JPH0519573B2 - - Google Patents
Info
- Publication number
- JPH0519573B2 JPH0519573B2 JP60016601A JP1660185A JPH0519573B2 JP H0519573 B2 JPH0519573 B2 JP H0519573B2 JP 60016601 A JP60016601 A JP 60016601A JP 1660185 A JP1660185 A JP 1660185A JP H0519573 B2 JPH0519573 B2 JP H0519573B2
- Authority
- JP
- Japan
- Prior art keywords
- mol
- dianhydride
- tetracarboxylic dianhydride
- bis
- film
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Polymers With Sulfur, Phosphorus Or Metals In The Main Chain (AREA)
- Macromolecular Compounds Obtained By Forming Nitrogen-Containing Linkages In General (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60016601A JPS61176630A (ja) | 1985-02-01 | 1985-02-01 | 耐熱性樹脂の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60016601A JPS61176630A (ja) | 1985-02-01 | 1985-02-01 | 耐熱性樹脂の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61176630A JPS61176630A (ja) | 1986-08-08 |
| JPH0519573B2 true JPH0519573B2 (enrdf_load_stackoverflow) | 1993-03-17 |
Family
ID=11920813
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP60016601A Granted JPS61176630A (ja) | 1985-02-01 | 1985-02-01 | 耐熱性樹脂の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61176630A (enrdf_load_stackoverflow) |
Families Citing this family (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS61176632A (ja) * | 1985-02-01 | 1986-08-08 | Sumitomo Bakelite Co Ltd | 耐熱性樹脂の製造方法 |
| JPS61176631A (ja) * | 1985-02-01 | 1986-08-08 | Sumitomo Bakelite Co Ltd | 耐熱性樹脂の製造方法 |
| JPS61176629A (ja) * | 1985-02-01 | 1986-08-08 | Sumitomo Bakelite Co Ltd | 耐熱性樹脂の製造方法 |
| JPS61181830A (ja) * | 1985-02-06 | 1986-08-14 | Sumitomo Bakelite Co Ltd | 耐熱性樹脂の製造方法 |
| TWI270243B (en) * | 2004-11-23 | 2007-01-01 | Ind Tech Res Inst | Device of micro vortex for ferro-fluid power generator |
Family Cites Families (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS61138629A (ja) * | 1984-12-10 | 1986-06-26 | Sumitomo Bakelite Co Ltd | 耐熱性樹脂の製造方法 |
| JPS61141734A (ja) * | 1984-12-14 | 1986-06-28 | Sumitomo Bakelite Co Ltd | 耐熱性樹脂の製造方法 |
| JPS61143436A (ja) * | 1984-12-18 | 1986-07-01 | Sumitomo Bakelite Co Ltd | 耐熱性樹脂の製造方法 |
| JPS61176632A (ja) * | 1985-02-01 | 1986-08-08 | Sumitomo Bakelite Co Ltd | 耐熱性樹脂の製造方法 |
| JPS61176631A (ja) * | 1985-02-01 | 1986-08-08 | Sumitomo Bakelite Co Ltd | 耐熱性樹脂の製造方法 |
| JPS61176629A (ja) * | 1985-02-01 | 1986-08-08 | Sumitomo Bakelite Co Ltd | 耐熱性樹脂の製造方法 |
| JPS61181830A (ja) * | 1985-02-06 | 1986-08-14 | Sumitomo Bakelite Co Ltd | 耐熱性樹脂の製造方法 |
-
1985
- 1985-02-01 JP JP60016601A patent/JPS61176630A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS61176630A (ja) | 1986-08-08 |