Prior art keywords
bath
master alloy
hot
plating
composition
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP10360484A
Other languages
English (en)
Japanese (ja)
Other versions
JPS60248855A (ja
Inventor
Hiroshi Kusuhashi
Kyoichi Fujinawa
Nobuhiro Tanaka
Yoshihiko Takano
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Sumitomo Metal Mining Co Ltd
Original Assignee
Sumitomo Metal Mining Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sumitomo Metal Mining Co Ltd filed Critical Sumitomo Metal Mining Co Ltd
Priority to JP10360484A priority Critical patent/JPS60248855A/ja
Publication of JPS60248855A publication Critical patent/JPS60248855A/ja
Publication of JPH0313296B2 publication Critical patent/JPH0313296B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Coating With Molten Metal (AREA)
JP10360484A 1984-05-24 1984-05-24 溶融亜鉛メツキ浴用ニツケル−亜鉛母合金 Granted JPS60248855A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP10360484A JPS60248855A (ja) 1984-05-24 1984-05-24 溶融亜鉛メツキ浴用ニツケル−亜鉛母合金

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP10360484A JPS60248855A (ja) 1984-05-24 1984-05-24 溶融亜鉛メツキ浴用ニツケル−亜鉛母合金

Publications (2)

Publication Number Publication Date
JPS60248855A JPS60248855A (ja) 1985-12-09
JPH0313296B2 true JPH0313296B2 (fr) 1991-02-22

Family

ID=14358374

Family Applications (1)

Application Number Title Priority Date Filing Date
JP10360484A Granted JPS60248855A (ja) 1984-05-24 1984-05-24 溶融亜鉛メツキ浴用ニツケル−亜鉛母合金

Country Status (1)

Country Link
JP (1) JPS60248855A (fr)

Families Citing this family (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US5441628A (en) * 1992-09-15 1995-08-15 Japan Energy Corporation Method for preparation for a Zn-Ni electroplating or hot-dip galvanizing bath using a Zn-Ni alloy, and method for producing a Zn-Ni alloy
CN105483591B (zh) * 2015-12-23 2018-12-07 常州大学 热浸镀用Zn-Al-Si-Ni合金镀层及热浸镀方法

Also Published As

Publication number Publication date
JPS60248855A (ja) 1985-12-09

Similar Documents

Publication Publication Date Title
WO2019009003A1 (fr) TÔLE D'ACIER PLAQUÉE DE Zn-Al-Mg FONDUS PRÉSENTANT UN EXCELLENT ASPECT DE SURFACE ET SON PROCÉDÉ DE PRODUCTION
CN106480338A (zh) 用于调整热浸镀液成分的锌铝镁合金及其直接熔炼方法
US2253502A (en) Malleable iron
JPS6350421B2 (fr)
JPS591653A (ja) ラジエ−タ−フイン用銅合金
CN103924123A (zh) 一种低铝热浸镀Zn-Al-Mg-Si合金及其制备方法
JPH0313296B2 (fr)
US2368128A (en) Terne coating process
CN107619974B (zh) 一种高强度高弹性模量铝合金及其制备方法
JP4287594B2 (ja) アルミニウム合金溶融物の処理
JP4399572B2 (ja) ニッケル−亜鉛母合金の製造方法
JP2964678B2 (ja) Zn−Al合金めっき方法
JPH0138869B2 (fr)
JPH11189857A (ja) 鉄鋼材料の溶融亜鉛二段めっき法
JPS61201743A (ja) 溶融メツキ用高耐食性高加工性Zn合金の製造法
JPH05117830A (ja) 溶融亜鉛−アルミニウム合金めつき法
JP2004353022A (ja) 溶融Zn−Al系合金めっき鋼材およびその製造方法
JPH03173754A (ja) 溶融亜鉛めっき浴組成物
JPS6144930B2 (fr)
JP2640405B2 (ja) 耐蝕性マグネシウム合金
JPH02282435A (ja) ニッケルを含有した亜鉛母合金の製造方法
JPH0353051A (ja) 溶融亜鉛めっき処理用のめっき浴
JPH03100152A (ja) 溶融Zn‐Al合金めっき用フラックス
JPH0372059A (ja) 溶融亜鉛めっき浴組成物
JPH03281766A (ja) 含アルミニゥム・亜鉛合金の溶融めっき方法

Legal Events

Date Code Title Description
EXPY Cancellation because of completion of term