- thermal shock
- ceramics
- weight
- fused silica
- alumina
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Compositions Of Oxide Ceramics (AREA)
- Catalysts (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60113612A JPS61270255A (ja) | 1985-05-27 | 1985-05-27 | 耐熱衝撃性セラミツクス |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60113612A JPS61270255A (ja) | 1985-05-27 | 1985-05-27 | 耐熱衝撃性セラミツクス |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61270255A JPS61270255A (ja) | 1986-11-29 |
| JPH0513101B2 true JPH0513101B2 (enrdf_load_html_response) | 1993-02-19 |
Family
ID=14616628
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP60113612A Granted JPS61270255A (ja) | 1985-05-27 | 1985-05-27 | 耐熱衝撃性セラミツクス |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61270255A (enrdf_load_html_response) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH029452A (ja) * | 1988-06-29 | 1990-01-12 | Matsushita Electric Ind Co Ltd | 排ガス浄化用触媒およびその製造法 |
| JPH02198641A (ja) * | 1989-01-26 | 1990-08-07 | Matsushita Electric Ind Co Ltd | 触媒およびその製造法 |
-
1985
- 1985-05-27 JP JP60113612A patent/JPS61270255A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS61270255A (ja) | 1986-11-29 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP0036052B2 (en) | Honeycomb structure for use as a catalyst support for automobile exhaust | |
| EP0037868B1 (en) | Method of producing low-expansion ceramic materials | |
| EP0231006B1 (en) | Method for producing ceramics with thermal shock resistance | |
| EP1027304A1 (en) | Method for firing ceramic honeycomb bodies | |
| US5288672A (en) | Ceramics based on aluminum titanate, process for their production and their use | |
| JPH0513101B2 (enrdf_load_html_response) | ||
| US4018614A (en) | Celsian-zirconia compositions | |
| JPH06305828A (ja) | チタン酸アルミニウム複合材料及びその製造方法 | |
| JPS589783B2 (ja) | 低膨脹セラミツクス | |
| JPH0688833B2 (ja) | 耐熱衝撃性セラミツクス | |
| JPH10194827A (ja) | 耐熱衝撃性セラミックスおよびその製造方法 | |
| JPH10212158A (ja) | ガラス溶解窯用耐火物 | |
| JPH0513102B2 (enrdf_load_html_response) | ||
| JPS6251909B2 (enrdf_load_html_response) | ||
| JPH01183463A (ja) | チタン酸アルミニウム/β−スポジューメン/ムライト系複合焼結体及びその製造方法 | |
| JPH0226863A (ja) | コージライト質セラミックスとその製造方法 | |
| JPS5851908B2 (ja) | コ−デイエライト焼結体の製法 | |
| JPH0149664B2 (enrdf_load_html_response) | ||
| JPS5919065B2 (ja) | マグネシア−スピネル煉瓦の製造法 | |
| JPH0152352B2 (enrdf_load_html_response) | ||
| JPH0149665B2 (enrdf_load_html_response) | ||
| JPS5913471B2 (ja) | 耐高温低膨脹セラミツクスの製造法 | |
| JPH0645501B2 (ja) | 耐熱衝撃性セラミックス構造体の製造法 | |
| JPS6033783B2 (ja) | アルミニウムチタネ−ト質のハニカム | |
| JPH01183458A (ja) | 低熱膨張性材料 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| EXPY | Cancellation because of completion of term |