JPH0419297B2 - - Google Patents
Info
- Publication number
- JPH0419297B2 JPH0419297B2 JP15881987A JP15881987A JPH0419297B2 JP H0419297 B2 JPH0419297 B2 JP H0419297B2 JP 15881987 A JP15881987 A JP 15881987A JP 15881987 A JP15881987 A JP 15881987A JP H0419297 B2 JPH0419297 B2 JP H0419297B2
- Authority
- JP
- Japan
- Prior art keywords
- less
- flux density
- magnetic flux
- annealing
- iron loss
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Manufacturing Of Steel Electrode Plates (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15881987A JPS6333518A (ja) | 1987-06-27 | 1987-06-27 | 鉄損が低くかつ磁束密度がすぐれた無方向性電磁鋼板およびその製造法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15881987A JPS6333518A (ja) | 1987-06-27 | 1987-06-27 | 鉄損が低くかつ磁束密度がすぐれた無方向性電磁鋼板およびその製造法 |
Related Parent Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP58009398A Division JPS59157259A (ja) | 1982-01-27 | 1983-01-25 | 鉄損が低くかつ磁束密度がすぐれた無方向性電磁鋼板およびその製造法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6333518A JPS6333518A (ja) | 1988-02-13 |
JPH0419297B2 true JPH0419297B2 (en, 2012) | 1992-03-30 |
Family
ID=15680063
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP15881987A Granted JPS6333518A (ja) | 1987-06-27 | 1987-06-27 | 鉄損が低くかつ磁束密度がすぐれた無方向性電磁鋼板およびその製造法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6333518A (en, 2012) |
Families Citing this family (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH01219126A (ja) * | 1988-02-26 | 1989-09-01 | Nkk Corp | 表面性状の優れた無方向性電磁鋼板の製造方法 |
JPH01219124A (ja) * | 1988-02-26 | 1989-09-01 | Nkk Corp | 酸洗性に優れた無方向性電磁鋼板の製造方法 |
JPH0686647B2 (ja) * | 1990-03-22 | 1994-11-02 | 住友金属工業株式会社 | 磁気特性に優れた無方向性電磁鋼板 |
KR100501000B1 (ko) * | 1997-11-25 | 2005-10-12 | 주식회사 포스코 | 응력제거소둔후철손이낮은무방향성전기강판및그제조방법 |
EP1825991B1 (en) | 2006-02-27 | 2014-04-02 | The Yokohama Rubber Co., Ltd. | Tire puncture sealant |
-
1987
- 1987-06-27 JP JP15881987A patent/JPS6333518A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS6333518A (ja) | 1988-02-13 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS6256225B2 (en, 2012) | ||
US4439251A (en) | Non-oriented electric iron sheet and method for producing the same | |
EP2775007B1 (en) | A process for the production of a grain-oriented electrical steel | |
KR100345706B1 (ko) | 자기적특성이우수한무방향성전기강판및그제조방법 | |
JP2000129410A (ja) | 磁束密度の高い無方向性電磁鋼板 | |
JPS6256922B2 (en, 2012) | ||
JPH0419297B2 (en, 2012) | ||
JPH0753886B2 (ja) | 鉄損の優れた薄手高磁束密度一方向性電磁鋼板の製造方法 | |
JP3430794B2 (ja) | 磁気特性に優れる無方向性電磁鋼板およびその製造方法 | |
JP3037878B2 (ja) | 歪取焼鈍後鉄損に優れる無方向性電磁鋼板およびその製造方法 | |
KR100340503B1 (ko) | 무방향성전기강판의제조방법 | |
KR950004933B1 (ko) | 자기특성이 우수한 무방향성 전기강판의 제조방법 | |
JPH0949023A (ja) | 鉄損が優れた一方向性電磁鋼板の製造方法 | |
KR100340548B1 (ko) | 자성이우수한무방향성전기강판의제조방법 | |
KR101110257B1 (ko) | 자속밀도가 우수한 무방향성 전기강판 및 그 제조방법 | |
JP4281119B2 (ja) | 電磁鋼板の製造方法 | |
JPH08143960A (ja) | 磁束密度が高くかつ鉄損が低い無方向性電磁鋼板の製造方法 | |
JPH06256847A (ja) | 磁気特性の優れた一方向性電磁鋼板の製造方法 | |
JPS6256924B2 (en, 2012) | ||
JP3294367B2 (ja) | 磁束密度が高くかつ鉄損が低い無方向性電磁鋼板およびその製造方法 | |
JPH0797628A (ja) | 磁束密度が高く、鉄損の低い無方向性電磁鋼板の製造方法 | |
JP2784661B2 (ja) | 高磁束密度薄手一方向性電磁鋼板の製造方法 | |
JP3331402B2 (ja) | 全周磁気特性の優れたセミプロセス無方向性電磁鋼板の製造方法 | |
JP2870817B2 (ja) | 磁気特性の優れたセミプロセス無方向性電磁鋼板の製造方法 | |
JPH05279826A (ja) | インピーダンス比透磁率の優れたパーマロイの製造方法 |