JPH0563542B2 - - Google Patents
Info
- Publication number
- JPH0563542B2 JPH0563542B2 JP62037172A JP3717287A JPH0563542B2 JP H0563542 B2 JPH0563542 B2 JP H0563542B2 JP 62037172 A JP62037172 A JP 62037172A JP 3717287 A JP3717287 A JP 3717287A JP H0563542 B2 JPH0563542 B2 JP H0563542B2
- Authority
- JP
- Japan
- Prior art keywords
- content
- delayed fracture
- low
- less
- cold heading
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Landscapes
- Solid-Phase Diffusion Into Metallic Material Surfaces (AREA)
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3717287A JPS63206449A (ja) | 1987-02-20 | 1987-02-20 | 冷間圧造用低炭素鋼 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3717287A JPS63206449A (ja) | 1987-02-20 | 1987-02-20 | 冷間圧造用低炭素鋼 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS63206449A JPS63206449A (ja) | 1988-08-25 |
| JPH0563542B2 true JPH0563542B2 (pm) | 1993-09-10 |
Family
ID=12490176
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP3717287A Granted JPS63206449A (ja) | 1987-02-20 | 1987-02-20 | 冷間圧造用低炭素鋼 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS63206449A (pm) |
Families Citing this family (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0826432B2 (ja) * | 1993-03-19 | 1996-03-13 | 愛知製鋼株式会社 | 高品質肌焼鋼 |
| JP3932102B2 (ja) * | 2001-07-17 | 2007-06-20 | 大同特殊鋼株式会社 | 肌焼鋼及びこれを用いた浸炭部品 |
| JP4773106B2 (ja) * | 2005-02-24 | 2011-09-14 | 株式会社神戸製鋼所 | 強度−捻れ特性バランスに優れた鋼部品およびその製造方法と該鋼部品用鋼材 |
| US8075420B2 (en) * | 2009-06-24 | 2011-12-13 | Acushnet Company | Hardened golf club head |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS59126718A (ja) * | 1983-01-07 | 1984-07-21 | Daido Steel Co Ltd | 冷間加工性に優れた鋼材の製造方法 |
-
1987
- 1987-02-20 JP JP3717287A patent/JPS63206449A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS63206449A (ja) | 1988-08-25 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2001240940A (ja) | 冷間鍛造用棒線材とその製造方法 | |
| US20230250522A1 (en) | Austenite stainless steel material, method for producing same, and plate spring | |
| JP4321974B2 (ja) | 高強度ねじ用鋼および高強度ねじ | |
| CN109790602B (zh) | 钢 | |
| KR100712581B1 (ko) | 제조성과 내식성이 우수한 베어링 강 및 그 제조 방법 및베어링 부품 및 그 제조 방법 | |
| JP3606024B2 (ja) | 高周波焼入部品およびその製造方法 | |
| JP2004238702A (ja) | 耐低サイクル衝撃疲労特性に優れた浸炭部品 | |
| JP2001026836A (ja) | 冷間加工性、転動疲労強度およびねじり疲労強度に優れた高周波焼入用鋼ならびに機械構造用部品 | |
| JP3550886B2 (ja) | 被削性および疲労強度に優れた高周波焼入用の歯車用鋼材の製造方法 | |
| JPH0563542B2 (pm) | ||
| JP4422924B2 (ja) | 高強度タッピングボルト用鋼、高強度タッピングボルトおよび高強度タッピングボルトの製造方法 | |
| JP3644217B2 (ja) | 高周波焼入部品およびその製造方法 | |
| JP3887461B2 (ja) | 非調質ボルト用鋼 | |
| JPH0254416B2 (pm) | ||
| JPH09217143A (ja) | 冷間鍛造性、高周波焼入れ性および転動疲労特性に優れた機械構造用鋼 | |
| JPH09104945A (ja) | 冷間加工性および耐遅れ破壊性に優れた高強度ボルト用鋼、高強度ボルトの製造方法および高強度ボルト | |
| JP3428282B2 (ja) | 高周波焼入用の歯車用鋼材およびその製造方法 | |
| JP3371490B2 (ja) | 冷間鍛造性に優れた機械構造用強靭鋼の製造方法 | |
| JPH0557350B2 (pm) | ||
| JPH0967625A (ja) | 耐遅れ破壊性に優れた浸炭高強度ネジの製造方法 | |
| JPS61253347A (ja) | 冷間加工性に優れた低炭素鋼 | |
| JP3748696B2 (ja) | 自動車用コネクティングロッドの製造方法 | |
| JPH05239553A (ja) | 深絞り性と溶接性に優れた中炭素冷延鋼板の製造方法 | |
| JPH11100644A (ja) | 高強度・高靱性ばね用鋼およびばねの製造方法 | |
| JP3269402B2 (ja) | 耐火性に優れた焼鈍省略型高力ボルト用鋼及びその製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |