JP3449428B2 - 半導体装置の製造方法 - Google Patents
半導体装置の製造方法Info
- Publication number
- JP3449428B2 JP3449428B2 JP13361893A JP13361893A JP3449428B2 JP 3449428 B2 JP3449428 B2 JP 3449428B2 JP 13361893 A JP13361893 A JP 13361893A JP 13361893 A JP13361893 A JP 13361893A JP 3449428 B2 JP3449428 B2 JP 3449428B2
- Authority
- JP
- Japan
- Prior art keywords
- gas
- film
- refractory metal
- chamber
- tin
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C16/00—Chemical coating by decomposition of gaseous compounds, without leaving reaction products of surface material in the coating, i.e. chemical vapour deposition [CVD] processes
- C23C16/22—Chemical coating by decomposition of gaseous compounds, without leaving reaction products of surface material in the coating, i.e. chemical vapour deposition [CVD] processes characterised by the deposition of inorganic material, other than metallic material
- C23C16/30—Deposition of compounds, mixtures or solid solutions, e.g. borides, carbides, nitrides
- C23C16/34—Nitrides
Landscapes
- Electrodes Of Semiconductors (AREA)
- Internal Circuitry In Semiconductor Integrated Circuit Devices (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13361893A JP3449428B2 (ja) | 1992-06-08 | 1993-06-03 | 半導体装置の製造方法 |
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14765692 | 1992-06-08 | ||
| JP4-147656 | 1992-06-08 | ||
| JP13361893A JP3449428B2 (ja) | 1992-06-08 | 1993-06-03 | 半導体装置の製造方法 |
Related Child Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2003036183A Division JP4012090B2 (ja) | 1992-06-08 | 2003-02-14 | 高融点金属窒化膜の堆積方法及び半導体装置の製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH0661229A JPH0661229A (ja) | 1994-03-04 |
| JPH0661229A5 JPH0661229A5 (enExample) | 2001-03-16 |
| JP3449428B2 true JP3449428B2 (ja) | 2003-09-22 |
Family
ID=26467931
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP13361893A Expired - Fee Related JP3449428B2 (ja) | 1992-06-08 | 1993-06-03 | 半導体装置の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3449428B2 (enExample) |
Families Citing this family (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5591483A (en) * | 1994-08-31 | 1997-01-07 | Wayne State University | Process for the preparation of metal nitride coatings from single source precursors |
| US6891269B1 (en) | 1995-07-05 | 2005-05-10 | Fujitsu Limited | Embedded electroconductive layer structure |
| US5895267A (en) * | 1997-07-09 | 1999-04-20 | Lsi Logic Corporation | Method to obtain a low resistivity and conformity chemical vapor deposition titanium film |
| US6107192A (en) * | 1997-12-30 | 2000-08-22 | Applied Materials, Inc. | Reactive preclean prior to metallization for sub-quarter micron application |
| KR20010075977A (ko) * | 2000-01-21 | 2001-08-11 | 윤덕용 | 부가 단량체 단일선구물질을 이용한 13 족 질화물 박막의제조방법 |
| JP4656525B2 (ja) * | 2006-04-24 | 2011-03-23 | 株式会社沖データ | 半導体装置、ledヘッド及び画像形成装置 |
| CN102365386A (zh) * | 2009-03-27 | 2012-02-29 | 东京毅力科创株式会社 | 金属氮化膜的成膜方法和存储介质 |
-
1993
- 1993-06-03 JP JP13361893A patent/JP3449428B2/ja not_active Expired - Fee Related
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0661229A (ja) | 1994-03-04 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR960008150B1 (ko) | 고융점 금속 질화물의 증착방법 및 고융점 금속 질화물을 함유하는 전도막의 형성방법 | |
| US7521379B2 (en) | Deposition and densification process for titanium nitride barrier layers | |
| US5498768A (en) | Process for forming multilayer wiring | |
| US5906866A (en) | Process for chemical vapor deposition of tungsten onto a titanium nitride substrate surface | |
| US6171943B1 (en) | Methods of forming a contact having titanium silicide formed by chemical vapor deposition | |
| US20020114886A1 (en) | Method of tisin deposition using a chemical vapor deposition process | |
| US5747384A (en) | Process of forming a refractory metal thin film | |
| US6475912B1 (en) | Semiconductor device and method and apparatus for fabricating the same while minimizing operating failures and optimizing yield | |
| US6933021B2 (en) | Method of TiSiN deposition using a chemical vapor deposition (CVD) process | |
| EP0732731A2 (en) | Treatment of a titanium nitride layer to improve resistance to elevated temperatures | |
| JPH05209279A (ja) | 金属膜形成装置および金属膜形成法 | |
| KR100259692B1 (ko) | 매립형 접촉 구조를 가진 반도체 장치의 제조 방법 | |
| US6197674B1 (en) | CVD-Ti film forming method | |
| KR19990014078A (ko) | Cvd 장치의 챔버 클리닝 방법 | |
| JP3208124B2 (ja) | 半導体装置、半導体装置の製造方法、および半導体装置の製造装置 | |
| JPH0661229A (ja) | 半導体装置の製造方法 | |
| US6444556B2 (en) | Chemistry for chemical vapor deposition of titanium containing films | |
| JPH08279558A (ja) | 半導体装置の製造方法 | |
| JP4308867B2 (ja) | 高融点金属窒化膜の形成方法 | |
| JP3138892B2 (ja) | 薄膜形成方法及びその装置 | |
| JP4012090B2 (ja) | 高融点金属窒化膜の堆積方法及び半導体装置の製造方法 | |
| US6537621B1 (en) | Method of forming a titanium film and a barrier film on a surface of a substrate through lamination | |
| JPH0238568A (ja) | 薄膜形成装置 | |
| JPH03110840A (ja) | 堆積膜形成法 | |
| JP4312291B2 (ja) | プラズマcvdによる成膜方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| A01 | Written decision to grant a patent or to grant a registration (utility model) |
Free format text: JAPANESE INTERMEDIATE CODE: A01 Effective date: 20030624 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20080711 Year of fee payment: 5 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20090711 Year of fee payment: 6 |
|
| LAPS | Cancellation because of no payment of annual fees |