JPH0271827A - エチレンビニルアルコール系共重合体中空糸膜の製造法 - Google Patents
エチレンビニルアルコール系共重合体中空糸膜の製造法Info
- Publication number
- JPH0271827A JPH0271827A JP22509388A JP22509388A JPH0271827A JP H0271827 A JPH0271827 A JP H0271827A JP 22509388 A JP22509388 A JP 22509388A JP 22509388 A JP22509388 A JP 22509388A JP H0271827 A JPH0271827 A JP H0271827A
- Authority
- JP
- Japan
- Prior art keywords
- vinyl alcohol
- alcohol copolymer
- water
- soln
- ethylene
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- External Artificial Organs (AREA)
- Separation Using Semi-Permeable Membranes (AREA)
- Artificial Filaments (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP22509388A JPH0271827A (ja) | 1988-09-07 | 1988-09-07 | エチレンビニルアルコール系共重合体中空糸膜の製造法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP22509388A JPH0271827A (ja) | 1988-09-07 | 1988-09-07 | エチレンビニルアルコール系共重合体中空糸膜の製造法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPH0271827A true JPH0271827A (ja) | 1990-03-12 |
JPH0578372B2 JPH0578372B2 (enrdf_load_stackoverflow) | 1993-10-28 |
Family
ID=16823887
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP22509388A Granted JPH0271827A (ja) | 1988-09-07 | 1988-09-07 | エチレンビニルアルコール系共重合体中空糸膜の製造法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPH0271827A (enrdf_load_stackoverflow) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2001038169A (ja) * | 1999-08-03 | 2001-02-13 | Kuraray Co Ltd | 血漿成分分離膜 |
-
1988
- 1988-09-07 JP JP22509388A patent/JPH0271827A/ja active Granted
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2001038169A (ja) * | 1999-08-03 | 2001-02-13 | Kuraray Co Ltd | 血漿成分分離膜 |
Also Published As
Publication number | Publication date |
---|---|
JPH0578372B2 (enrdf_load_stackoverflow) | 1993-10-28 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US4269713A (en) | Ethylene-vinyl alcohol copolymer membrane and a method for producing the same | |
US5976433A (en) | Polyvinyl alcohol-based hollow fiber membrane and process for producing the same | |
US4385094A (en) | Ethylene-vinyl alcohol hollow fiber membrane and method for the production thereof | |
JPS61257203A (ja) | 親水性多孔質膜およびその製造方法 | |
WO1992009359A1 (en) | Large-pore-diameter porous hollow yarn membrane of polyethylene, production thereof, and hydrophilic porous hollow yarn membrane of polyethylene | |
JPS6214642B2 (enrdf_load_stackoverflow) | ||
JPH0549878A (ja) | 大孔径多孔質ポリエチレン中空糸膜、その製造方法及び親水化多孔質ポリエチレン中空糸膜 | |
JPS61164602A (ja) | ポリスルホン系樹脂製中空糸膜 | |
JP2003010654A (ja) | 中空糸膜の製造方法 | |
JPH0271827A (ja) | エチレンビニルアルコール系共重合体中空糸膜の製造法 | |
JP3203047B2 (ja) | エチレンビニルアルコール系共重合体中空糸膜の製造法 | |
JPH0371144B2 (enrdf_load_stackoverflow) | ||
JP2572895B2 (ja) | 多孔質中空糸膜の製造法 | |
JPS5836602B2 (ja) | エチレン−ビニルアルコ−ル系共重合体膜およびその製法 | |
JPH07185278A (ja) | 分離膜の製造方法 | |
JPH0578373B2 (enrdf_load_stackoverflow) | ||
JPS6320339A (ja) | 多孔質膜の製造方法 | |
JPH1057787A (ja) | 分離膜とその製造方法 | |
JPH0952030A (ja) | ポリビニルアルコール系中空繊維膜及びその製造方法 | |
JP4794716B2 (ja) | 中空糸膜およびその製造方法 | |
JPH0938473A (ja) | ポリスルホン系多孔質中空糸膜の製造方法 | |
JPH04222204A (ja) | ポリアクリロニトリル中空糸 | |
JPH0924261A (ja) | ポリスルホン系多孔質中空糸膜の製造方法 | |
JP2000237558A (ja) | 高性能選択透過性中空糸膜 | |
JP3537539B2 (ja) | ビニルアルコール系共重合体中空糸膜の製造方法 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
LAPS | Cancellation because of no payment of annual fees |