JPH0318498Y2 - - Google Patents
Info
- Publication number
- JPH0318498Y2 JPH0318498Y2 JP1986029980U JP2998086U JPH0318498Y2 JP H0318498 Y2 JPH0318498 Y2 JP H0318498Y2 JP 1986029980 U JP1986029980 U JP 1986029980U JP 2998086 U JP2998086 U JP 2998086U JP H0318498 Y2 JPH0318498 Y2 JP H0318498Y2
- Authority
- JP
- Japan
- Prior art keywords
- snout
- plating
- duct
- opening
- molten metal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Coating With Molten Metal (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1986029980U JPH0318498Y2 (en:Method) | 1986-02-28 | 1986-02-28 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1986029980U JPH0318498Y2 (en:Method) | 1986-02-28 | 1986-02-28 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS62141059U JPS62141059U (en:Method) | 1987-09-05 |
JPH0318498Y2 true JPH0318498Y2 (en:Method) | 1991-04-18 |
Family
ID=30834367
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP1986029980U Expired JPH0318498Y2 (en:Method) | 1986-02-28 | 1986-02-28 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPH0318498Y2 (en:Method) |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
KR102148459B1 (ko) * | 2019-05-03 | 2020-08-26 | (주)스텝이엔지 | 강판 용융아연도금 공정에서의 탕면 이물질제거장치 |
Family Cites Families (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5335920U (en:Method) * | 1976-09-03 | 1978-03-29 | ||
JPS55131144A (en) * | 1979-03-30 | 1980-10-11 | Nippon Kokan Kk <Nkk> | Top dross collecting method |
JPS5727802Y2 (en:Method) * | 1979-05-17 | 1982-06-17 | ||
JPS60230969A (ja) * | 1984-04-27 | 1985-11-16 | Kawatetsu Kohan Kk | 連続溶融金属メツキラインにおけるスナウト内金属浴面の夾雑物除去方法 |
-
1986
- 1986-02-28 JP JP1986029980U patent/JPH0318498Y2/ja not_active Expired
Also Published As
Publication number | Publication date |
---|---|
JPS62141059U (en:Method) | 1987-09-05 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US20020076502A1 (en) | Apparatus for hot dip galvanizing | |
CA3051026C (en) | Method and device for controlling flow of liquid zinc in zinc pot for hot-dip galvanization | |
JPH0318498Y2 (en:Method) | ||
JPH0126764Y2 (en:Method) | ||
JPH0126763Y2 (en:Method) | ||
JP2005171361A (ja) | 溶融金属めっきにおけるスナウト内浴面の異物除去装置 | |
JPH0892710A (ja) | 溶融亜鉛めっき浴中のドロス排出方法およびその装置 | |
JPH0248419Y2 (en:Method) | ||
JP5235655B2 (ja) | アルミニウム溶湯処理装置および方法 | |
JPS60114397A (ja) | 水処理装置 | |
JPH0523576Y2 (en:Method) | ||
JPS6026819B2 (ja) | 亜鉛回収用反応装置 | |
JP3399370B2 (ja) | 鋼帯の連続溶融金属めっき装置のスナウト | |
JP2010155255A (ja) | アルミニウム溶湯処理装置 | |
JP2928454B2 (ja) | 連続溶融金属めっき装置 | |
JP3180932B2 (ja) | 鋼板の連続溶融金属めっき装置 | |
JPS6393850A (ja) | 溶融亜鉛メツキ浴中の介在物除去方法 | |
JP2000265254A (ja) | 連続溶融金属メッキ設備の異物除去装置 | |
JPH076048B2 (ja) | ボトムドロス巻上げ防止方法および装置 | |
CN218089876U (zh) | 一种锌镍合金电镀液搅拌装置 | |
CN114567103B (zh) | 一种屏蔽永磁同步电机直连水车式增氧系统 | |
JPH0114676Y2 (en:Method) | ||
JP2516430B2 (ja) | 溶融金属めっき設備におけるポット内のドロス回収装置 | |
JPH0128931Y2 (en:Method) | ||
JPS6038669Y2 (ja) | 片面溶融亜鉛メツキ用噴流発生装置 |