JPH0550529B2 - - Google Patents
Info
- Publication number
- JPH0550529B2 JPH0550529B2 JP17438884A JP17438884A JPH0550529B2 JP H0550529 B2 JPH0550529 B2 JP H0550529B2 JP 17438884 A JP17438884 A JP 17438884A JP 17438884 A JP17438884 A JP 17438884A JP H0550529 B2 JPH0550529 B2 JP H0550529B2
- Authority
- JP
- Japan
- Prior art keywords
- acrylonitrile
- polymer
- producing
- weight
- water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Landscapes
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
- Polymerisation Methods In General (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP17438884A JPS6153301A (ja) | 1984-08-22 | 1984-08-22 | アクリロニトリル系重合体の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP17438884A JPS6153301A (ja) | 1984-08-22 | 1984-08-22 | アクリロニトリル系重合体の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6153301A JPS6153301A (ja) | 1986-03-17 |
| JPH0550529B2 true JPH0550529B2 (enExample) | 1993-07-29 |
Family
ID=15977733
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP17438884A Granted JPS6153301A (ja) | 1984-08-22 | 1984-08-22 | アクリロニトリル系重合体の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6153301A (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP5320227B2 (ja) * | 2009-09-10 | 2013-10-23 | 株式会社クレハ | 耐酸着色性の優れたフッ化ビニリデン重合体の製造方法 |
-
1984
- 1984-08-22 JP JP17438884A patent/JPS6153301A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6153301A (ja) | 1986-03-17 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS6154801B2 (enExample) | ||
| JPS6339606B2 (enExample) | ||
| JP4632665B2 (ja) | 重合反応の間の有機開始剤及び保護コロイドの同時計量供給 | |
| JPS6153301A (ja) | アクリロニトリル系重合体の製造方法 | |
| JPH0655792B2 (ja) | アクリロニトリル系重合体の製造方法 | |
| KR890002929B1 (ko) | 염화비닐 단량체의 현탁 중합 방법 | |
| JP2964662B2 (ja) | ビニル系重合体粒子の製造方法 | |
| JPH0195103A (ja) | ビニル系化合物の懸濁重合用の分散安定剤 | |
| JPS61123613A (ja) | 水性重合による低分子量のハロゲン化ビニル/ビニルエステルコポリマ−の製法 | |
| JPH02305804A (ja) | 塩化ビニル系重合体の製造方法 | |
| JP3742182B2 (ja) | ビニル系樹脂の製造方法 | |
| JPH03134003A (ja) | ビニル系化合物の懸濁重合用の分散助剤および分散安定剤 | |
| JPH03290402A (ja) | 塩化ビニル系モノマーの懸濁重合用分散安定剤 | |
| JPH0778083B2 (ja) | 塩化ビニル系懸濁重合方法における懸濁安定剤の仕込み方法 | |
| JPS6124047B2 (enExample) | ||
| JP3599956B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JP2588569B2 (ja) | 塩化ビニル懸濁重合方法 | |
| JP3414026B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JP3668692B2 (ja) | アルカリ可溶性ポリマー水分散体の製造方法 | |
| JPS6047007A (ja) | 塩化ビニル系単量体の懸濁重合方法 | |
| JPS5964607A (ja) | 塩化ビニル樹脂の製造方法 | |
| JPS638402A (ja) | 逆相懸濁重合用分散剤 | |
| JPH05295008A (ja) | 塩化ビニル系単量体の懸濁重合方法 | |
| JPH068329B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JPH07119249B2 (ja) | 塩化ビニル重合体の製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |