JPH02229712A - 水酸化マグネシウムの製法 - Google Patents
水酸化マグネシウムの製法Info
- Publication number
- JPH02229712A JPH02229712A JP1501790A JP1501790A JPH02229712A JP H02229712 A JPH02229712 A JP H02229712A JP 1501790 A JP1501790 A JP 1501790A JP 1501790 A JP1501790 A JP 1501790A JP H02229712 A JPH02229712 A JP H02229712A
- Authority
- JP
- Japan
- Prior art keywords
- slaked lime
- quicklime
- slurry
- ions
- aqueous solution
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C01—INORGANIC CHEMISTRY
- C01F—COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS
- C01F5/00—Compounds of magnesium
- C01F5/14—Magnesium hydroxide
- C01F5/22—Magnesium hydroxide from magnesium compounds with alkali hydroxides or alkaline- earth oxides or hydroxides
Landscapes
- Chemical & Material Sciences (AREA)
- Organic Chemistry (AREA)
- Life Sciences & Earth Sciences (AREA)
- Geology (AREA)
- Inorganic Chemistry (AREA)
- Compounds Of Alkaline-Earth Elements, Aluminum Or Rare-Earth Metals (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1501790A JPH02229712A (ja) | 1990-01-26 | 1990-01-26 | 水酸化マグネシウムの製法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1501790A JPH02229712A (ja) | 1990-01-26 | 1990-01-26 | 水酸化マグネシウムの製法 |
Related Parent Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP56108823A Division JPS5815030A (ja) | 1981-07-14 | 1981-07-14 | 消石灰 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH02229712A true JPH02229712A (ja) | 1990-09-12 |
| JPH0345011B2 JPH0345011B2 (enFirst) | 1991-07-09 |
Family
ID=11877099
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1501790A Granted JPH02229712A (ja) | 1990-01-26 | 1990-01-26 | 水酸化マグネシウムの製法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH02229712A (enFirst) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2007500116A (ja) * | 2003-07-28 | 2007-01-11 | ソシエテ アノニム ロワスト レシェルシュ エ デブロプマン | カルシウム−マグネシウム含有水性懸濁液及びその調製方法 |
| JP2007302555A (ja) * | 2007-06-26 | 2007-11-22 | Kaisui Kagaku Kenkyusho:Kk | 水酸化カルシウム系化合物及びその製造方法 |
| JP2011195384A (ja) * | 2010-03-19 | 2011-10-06 | Fujifilm Corp | 金属水酸化物微粒子の製造方法 |
Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS567545A (en) * | 1979-07-02 | 1981-01-26 | Nec Corp | Parity check circuit |
| JPS6218742U (enFirst) * | 1985-07-13 | 1987-02-04 | ||
| JPS6231724A (ja) * | 1985-08-02 | 1987-02-10 | Toyota Motor Corp | 等速ジヨイント付プロペラシヤフトのバランス取り方法 |
-
1990
- 1990-01-26 JP JP1501790A patent/JPH02229712A/ja active Granted
Patent Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS567545A (en) * | 1979-07-02 | 1981-01-26 | Nec Corp | Parity check circuit |
| JPS6218742U (enFirst) * | 1985-07-13 | 1987-02-04 | ||
| JPS6231724A (ja) * | 1985-08-02 | 1987-02-10 | Toyota Motor Corp | 等速ジヨイント付プロペラシヤフトのバランス取り方法 |
Cited By (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2007500116A (ja) * | 2003-07-28 | 2007-01-11 | ソシエテ アノニム ロワスト レシェルシュ エ デブロプマン | カルシウム−マグネシウム含有水性懸濁液及びその調製方法 |
| JP4842813B2 (ja) * | 2003-07-28 | 2011-12-21 | ソシエテ アノニム ロワスト レシェルシュ エ デブロプマン | 水性懸濁液及びその調製方法 |
| US8206680B2 (en) | 2003-07-28 | 2012-06-26 | S.A. Lhoist Recherche Et Developpement | Calco-magnesian aqueous suspension and method for the production thereof |
| JP2007302555A (ja) * | 2007-06-26 | 2007-11-22 | Kaisui Kagaku Kenkyusho:Kk | 水酸化カルシウム系化合物及びその製造方法 |
| JP2011195384A (ja) * | 2010-03-19 | 2011-10-06 | Fujifilm Corp | 金属水酸化物微粒子の製造方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0345011B2 (enFirst) | 1991-07-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4539195A (en) | Basic magnesium aluminum hydroxycarbonate | |
| US4981675A (en) | Polymeric basic aluminum silicate-sulphate | |
| US4472370A (en) | Processes for the production of slaked lime and magnesium hydroxide | |
| US5021192A (en) | Colloidal dispersions of cerium (IV) compound | |
| US3497459A (en) | Process for producing water soluble basic salts of aluminum and/or iron | |
| JP2574735B2 (ja) | 新規なポリアルミニウムクロロ硫酸塩と、その合成方法と、その応用 | |
| JP2681464B2 (ja) | 新規なセリウム▲iv▼化合物の製造方法 | |
| EP0541329B1 (en) | Composite metal hydroxide and process for the production thereof | |
| US4404169A (en) | Process for producing cupric hydroxide | |
| JP3674009B2 (ja) | 無定形酸化チタンゾルの製造方法 | |
| JPH02229712A (ja) | 水酸化マグネシウムの製法 | |
| US4490337A (en) | Preparation of cupric hydroxide | |
| JP4330182B2 (ja) | 炭酸型ハイドロカルマイトの合成方法 | |
| DE69402270T2 (de) | Getrocknetes Aluminiumhydroxydgel, Verfahren zu seiner Herstellung und Antisäure | |
| KR920003219B1 (ko) | 제올라이트의 제조방법 | |
| CN111792678B (zh) | 一种纯钴类水滑石化合物及其制备方法 | |
| JPS62288104A (ja) | 固体状の塩基性金属ヒドロキシ硫酸塩錯体及びその製造方法 | |
| US4294810A (en) | Alkali calcium silicates and process for preparation thereof | |
| JPH072505A (ja) | ヒドロキシアパタイトの製造方法 | |
| JPH10245220A (ja) | 塩基性塩化アルミニウム及びその製造方法 | |
| US4447351A (en) | Preparation of alumina hydrosol from aluminum sulfate solution | |
| KR100192711B1 (ko) | 은 함유 무기 항균제의 제조방법 | |
| JPH0632611A (ja) | 塩基性硫酸アルミニウム水溶液及びその製造方法 | |
| JPH0258209B2 (enFirst) | ||
| JPH0258205B2 (enFirst) |