- JPH0435541B2 JPH0435541B2 JP60090571A JP9057185A JPH0435541B2 JP H0435541 B2 JPH0435541 B2 JP H0435541B2 JP 60090571 A JP60090571 A JP 60090571A JP 9057185 A JP9057185 A JP 9057185A JP H0435541 B2 JPH0435541 B2 JP H0435541B2
- Authority
- JP
- Japan
- Prior art keywords
- alloy
- weight
- cao
- desulfurization
- less
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Furnace Housings, Linings, Walls, And Ceilings (AREA)
- Manufacture And Refinement Of Metals (AREA)
Priority Applications (11)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9057185A JPS61250125A (ja) | 1985-04-26 | 1985-04-26 | 高純度超極低硫黄合金の製造方法 |
GB8609901A GB2174716B (en) | 1985-04-26 | 1986-04-23 | Method of producing an iron-cobalt-and nickel-base alloy having low contents of sulphur, oxygen and nitrogen |
CN86102879.1A CN1010105B (zh) | 1985-04-26 | 1986-04-25 | 硫、氧和氮含量低的铁-钴-和镍-基合金的生产方法 |
CN90106761.XA CN1017067B (zh) | 1985-04-26 | 1986-04-25 | 硫、氧和氮含量低的铁基合金 |
FR868606058A FR2587367B1 (fr) | 1985-04-26 | 1986-04-25 | Procede pour la production d'un alliage a base de fer, de cobalt et de nickel, a faible teneur en soufre, en oxygene et en azote |
US06/937,426 US4729787A (en) | 1985-04-26 | 1986-12-03 | Method of producing an iron; cobalt and nickel base alloy having low contents of sulphur, oxygen and nitrogen |
US07/010,598 US4820485A (en) | 1985-04-26 | 1987-02-03 | Method of producing an iron-, cobalt- and nickel-base alloy having low contents of sulphur, oxygen and nitrogen |
GB8901402A GB2212513B (en) | 1985-04-26 | 1989-01-23 | A nickel-base alloy having low contents of sulphur, oxygen and nitrogen |
GB8901401A GB2212512B (en) | 1985-04-26 | 1989-01-23 | An iron-base alloy having low contents of sulphur, oxygen and nitrogen |
US07/441,600 US4999053A (en) | 1985-04-26 | 1989-11-27 | Method of producing an iron-, cobalt- and nickel-base alloy having low contents of sulphur, oxygen and nitrogen |
US07/702,347 US5268141A (en) | 1985-04-26 | 1991-05-15 | Iron based alloy having low contents of aluminum silicon, magnesium, calcium, oxygen, sulphur, and nitrogen |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9057185A JPS61250125A (ja) | 1985-04-26 | 1985-04-26 | 高純度超極低硫黄合金の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS61250125A JPS61250125A (ja) | 1986-11-07 |
JPH0435541B2 true JPH0435541B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1992-06-11 |
Family
ID=14002109
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP9057185A Granted JPS61250125A (ja) | 1985-04-26 | 1985-04-26 | 高純度超極低硫黄合金の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS61250125A (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) |
Family Cites Families (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6025486B2 (ja) * | 1975-11-08 | 1985-06-18 | 東北大学金属材料研究所長 | 酸素,硫黄,窒素含有量の少ない清浄な鋼の製造方法 |
JPS592209B2 (ja) * | 1977-06-03 | 1984-01-17 | 日本電気株式会社 | Pll発振回路 |
JPS5424688A (en) * | 1977-07-27 | 1979-02-24 | Toyo Boorudouin Kk | Chuck for material tester |
JPS57200513A (en) * | 1981-06-02 | 1982-12-08 | Metal Res Corp:Kk | Preparation of iron base alloy with reduced oxygen, sulfur and nitrogen contents |
-
1985
- 1985-04-26 JP JP9057185A patent/JPS61250125A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS61250125A (ja) | 1986-11-07 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US4484946A (en) | Method of producing iron-, nickle-, or cobalt-base alloy with low contents of oxygen, sulphur, and nitrogen | |
JPH0699737B2 (ja) | 清浄鋼の製造方法 | |
US5268141A (en) | Iron based alloy having low contents of aluminum silicon, magnesium, calcium, oxygen, sulphur, and nitrogen | |
US4820485A (en) | Method of producing an iron-, cobalt- and nickel-base alloy having low contents of sulphur, oxygen and nitrogen | |
JPH03223414A (ja) | 硫黄、酸素及び窒素の各含有量が極めて低い鉄―、ニッケル―、及びコバルト―基合金の製造方法 | |
US4999053A (en) | Method of producing an iron-, cobalt- and nickel-base alloy having low contents of sulphur, oxygen and nitrogen | |
WO2025047169A1 (ja) | 表面性状に優れたNi基合金 | |
JPH03236434A (ja) | 硫黄、酸素及び窒素の各含有量が極めて低いニッケル基合金 | |
JPH0435541B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
US5055018A (en) | Clean steel | |
KR910001488B1 (ko) | 황, 산소 및 질소의 낮은 함량을 갖는 철기합금, 코발트기합금, 니켈기합금 및 그 제조방법 | |
US5225156A (en) | Clean steel composition | |
JPS6184341A (ja) | 酸素、硫黄、窒素含有量の少ない合金の製造方法 | |
JPS6286111A (ja) | 精錬用カルシア系耐火組成物及びそれを用いた脱硫方法 | |
JP7438435B1 (ja) | 表面性状に優れたステンレス鋼 | |
JPH03236435A (ja) | 硫黄、酸素及び窒素の各含有量が極めて低いコバルト基合金 | |
GB2212512A (en) | Iron-, cobalt- and nickel-base alloy having low contents of sulphur, oxygen and nitrogen | |
JPS61243134A (ja) | 超極低硫黄合金の製造方法 | |
US12215395B2 (en) | Method for recycling chromium oxide and forming chromium-alloy steel | |
KR940008928B1 (ko) | 정제강의 제조방법 및 그 정제강 | |
JPS6252021B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
JPS6025486B2 (ja) | 酸素,硫黄,窒素含有量の少ない清浄な鋼の製造方法 | |
JPH03223440A (ja) | 硫黄、酸素及び窒素の各含有量が極めて低い鉄基合金 | |
JPH0613431B2 (ja) | 精錬用耐火材及び精錬方法 | |
Sunulahpašić et al. | INTENSIFICATION OF LOW-CARBON STEEL DESULPHURISATION IN THE INDUCTION FURNACE |