JPH0519260B2 - - Google Patents
Info
- Publication number
- JPH0519260B2 JPH0519260B2 JP61099213A JP9921386A JPH0519260B2 JP H0519260 B2 JPH0519260 B2 JP H0519260B2 JP 61099213 A JP61099213 A JP 61099213A JP 9921386 A JP9921386 A JP 9921386A JP H0519260 B2 JPH0519260 B2 JP H0519260B2
- Authority
- JP
- Japan
- Prior art keywords
- polyvinyl alcohol
- cathode plate
- cadmium
- powder
- alkaline storage
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/24—Electrodes for alkaline accumulators
- H01M4/26—Processes of manufacture
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/62—Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M4/621—Binders
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP61099213A JPS62256373A (ja) | 1986-04-28 | 1986-04-28 | ニツケル・カドミウムアルカリ蓄電池用陰極板の製造法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP61099213A JPS62256373A (ja) | 1986-04-28 | 1986-04-28 | ニツケル・カドミウムアルカリ蓄電池用陰極板の製造法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS62256373A JPS62256373A (ja) | 1987-11-09 |
JPH0519260B2 true JPH0519260B2 (enrdf_load_stackoverflow) | 1993-03-16 |
Family
ID=14241374
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP61099213A Granted JPS62256373A (ja) | 1986-04-28 | 1986-04-28 | ニツケル・カドミウムアルカリ蓄電池用陰極板の製造法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS62256373A (enrdf_load_stackoverflow) |
-
1986
- 1986-04-28 JP JP61099213A patent/JPS62256373A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS62256373A (ja) | 1987-11-09 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPH07331201A (ja) | 導電性接着剤及び該導電性接着剤による接着構造 | |
JP2001250536A (ja) | 非水電解液二次電池用負極板の製造法 | |
JPH0519260B2 (enrdf_load_stackoverflow) | ||
US3713891A (en) | Chloride free leaching process for porous zinc anodes | |
JP2871077B2 (ja) | 非水電解質二次電池用負極の製造法 | |
JPH0624148B2 (ja) | 密閉形ニツケルカドミウム蓄電池 | |
JP2584280B2 (ja) | アルカリ蓄電池及びその製造方法 | |
JP2968813B2 (ja) | アルカリ蓄電池用カドミウム負極の製造方法 | |
JP2733231B2 (ja) | 水素吸蔵合金電極の製造法 | |
JPS61294762A (ja) | ニツケル・カドミウムアルカリ蓄電池用陰極板の製造法 | |
JPS5835351B2 (ja) | 一次または二次電池用電極 | |
JP2692795B2 (ja) | アルカリ蓄電池用ペースト式カドミウム陰極 | |
JPH071694B2 (ja) | 密閉形ニッケルカドミウム蓄電池用陰極板 | |
JPS6113564A (ja) | カドミウム負極板の製造方法 | |
JPS6298563A (ja) | ニツケル・カドミウムアルカリ蓄電池用陰極板の製造法 | |
JP3043775B2 (ja) | アルカリ蓄電池用カドミウム負極 | |
CN117457886A (zh) | 一种双层氧化物包覆的硅基负极材料及其制备方法和应用 | |
JPH0675397B2 (ja) | ペ−スト式カドミウム負極の製造法 | |
JPS63164162A (ja) | アルカリ蓄電池用カドミウム負極 | |
JPH08203515A (ja) | ニッケル電極の製造方法 | |
JPH0298047A (ja) | アルカリ蓄電池用カドミウム負極 | |
JPH01189862A (ja) | 密閉式アルカリ蓄電池用陰極板の製造方法 | |
JPH0831316B2 (ja) | ペ−スト式カドミウム負極の製造方法 | |
JPH01140556A (ja) | アルカリ蓄電池用カドミウム負極 | |
JPH0773047B2 (ja) | 密閉形アルカリ蓄電池用負極 |