JPH0217228B2 - - Google Patents
Info
- Publication number
- JPH0217228B2 JPH0217228B2 JP61026620A JP2662086A JPH0217228B2 JP H0217228 B2 JPH0217228 B2 JP H0217228B2 JP 61026620 A JP61026620 A JP 61026620A JP 2662086 A JP2662086 A JP 2662086A JP H0217228 B2 JPH0217228 B2 JP H0217228B2
- Authority
- JP
- Japan
- Prior art keywords
- coal ash
- iron
- pressure steam
- stabilizing
- iron chloride
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Processing Of Solid Wastes (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP61026620A JPS62183896A (ja) | 1986-02-07 | 1986-02-07 | 石炭灰の安定化方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP61026620A JPS62183896A (ja) | 1986-02-07 | 1986-02-07 | 石炭灰の安定化方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS62183896A JPS62183896A (ja) | 1987-08-12 |
JPH0217228B2 true JPH0217228B2 (enrdf_load_stackoverflow) | 1990-04-19 |
Family
ID=12198514
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP61026620A Granted JPS62183896A (ja) | 1986-02-07 | 1986-02-07 | 石炭灰の安定化方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS62183896A (enrdf_load_stackoverflow) |
Families Citing this family (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2741645B2 (ja) * | 1992-09-08 | 1998-04-22 | 新日本製鐵株式会社 | 重金属含有灰の処理方法 |
NL9202033A (nl) * | 1992-11-23 | 1994-06-16 | Tauw Milieu Bv | Werkwijze voor de behandeling van verbrandingsresiduen en de toepassing daarvan als adsorptiemiddel. |
JP3969617B2 (ja) * | 1998-07-21 | 2007-09-05 | 不二倉業株式会社 | 有害物質固定化材 |
JP4789411B2 (ja) * | 2003-11-10 | 2011-10-12 | 川崎重工業株式会社 | 廃棄物の安定化処理物及び処理装置 |
JP4835359B2 (ja) * | 2005-09-30 | 2011-12-14 | 宇部興産株式会社 | 石炭灰造粒砂および石炭灰造粒砂の製造方法 |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5178078A (en) * | 1974-12-28 | 1976-07-07 | Betsuku Kk | Jinkaishokyakubainoshorihoho |
JPS5644085A (en) * | 1979-06-29 | 1981-04-23 | Nippon Jiryoku Senko Kk | Processing method of chromium-containing dust |
-
1986
- 1986-02-07 JP JP61026620A patent/JPS62183896A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS62183896A (ja) | 1987-08-12 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB2042025A (en) | Strengthening soft soil | |
JP2005146275A (ja) | 土壌、土質改良及び固化安定剤 | |
CN101502840B (zh) | 固体危险废物无害化处理工艺 | |
JP4209223B2 (ja) | 六価クロムの溶出抑制方法 | |
CN112495984B (zh) | 一种危险废物固化/稳定化综合处理方法 | |
JPH0217228B2 (enrdf_load_stackoverflow) | ||
JP3919648B2 (ja) | 有害重金属捕集材 | |
JPH10137716A (ja) | 廃棄物処理材および廃棄物処理方法 | |
CN102335494B (zh) | 含重金属粉尘的重金属稳定化处理方法 | |
JP2006015290A (ja) | 混合、混練装置を用いない飛灰中の重金属固定化処理方法 | |
JP2000093927A (ja) | 有害物質固定化材 | |
JP2008255171A (ja) | 無機系有害成分の固定化剤 | |
JP2004305833A (ja) | 廃棄物の安定化処理方法 | |
JP2006102643A (ja) | 硫化カルシウム系重金属固定化剤、及びその製造方法、並びに地盤改良材の製造方法、及び処理対象物の処理方法 | |
JP3675766B2 (ja) | 環境改善セメント組成物 | |
JP3213054B2 (ja) | 重金属含有焼却灰の処理方法 | |
JPH0154111B2 (enrdf_load_stackoverflow) | ||
JP4516780B2 (ja) | 重金属固定化材、セメント系固化材、重金属固定化材の製造方法、地盤改良材の製造方法、及び処理対象土の処理方法 | |
JP4129832B2 (ja) | 泥土改良固化安定剤 | |
JP2001121109A (ja) | 可溶性六価クロムを含有する構築物廃材の無害化処理方法 | |
JP5077777B2 (ja) | 溶出低減材および溶出低減処理方法 | |
JP5470699B2 (ja) | 重金属含有塩基性廃棄物の無害化処理方法 | |
JPH01262978A (ja) | 廃棄物の焼却で生ずる固形体残留物中の鉛およびカドミウムを石灰およびホスフェートを用いて、固定化する方法 | |
JPH10180224A (ja) | 廃棄物焼却飛灰中の重金属固定化剤及び無害化処理方法 | |
JP5599574B2 (ja) | 焼却灰からの土壌改良材およびその製造方法 |