JPH0553857B2 - - Google Patents
Info
- Publication number
- JPH0553857B2 JPH0553857B2 JP61068510A JP6851086A JPH0553857B2 JP H0553857 B2 JPH0553857 B2 JP H0553857B2 JP 61068510 A JP61068510 A JP 61068510A JP 6851086 A JP6851086 A JP 6851086A JP H0553857 B2 JPH0553857 B2 JP H0553857B2
- Authority
- JP
- Japan
- Prior art keywords
- toughness
- steel
- electric resistance
- present
- sour
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Landscapes
- Heat Treatment Of Articles (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6851086A JPS62227067A (ja) | 1986-03-28 | 1986-03-28 | 耐サワ−性の優れた高靭性電縫鋼管 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6851086A JPS62227067A (ja) | 1986-03-28 | 1986-03-28 | 耐サワ−性の優れた高靭性電縫鋼管 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS62227067A JPS62227067A (ja) | 1987-10-06 |
JPH0553857B2 true JPH0553857B2 (enrdf_load_stackoverflow) | 1993-08-11 |
Family
ID=13375780
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6851086A Granted JPS62227067A (ja) | 1986-03-28 | 1986-03-28 | 耐サワ−性の優れた高靭性電縫鋼管 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS62227067A (enrdf_load_stackoverflow) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH07122098B2 (ja) * | 1989-08-18 | 1995-12-25 | 川崎製鉄株式会社 | 低温靭性に優れた高強度電縫鋼管の製造方法 |
JP2733807B2 (ja) * | 1991-06-07 | 1998-03-30 | 株式会社日本製鋼所 | 耐硫化物応力腐食割れ性および低温靱性に優れた溶接構造用鋼 |
Family Cites Families (16)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5949285B2 (ja) * | 1977-08-26 | 1984-12-01 | 川崎製鉄株式会社 | 不安定破壊特性のすぐれた鋼板の製造法 |
JPS5488827A (en) * | 1977-12-26 | 1979-07-14 | Kawasaki Steel Co | Production of high tensile hot rolling steel plate with excellent extensibility and flanging property |
JPS5531101A (en) * | 1978-03-02 | 1980-03-05 | Nippon Kokan Kk <Nkk> | Manufacture of steel having superior hydrogen cracking resistance in wet hydrogen sulfide surroundings of high hydrogen ion concentration |
JPS5538901A (en) * | 1978-03-17 | 1980-03-18 | Nippon Kokan Kk <Nkk> | Manufacture of unrefined steel sheet having excellent hydrogen cracking resistance in wet hydrogen sulfide environment of high hydrogen ion concentration |
JPS56119759A (en) * | 1980-02-28 | 1981-09-19 | Nippon Kokan Kk <Nkk> | High tensile steel with superior sulfide corrosion crack resistance |
JPS589926A (ja) * | 1981-07-09 | 1983-01-20 | Kawasaki Steel Corp | 低温靭性にすぐれたapi規格x80級鋼管の製造方法 |
JPS589919A (ja) * | 1981-07-09 | 1983-01-20 | Kawasaki Steel Corp | 低温靭性にすぐれた高張力熱延鋼帯の製造方法 |
JPS5834133A (ja) * | 1981-08-22 | 1983-02-28 | Kawasaki Steel Corp | 低温靭性にすぐれたapi規格x80級鋼管の製造方法 |
JPS5834132A (ja) * | 1981-08-22 | 1983-02-28 | Kawasaki Steel Corp | 低温靭性にすぐれたapi規格x80級鋼管の製造方法 |
JPS5884958A (ja) * | 1981-11-13 | 1983-05-21 | Nippon Steel Corp | 熱間圧延用キルド鋼鋳片の製造方法 |
JPS6199656A (ja) * | 1984-10-22 | 1986-05-17 | Sumitomo Metal Ind Ltd | ラインパイプ用高強度溶接鋼管 |
JPS6199660A (ja) * | 1984-10-22 | 1986-05-17 | Sumitomo Metal Ind Ltd | ラインパイプ用高強度溶接鋼管 |
JPS61113749A (ja) * | 1984-11-09 | 1986-05-31 | Kawasaki Steel Corp | 油井用高耐食性合金 |
JPS61213346A (ja) * | 1985-03-19 | 1986-09-22 | Nippon Kokan Kk <Nkk> | 耐水素誘起割れ及び耐硫化物応力腐食割れ性に優れた鋼 |
JPS61279621A (ja) * | 1985-06-04 | 1986-12-10 | Kawasaki Steel Corp | 耐水素誘起割れに優れたラインパイプ用ホツトコイルの製造方法 |
JPS62170458A (ja) * | 1986-01-23 | 1987-07-27 | Nippon Steel Corp | 耐サワ−性の優れた高靭性電縫鋼管用鋼 |
-
1986
- 1986-03-28 JP JP6851086A patent/JPS62227067A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS62227067A (ja) | 1987-10-06 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US8562758B2 (en) | Austenitic-ferritic stainless steel | |
KR100628360B1 (ko) | 고강도 전기저항용접 파이프용 열연강대 | |
CN105143489B (zh) | 管线管用钢板和管线管 | |
BRPI0711795A2 (pt) | tubo de aço para tubulação de alta resistência superior em resistência ao envelhecimento após encruamento e chapa de aço para tubulação de alta resistência e métodos de produção da mesma | |
JP2003193204A (ja) | マルテンサイト系ステンレス鋼 | |
CN111108225B (zh) | 钢板及其制造方法 | |
JPH0674487B2 (ja) | 耐サワ−性の優れた高靱性電縫鋼管 | |
JPS61124554A (ja) | 耐サワ−性の優れた高靭性電縫鋼管用鋼 | |
GB2131832A (en) | Steel material exhibiting superior hydrogen cracking resistance in a wet sour gas environment | |
JPH0382740A (ja) | 熱間加工性と耐食性に優る2相ステンレス鋼 | |
JPS6145697B2 (enrdf_load_stackoverflow) | ||
JPH03211230A (ja) | 高耐食性低合金ラインパイプ用鋼の製造法 | |
JPH0553857B2 (enrdf_load_stackoverflow) | ||
JPS63274743A (ja) | 硫化水素の存在する環境で高い割れ抵抗を有するオ−ステナイト合金 | |
JPS6160866A (ja) | 耐サワ−性に優れたラインパイプ用鋼材 | |
JPH08232042A (ja) | 耐食性電縫溶接鋼管用鋼 | |
JP3293024B2 (ja) | 耐サワー性の優れた高靱性電縫鋼管用鋼の製造方法 | |
JP3549365B2 (ja) | 電縫鋼管用鋼の製造方法 | |
JPS61124555A (ja) | 耐サワ−性の優れた鋼 | |
JPH0366385B2 (enrdf_load_stackoverflow) | ||
JPS62170458A (ja) | 耐サワ−性の優れた高靭性電縫鋼管用鋼 | |
JPH08269566A (ja) | Sr特性に優れた高強度・高靱性uoe鋼管の製造方法 | |
JP3241912B2 (ja) | 塑性変形環境での耐硫化物応力腐食割れ性に優れる熱延鋼板の製造方法 | |
JPH0366380B2 (enrdf_load_stackoverflow) | ||
JPH02240211A (ja) | 耐水素誘起割れ性に優れる電縫鋼管の製法 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
LAPS | Cancellation because of no payment of annual fees |