JPH046046B2 - - Google Patents
Info
- Publication number
- JPH046046B2 JPH046046B2 JP57157472A JP15747282A JPH046046B2 JP H046046 B2 JPH046046 B2 JP H046046B2 JP 57157472 A JP57157472 A JP 57157472A JP 15747282 A JP15747282 A JP 15747282A JP H046046 B2 JPH046046 B2 JP H046046B2
- Authority
- JP
- Japan
- Prior art keywords
- glass
- powder
- insulating
- insulating layer
- paste
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Compositions Of Oxide Ceramics (AREA)
- Glass Compositions (AREA)
- Inorganic Insulating Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP57157472A JPS5946702A (ja) | 1982-09-10 | 1982-09-10 | 絶縁性セラミツクペ−スト用無機組成物 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP57157472A JPS5946702A (ja) | 1982-09-10 | 1982-09-10 | 絶縁性セラミツクペ−スト用無機組成物 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5946702A JPS5946702A (ja) | 1984-03-16 |
| JPH046046B2 true JPH046046B2 (enEXAMPLES) | 1992-02-04 |
Family
ID=15650420
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP57157472A Granted JPS5946702A (ja) | 1982-09-10 | 1982-09-10 | 絶縁性セラミツクペ−スト用無機組成物 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5946702A (enEXAMPLES) |
Families Citing this family (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS62192243A (ja) * | 1986-02-17 | 1987-08-22 | Nippon Kokan Kk <Nkk> | 連続鋳造における鋳片縦割れの検出方法 |
| JP2507418B2 (ja) * | 1986-05-02 | 1996-06-12 | 旭硝子株式会社 | 回路基板用組成物 |
| EP0253342A1 (en) * | 1986-07-15 | 1988-01-20 | E.I. Du Pont De Nemours And Company | Glass ceramic dielectric compositions |
| US5821181A (en) * | 1996-04-08 | 1998-10-13 | Motorola Inc. | Ceramic composition |
| JP3941201B2 (ja) | 1998-01-20 | 2007-07-04 | 株式会社デンソー | 導体ペースト組成物及び回路基板 |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6447412A (en) * | 1987-05-29 | 1989-02-21 | Hayashi Seisakusho Kk | Deaerating packing device for vessel packed with adhesive substance |
-
1982
- 1982-09-10 JP JP57157472A patent/JPS5946702A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5946702A (ja) | 1984-03-16 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US7176152B2 (en) | Lead-free and cadmium-free conductive copper thick film pastes | |
| US5645765A (en) | Lead-free conductive paste | |
| JP5303552B2 (ja) | セラミック基板用導体ペーストおよび電気回路 | |
| US4812422A (en) | Dielectric paste and method of manufacturing the paste | |
| JP4958904B2 (ja) | コンデンサ用の鉛フリー及びカドミウムフリーガラスを含む銅端子インク | |
| JP4805268B2 (ja) | コンデンサ用の鉛フリー及びカドミウムフリーガラスを含有する銅成端インク | |
| TW200418221A (en) | Terminal electrode compositions for multilayer ceramic capacitors | |
| JPS58156552A (ja) | 絶縁性セラミツクペ−スト用無機組成物 | |
| JPH046045B2 (enEXAMPLES) | ||
| JPH046046B2 (enEXAMPLES) | ||
| JPH046047B2 (enEXAMPLES) | ||
| JP2713376B2 (ja) | 絶縁層用ガラス組成物 | |
| JPH057343B2 (enEXAMPLES) | ||
| JPH0452561B2 (enEXAMPLES) | ||
| JP2500692B2 (ja) | 低温焼結性低誘電率無機組成物 | |
| JPS5954106A (ja) | 絶縁性セラミツクペ−スト用無機組成物 | |
| JPS6221739B2 (enEXAMPLES) | ||
| JPH0147412B2 (enEXAMPLES) | ||
| KR102820137B1 (ko) | 후막 저항 페이스트, 후막 저항체, 및 전자 부품 | |
| JPH057344B2 (enEXAMPLES) | ||
| KR102851511B1 (ko) | 후막 저항 페이스트, 후막 저항체, 및 전자 부품 | |
| JPH01119543A (ja) | 絶縁性セラミックペースト用無機組成物 | |
| JPS6233682B2 (enEXAMPLES) | ||
| JPH0260236B2 (enEXAMPLES) | ||
| JPH02212336A (ja) | ガラスセラミック組成物及びその用途 |