JPH0376177B2 - - Google Patents
Info
- Publication number
- JPH0376177B2 JPH0376177B2 JP60280272A JP28027285A JPH0376177B2 JP H0376177 B2 JPH0376177 B2 JP H0376177B2 JP 60280272 A JP60280272 A JP 60280272A JP 28027285 A JP28027285 A JP 28027285A JP H0376177 B2 JPH0376177 B2 JP H0376177B2
- Authority
- JP
- Japan
- Prior art keywords
- powder
- impact
- particles
- solid particles
- film
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Processing And Handling Of Plastics And Other Materials For Molding In General (AREA)
- Glanulating (AREA)
- Crushing And Pulverization Processes (AREA)
- Processes Of Treating Macromolecular Substances (AREA)
Priority Applications (6)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP60280272A JPS62140636A (ja) | 1985-12-13 | 1985-12-13 | 固体粒子表面の成膜方法 |
EP86112228A EP0224659B1 (en) | 1985-10-07 | 1986-09-04 | Method of improving quality of surface of solid particles and apparatus thereof |
DE8686112228T DE3687219T2 (de) | 1985-10-07 | 1986-09-04 | Methode zur verbesserung der oberflaechenqualitaet von festen teilchen und vorrichtung dazu. |
SU864028279A RU2047362C1 (ru) | 1985-10-07 | 1986-10-03 | Способ обработки поверхности твердых частиц и устройство для его осуществления |
KR1019860010468A KR900001366B1 (ko) | 1985-12-13 | 1986-12-08 | 고체입자의 표면개질 방법과 그 장치 |
US07/183,297 US4915987A (en) | 1985-10-07 | 1988-04-11 | Method of improving quality of surface of solid particles and apparatus thereof |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP60280272A JPS62140636A (ja) | 1985-12-13 | 1985-12-13 | 固体粒子表面の成膜方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS62140636A JPS62140636A (ja) | 1987-06-24 |
JPH0376177B2 true JPH0376177B2 (enrdf_load_stackoverflow) | 1991-12-04 |
Family
ID=17622678
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP60280272A Granted JPS62140636A (ja) | 1985-10-07 | 1985-12-13 | 固体粒子表面の成膜方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS62140636A (enrdf_load_stackoverflow) |
Families Citing this family (11)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS62298443A (ja) * | 1986-06-17 | 1987-12-25 | Nara Kikai Seisakusho:Kk | 固体粒子の表面改質方法 |
JPH0775665B2 (ja) * | 1986-10-27 | 1995-08-16 | 日本合成ゴム株式会社 | マイクロカプセル化微粒子の製造方法 |
JPH02157027A (ja) * | 1988-12-07 | 1990-06-15 | Canon Inc | 乾式トナーの製造方法 |
JPH02194828A (ja) * | 1989-01-20 | 1990-08-01 | Nippon Spindle Mfg Co Ltd | 粉体表面の改質方法及びその装置 |
JP2576462Y2 (ja) * | 1992-12-01 | 1998-07-09 | 株式会社小松製作所 | 操作レバー装置の継手 |
JP3301569B2 (ja) * | 1993-12-07 | 2002-07-15 | 株式会社小松製作所 | 電気式レバー装置 |
JP2003025325A (ja) * | 2001-07-23 | 2003-01-29 | Sumitomo Bakelite Co Ltd | 複合粒子の製造方法 |
KR20070108798A (ko) * | 2006-05-08 | 2007-11-13 | 최길배 | 나노입자 및 메조입자로 표면 개질된 중합체 거대입자,이를 이용한 나노입자-고분자 복합소재, 및 이들의제조방법 |
JP2013026014A (ja) * | 2011-07-21 | 2013-02-04 | Honda Motor Co Ltd | 燃料電池用触媒及び燃料電池用触媒の製造方法 |
JP6385321B2 (ja) * | 2015-09-30 | 2018-09-05 | 積水化成品工業株式会社 | 表面改質発泡性粒子、発泡粒子の製造方法及び発泡成形体の製造方法 |
DE102020131233A1 (de) * | 2020-11-25 | 2022-05-25 | Netzsch Trockenmahltechnik Gmbh | Verfahren zur herstellung eines homogenisierten gemischs aus kohlenstoff, schwefel und ptfe |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5318650A (en) * | 1976-08-04 | 1978-02-21 | Mitsui Aluminium Kogyo Kk | Granules for molding building materials made by bonding gypsum dihydrate and high polymer and method of manufacture |
JPS60129144A (ja) * | 1983-12-16 | 1985-07-10 | 株式会社奈良機械製作所 | 微粉砕機 |
JPS6283029A (ja) * | 1985-10-07 | 1987-04-16 | Nara Kikai Seisakusho:Kk | 固体粒子の表面改質方法 |
-
1985
- 1985-12-13 JP JP60280272A patent/JPS62140636A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS62140636A (ja) | 1987-06-24 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPH032009B2 (enrdf_load_stackoverflow) | ||
US4915987A (en) | Method of improving quality of surface of solid particles and apparatus thereof | |
JPH0376177B2 (enrdf_load_stackoverflow) | ||
JPH0510970B2 (enrdf_load_stackoverflow) | ||
EP0421980A2 (en) | Particulate material treating apparatus | |
GB2130504A (en) | Granulating and coating machine | |
US6197369B1 (en) | Method of particle coating | |
EP0555947A1 (en) | Method for surface treatment of solid Particles and apparatus therefor | |
JPH0461687B2 (enrdf_load_stackoverflow) | ||
JPH0751288B2 (ja) | 粒子の複合化方法 | |
JPH0510971B2 (enrdf_load_stackoverflow) | ||
JP2941081B2 (ja) | 結晶性有機化合物の非晶質割合の増加と再結晶化を抑制する方法 | |
JP4596134B2 (ja) | カーボンナノチューブの分散性向上方法 | |
JPH043250B2 (enrdf_load_stackoverflow) | ||
US20210205850A1 (en) | De-agglomerating sieve with de-ionization | |
KR900001366B1 (ko) | 고체입자의 표면개질 방법과 그 장치 | |
JPH0816795B2 (ja) | トナ−の製造方法およびその装置 | |
JP2001315127A (ja) | 塗膜剥離方法及びその装置 | |
RU2047362C1 (ru) | Способ обработки поверхности твердых частиц и устройство для его осуществления | |
JPH05168895A (ja) | 固体粒子の表面改質方法 | |
KR100665042B1 (ko) | 나노입자 및 메조입자로 표면 개질된 중합체 거대입자,이를 이용한 나노입자-고분자 복합소재, 및 이들의제조방법 | |
US4762765A (en) | Method of generating a spherical grain | |
US6635207B1 (en) | Process for recycling of powder coating waste | |
JP6713332B2 (ja) | 造粒冷却装置 | |
JPH0618580Y2 (ja) | 固体粒子の表面改質装置に用いる回転盤 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
LAPS | Cancellation because of no payment of annual fees |