JPH0317897B2 - - Google Patents

Info

Publication number
JPH0317897B2
JPH0317897B2 JP28517988A JP28517988A JPH0317897B2 JP H0317897 B2 JPH0317897 B2 JP H0317897B2 JP 28517988 A JP28517988 A JP 28517988A JP 28517988 A JP28517988 A JP 28517988A JP H0317897 B2 JPH0317897 B2 JP H0317897B2
Authority
JP
Japan
Prior art keywords
metal
melting point
plating
wire
copper
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP28517988A
Other languages
English (en)
Japanese (ja)
Other versions
JPH02133558A (ja
Inventor
Tatsuro Sakairi
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SANO KOGYO KK
Original Assignee
SANO KOGYO KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SANO KOGYO KK filed Critical SANO KOGYO KK
Priority to JP28517988A priority Critical patent/JPH02133558A/ja
Publication of JPH02133558A publication Critical patent/JPH02133558A/ja
Publication of JPH0317897B2 publication Critical patent/JPH0317897B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Coating With Molten Metal (AREA)
  • Other Surface Treatments For Metallic Materials (AREA)
JP28517988A 1988-11-11 1988-11-11 金属細管内面の溶融メッキ方法 Granted JPH02133558A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP28517988A JPH02133558A (ja) 1988-11-11 1988-11-11 金属細管内面の溶融メッキ方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP28517988A JPH02133558A (ja) 1988-11-11 1988-11-11 金属細管内面の溶融メッキ方法

Publications (2)

Publication Number Publication Date
JPH02133558A JPH02133558A (ja) 1990-05-22
JPH0317897B2 true JPH0317897B2 (enrdf_load_stackoverflow) 1991-03-11

Family

ID=17688126

Family Applications (1)

Application Number Title Priority Date Filing Date
JP28517988A Granted JPH02133558A (ja) 1988-11-11 1988-11-11 金属細管内面の溶融メッキ方法

Country Status (1)

Country Link
JP (1) JPH02133558A (enrdf_load_stackoverflow)

Families Citing this family (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CA2801874C (en) * 2010-06-09 2014-09-09 Sanoh Kogyo Kabushiki Kaisha Metal pipe for vehicle piping and method of surface-treating the same
JP6467195B2 (ja) 2014-11-10 2019-02-06 三桜工業株式会社 車輌配管用被覆金属管

Also Published As

Publication number Publication date
JPH02133558A (ja) 1990-05-22

Similar Documents

Publication Publication Date Title
US5553640A (en) Stainless steel strip plated with brazing alloy for multilayer tube manufacturing
GB2262460A (en) Method of manufacturing a multiple-walled tube.
CN106181106A (zh) 一种润湿先导的条状钎料及其制备方法
US2447980A (en) Method of making porous bearing surfaces
JPH0317897B2 (enrdf_load_stackoverflow)
EP1948388A1 (en) Lead-free solder alloy
JP2727184B2 (ja) 内表面にスズ又はスズ基合金が被覆された金属管の製造方法
US2586142A (en) Process for the production of lead coatings
JP4299591B2 (ja) 接合特性に優れた溶融Sn−Zn系めっき鋼板
US547381A (en) Robert mcknight
CN201586832U (zh) 一种用于二氧化碳气体保护焊的镀层焊丝
JPS6348948B2 (enrdf_load_stackoverflow)
JPS6018745B2 (ja) 金属細管内面の溶融メツキ方法
JP3341242B2 (ja) 耐食性銅管とその製造方法
JPH04214848A (ja) 溶融亜鉛メッキ被覆物及び溶融亜鉛メッキ方法
JP2964678B2 (ja) Zn−Al合金めっき方法
JPS6082676A (ja) 熱交換器用管の製造方法
GB2189256A (en) Strip or wire material
JPS61130489A (ja) 耐食性に富む熱交換器用銅合金管
JP3176404B2 (ja) 内面の耐食性に優れた溶接管の製造方法
JPS6260839A (ja) 表面処理用合金
JPH0219490A (ja) アルミニウム材の表面処理方法
JPS59166664A (ja) 耐熱亜鉛合金めつき製品
JPS6261667B2 (enrdf_load_stackoverflow)
JPS5825010A (ja) 電子部品用光沢めつきリ−ド線

Legal Events

Date Code Title Description
R250 Receipt of annual fees

Free format text: JAPANESE INTERMEDIATE CODE: R250

R250 Receipt of annual fees

Free format text: JAPANESE INTERMEDIATE CODE: R250

R250 Receipt of annual fees

Free format text: JAPANESE INTERMEDIATE CODE: R250

FPAY Renewal fee payment (prs date is renewal date of database)

Free format text: PAYMENT UNTIL: 20090311

Year of fee payment: 18

EXPY Cancellation because of completion of term
FPAY Renewal fee payment (prs date is renewal date of database)

Year of fee payment: 18

Free format text: PAYMENT UNTIL: 20090311