A (ja) 1992-12-24 1992-12-24 共重合体水溶液の製造方法

Publications (2)

Publication Number Publication Date
JPH06192343A JPH06192343A (ja) 1994-07-12
JPH06192343A5 true JPH06192343A5 (enExample) 1999-11-26

Family

ID=18368514

Family Applications (1)

Application Number Title Priority Date Filing Date
JP34434492A Ceased JPH06192343A (ja) 1992-12-24 1992-12-24 共重合体水溶液の製造方法

Country Status (1)

Country Link
JP (1) JPH06192343A (enExample)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP4889237B2 (ja) * 2005-04-28 2012-03-07 東邦化学工業株式会社 カチオン性共重合体の製造方法
CN105568722B (zh) * 2015-12-31 2019-01-22 浙江大川新材料股份有限公司 阳离子固色剂乳液的制备方法
CN105908543A (zh) * 2016-06-07 2016-08-31 苏州联胜化学有限公司 一种环保型棉用耐氯牢度提升剂及其制备方法

Similar Documents

Publication Publication Date Title
WO1988007559A1 (fr) Polymere cationique soluble dans l'eau
KR950011485A (ko) 다른 과플루오르화 단량체에 의한 테트라플루오로에틸렌 공중합체 제조방법
KR960017706A (ko) 메트(아크릴아미드), 에틸렌형 불포화 지방족 카복실산 또는 그의 염 및 폴리비닐 단량체로부터 제조한 수용성 중합체 및 페이퍼용 건조 강도 첨가제로서의 용도
US5750781A (en) Process for preparing an aqueous copolymer solution
JP3296580B2 (ja) 超高分子量重合体エマルジョンの製造法
JPS5867706A (ja) モノエチレン性不飽和のモノ−及びジカルボン酸からの共重合物の製法
JPH06179727A5 (enExample)
JPH06345820A5 (enExample)
JPH0437846B2 (enExample)
JPH06184246A5 (enExample)
JPH05239114A5 (enExample)
US5422408A (en) Polymerization of diallyldialkyl ammonium halide compounds with azo compound and inorganic salt
JPH038367B2 (enExample)
JP2615681B2 (ja) 水溶性共重合体の製造方法
JPH06234817A5 (enExample)
JPS5814425B2 (ja) 不飽和第3級アミンまたはその第4級アンモニウム塩の安定化法
JPH0586125A (ja) 水溶性ポリマーおよびその製造法
JPH06179727A (ja) 水溶性共重合体の製造方法
JPH06192343A (ja) 共重合体水溶液の製造方法
JP3227847B2 (ja) 水溶性共重合体の製造方法
DE60314864D1 (de) Verfahren zur herstellung von polymerdispersionen
JPH0341108A (ja) 両性高分子電解質およびその製造方法
JP4168551B2 (ja) 両性共重合体の製造方法
JPH05117327A (ja) 第3級アミノ基含有アクリルポリマーの製造方法
JP2678637B2 (ja) ビニルモノマーの重合法