JPH0156125B2 - - Google Patents

Info

Publication number
JPH0156125B2
JPH0156125B2 JP60002814A JP281485A JPH0156125B2 JP H0156125 B2 JPH0156125 B2 JP H0156125B2 JP 60002814 A JP60002814 A JP 60002814A JP 281485 A JP281485 A JP 281485A JP H0156125 B2 JPH0156125 B2 JP H0156125B2
Authority
JP
Japan
Prior art keywords
wall thickness
steel
less
corrosion cracking
stress corrosion
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP60002814A
Other languages
English (en)
Japanese (ja)
Other versions
JPS61163215A (ja
Inventor
Kuniaki Motoda
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JFE Steel Corp
Original Assignee
Kawasaki Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kawasaki Steel Corp filed Critical Kawasaki Steel Corp
Priority to JP281485A priority Critical patent/JPS61163215A/ja
Publication of JPS61163215A publication Critical patent/JPS61163215A/ja
Publication of JPH0156125B2 publication Critical patent/JPH0156125B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Heat Treatment Of Steel (AREA)
  • Heat Treatment Of Articles (AREA)
JP281485A 1985-01-11 1985-01-11 耐サワ−性の優れた極厚肉高強度継目無鋼管の製造方法 Granted JPS61163215A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP281485A JPS61163215A (ja) 1985-01-11 1985-01-11 耐サワ−性の優れた極厚肉高強度継目無鋼管の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP281485A JPS61163215A (ja) 1985-01-11 1985-01-11 耐サワ−性の優れた極厚肉高強度継目無鋼管の製造方法

Publications (2)

Publication Number Publication Date
JPS61163215A JPS61163215A (ja) 1986-07-23
JPH0156125B2 true JPH0156125B2 (https=) 1989-11-29

Family

ID=11539862

Family Applications (1)

Application Number Title Priority Date Filing Date
JP281485A Granted JPS61163215A (ja) 1985-01-11 1985-01-11 耐サワ−性の優れた極厚肉高強度継目無鋼管の製造方法

Country Status (1)

Country Link
JP (1) JPS61163215A (https=)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
SE525378C2 (sv) * 2002-01-21 2005-02-08 Sandvik Ab Element för slående bergborrning och metod för dess framställning
CN102330030B (zh) * 2011-10-14 2013-02-20 天津钢管集团股份有限公司 直径559~711mm车载高压气瓶用无缝钢管及生产方法
CN106756500B (zh) * 2016-12-26 2018-10-02 天津钢管集团股份有限公司 高强度高韧性气瓶用无缝钢管及生产方法

Family Cites Families (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5996217A (ja) * 1982-11-24 1984-06-02 Sumitomo Metal Ind Ltd 耐硫化物割れ性に優れた鋼の製造方法
JPS5996216A (ja) * 1982-11-24 1984-06-02 Sumitomo Metal Ind Ltd 耐硫化物割れ性の優れた高強度鋼の製造方法

Also Published As

Publication number Publication date
JPS61163215A (ja) 1986-07-23

Similar Documents

Publication Publication Date Title
EA019473B1 (ru) Низколегированная сталь с высокой прочностью на разрыв и высокой стойкостью к сульфидному растрескиванию под напряжением
AU2017226127B2 (en) Steel material and oil-well steel pipe
JP5499575B2 (ja) 油井管用マルテンサイト系ステンレス継目無鋼管およびその製造方法
AU2003295014A1 (en) Method for making an abrasion resistant steel plate and plate obtained
EP1862561A1 (en) Steel for oil well pipe having excellent sulfide stress cracking resistance and method for manufacturing seamless steel pipe for oil well
JP7173405B2 (ja) マルテンサイト系ステンレス鋼材
BR112021010529A2 (pt) Aço laminado a quente, folha de aço laminada a quente, método de produção de um aço laminado a quente, uso de um aço e tubo sem emenda
WO2017150251A1 (ja) 鋼材及び油井用鋼管
JPS60174822A (ja) 厚肉高強度継目無鋼管の製造方法
JP7173404B2 (ja) マルテンサイト系ステンレス鋼材
US2532117A (en) Nickel steel alloys
JPS64455B2 (https=)
US10487373B2 (en) Steel pipe for line pipe and method of manufacturing the same
JPS63230847A (ja) 耐食性に優れた油井管用低合金鋼
JPH05287381A (ja) 高強度耐食性鋼管の製造方法
US5858128A (en) High chromium martensitic steel pipe having excellent pitting resistance and method of manufacturing
JPH02243740A (ja) 油井用マルテンサイト系ステンレス鋼材とその製造方法
JPH09241746A (ja) 高強度二相ステンレス鋼管の製造方法
JPH10287924A (ja) マルテンサイト単相のステンレス鋼管の製造方法
JPH0156125B2 (https=)
EP0224591A1 (en) Process for producing high-strength seamless steel pipes excellent in sulfide stress corrosion cracking resistance
JPH0348261B2 (https=)
JPH0360904B2 (https=)
JP7445173B2 (ja) 鋼材
JPS6216250B2 (https=)