JPH0257561B2 - - Google Patents
Info
- Publication number
- JPH0257561B2 JPH0257561B2 JP57175872A JP17587282A JPH0257561B2 JP H0257561 B2 JPH0257561 B2 JP H0257561B2 JP 57175872 A JP57175872 A JP 57175872A JP 17587282 A JP17587282 A JP 17587282A JP H0257561 B2 JPH0257561 B2 JP H0257561B2
- Authority
- JP
- Japan
- Prior art keywords
- vinyl chloride
- polymerization
- containing compound
- weight
- group
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Polymerisation Methods In General (AREA)
- Polymerization Catalysts (AREA)
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP57175872A JPS5964607A (ja) | 1982-10-06 | 1982-10-06 | 塩化ビニル樹脂の製造方法 |
| JP4197409A JPH0641209A (ja) | 1982-10-06 | 1992-07-02 | 塩化ビニル樹脂の製造方法 |
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP57175872A JPS5964607A (ja) | 1982-10-06 | 1982-10-06 | 塩化ビニル樹脂の製造方法 |
| JP4197409A JPH0641209A (ja) | 1982-10-06 | 1992-07-02 | 塩化ビニル樹脂の製造方法 |
Related Child Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP4197409A Division JPH0641209A (ja) | 1982-10-06 | 1992-07-02 | 塩化ビニル樹脂の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5964607A JPS5964607A (ja) | 1984-04-12 |
| JPH0257561B2 true JPH0257561B2 (enExample) | 1990-12-05 |
Family
ID=26496991
Family Applications (2)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP57175872A Granted JPS5964607A (ja) | 1982-10-06 | 1982-10-06 | 塩化ビニル樹脂の製造方法 |
| JP4197409A Ceased JPH0641209A (ja) | 1982-10-06 | 1992-07-02 | 塩化ビニル樹脂の製造方法 |
Family Applications After (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP4197409A Ceased JPH0641209A (ja) | 1982-10-06 | 1992-07-02 | 塩化ビニル樹脂の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (2) | JPS5964607A (enExample) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0696616B2 (ja) * | 1987-03-19 | 1994-11-30 | チッソ株式会社 | 塩化ビニル重合体の製造方法 |
| WO2017191899A1 (ko) * | 2016-05-03 | 2017-11-09 | 주식회사 엘지화학 | 염화비닐계 중합체의 제조방법 및 이에 따라 제조된 염화비닐계 중합체 |
| KR101969074B1 (ko) * | 2016-05-03 | 2019-04-16 | 주식회사 엘지화학 | 염화비닐계 중합체의 제조방법 및 이에 따라 제조된 염화비닐계 중합체 |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2691282B2 (ja) * | 1988-08-12 | 1997-12-17 | 日本製箔株式会社 | 開封性に優れた包装体 |
-
1982
- 1982-10-06 JP JP57175872A patent/JPS5964607A/ja active Granted
-
1992
- 1992-07-02 JP JP4197409A patent/JPH0641209A/ja not_active Ceased
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0641209A (ja) | 1994-02-15 |
| JPS5964607A (ja) | 1984-04-12 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP0287757B1 (en) | Crosslinked porous skinless particles of PVC resin and process for producing same | |
| US4612345A (en) | Hydroxypropyl methyl cellulose ethers useful as suspending agents for suspension polymerization of vinyl chloride | |
| JPH0832729B2 (ja) | ビニルモノマ−の重合方法及び多孔性ポリ塩化ビニル樹脂粒子の製造方法 | |
| JPS6410004B2 (enExample) | ||
| US3813373A (en) | Method for producing high bulk density polyvinyl chloride | |
| EP0061134B1 (en) | Improved polyvinyl chloride and preparation thereof | |
| US2812318A (en) | Method for granular polymerization of vinyl chloride | |
| JPH06107712A (ja) | 塩化ビニル系重合体の製造方法 | |
| JPH0641209A (ja) | 塩化ビニル樹脂の製造方法 | |
| JP3169673B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| JPS58168644A (ja) | ゲル化特性の優れたポリ塩化ビニルと高分子可塑剤から成る組成物 | |
| EP0015586B1 (en) | Process for the suspension polymerization of polyvinyl chloride | |
| JP3239613B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| EP0289933B1 (en) | Graft polymerization precurser and method manufacturing the same | |
| JP3340492B2 (ja) | ビニル系化合物の懸濁重合用分散助剤 | |
| JPH0370703A (ja) | 塩化ビニル系重合体の製造方法 | |
| JPH10503544A (ja) | 塩化ビニルコポリマー及びその製造方法 | |
| JPS6124047B2 (enExample) | ||
| JPS58206609A (ja) | 懸濁重合による塩化ビニルのポリマ−及びコポリマ−の製法及びペ−スト形成性塩化ビニルポリマ−及び塩化ビニルコポリマ−からなる懸濁液の粘度低下法 | |
| JP3385643B2 (ja) | 塩化ビニル系重合体の製造方法 | |
| US4963592A (en) | Super porous low molecular weight vinyl halide resins | |
| JP3066136B2 (ja) | 分散剤 | |
| JPH0892305A (ja) | 塩化ビニル系樹脂の製造方法 | |
| EP0442737B1 (en) | Method for the preparation of a polyvinyl chloride resin | |
| JP3241883B2 (ja) | 塩化ビニル系単量体の重合方法 |