JPH0577736B2 - - Google Patents
Info
- Publication number
- JPH0577736B2 JPH0577736B2 JP60289304A JP28930485A JPH0577736B2 JP H0577736 B2 JPH0577736 B2 JP H0577736B2 JP 60289304 A JP60289304 A JP 60289304A JP 28930485 A JP28930485 A JP 28930485A JP H0577736 B2 JPH0577736 B2 JP H0577736B2
- Authority
- JP
- Japan
- Prior art keywords
- corrosion resistance
- strength
- alloy
- titanium
- oxygen
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Preventing Corrosion Or Incrustation Of Metals (AREA)
- Conductive Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP28930485A JPS62149836A (ja) | 1985-12-24 | 1985-12-24 | 高強度高耐食性チタン基合金 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP28930485A JPS62149836A (ja) | 1985-12-24 | 1985-12-24 | 高強度高耐食性チタン基合金 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS62149836A JPS62149836A (ja) | 1987-07-03 |
| JPH0577736B2 true JPH0577736B2 (enrdf_load_stackoverflow) | 1993-10-27 |
Family
ID=17741445
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP28930485A Granted JPS62149836A (ja) | 1985-12-24 | 1985-12-24 | 高強度高耐食性チタン基合金 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS62149836A (enrdf_load_stackoverflow) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0436445A (ja) * | 1990-05-31 | 1992-02-06 | Sumitomo Metal Ind Ltd | 耐食性チタン合金継目無管の製造方法 |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS548529A (en) * | 1977-06-21 | 1979-01-22 | Nec Corp | Production of sintered type electrophotographic photoreceptor |
-
1985
- 1985-12-24 JP JP28930485A patent/JPS62149836A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS62149836A (ja) | 1987-07-03 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US12428708B2 (en) | Tantalum based alloy that is resistant to aqueous corrosion | |
| JP3395443B2 (ja) | 高クリープ強度チタン合金とその製造方法 | |
| JP2679109B2 (ja) | 金属間化合物TiA▲l▼基軽量耐熱合金 | |
| WO2011005745A1 (en) | Niobium based alloy that is resistant to aqueous corrosion | |
| EP3891313B1 (en) | Titanium alloys having improved corrosion resistance, strength, ductility, and toughness | |
| EP0379798B1 (en) | Titanium base alloy for superplastic forming | |
| JPH0257136B2 (enrdf_load_stackoverflow) | ||
| JP3274142B2 (ja) | アルミニウム−マンガン−シリコン−窒素オーステナイトステンレス耐酸鋼 | |
| JP2871867B2 (ja) | 耐蝕性Ti基合金 | |
| JPH0577736B2 (enrdf_load_stackoverflow) | ||
| US4526749A (en) | Tantalum-columbium-molybdenum-tungsten alloy | |
| JPH06108187A (ja) | 窒素添加高強度チタン合金 | |
| JPH0577733B2 (enrdf_load_stackoverflow) | ||
| JPS642662B2 (enrdf_load_stackoverflow) | ||
| RU2039113C1 (ru) | Сплав на основе титана | |
| JPH06228685A (ja) | 高強度高延性TiAl系金属間化合物およびその製造方法 | |
| JP2004027254A (ja) | 耐食性に優れたチタン合金及びその製造方法 | |
| GB2423089A (en) | Beta titanium eutectoid alloys | |
| JPH0577735B2 (enrdf_load_stackoverflow) | ||
| JPS62103330A (ja) | 冷間加工性の優れた高強度チタン合金 | |
| JPH07316682A (ja) | 形状記憶合金の製造法 | |
| JPS63144892A (ja) | 溶接棒 | |
| JPH03197631A (ja) | 金属間化合物TiAl―Cr基合金 | |
| JPH0366388B2 (enrdf_load_stackoverflow) | ||
| JPH05230570A (ja) | 高延性TiAl基合金 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| EXPY | Cancellation because of completion of term |