JP2813514B2 - 多孔質無機質板 - Google Patents

多孔質無機質板

Info

Publication number
JP2813514B2
JP2813514B2 JP4262272A JP26227292A JP2813514B2 JP 2813514 B2 JP2813514 B2 JP 2813514B2 JP 4262272 A JP4262272 A JP 4262272A JP 26227292 A JP26227292 A JP 26227292A JP 2813514 B2 JP2813514 B2 JP 2813514B2
Authority
JP
Japan
Prior art keywords
porous inorganic
inorganic
inorganic plate
substrate
coating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP4262272A
Other languages
English (en)
Other versions
JPH06108583A (ja
Inventor
聡 北川
仁 熊谷
Original Assignee
ナショナル住宅産業株式会社
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ナショナル住宅産業株式会社 filed Critical ナショナル住宅産業株式会社
Priority to JP4262272A priority Critical patent/JP2813514B2/ja
Publication of JPH06108583A publication Critical patent/JPH06108583A/ja
Application granted granted Critical
Publication of JP2813514B2 publication Critical patent/JP2813514B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Description

【発明の詳細な説明】
【0001】
【産業上の利用分野】この発明は、建造物の外装材等と
して使用される多孔質無機質板に関するものであり、詳
しくは表面の塗装構造に工夫がなされた多孔質無機質板
に関する。
【0002】
【従来の技術】多孔質無機質板は、外装用の建材として
一般に広く用いられている。多孔質無機質板の一例とし
て、たとえば、ALC(Autoclaved Light weight Conc
rete)等の気泡コンクリートが挙げられる。ALCは、
軽量で断熱性、耐火性に優れており、屋根、内外壁、床
等に使用されている。
【0003】従来、多孔質無機質板には、その表面の化
粧仕上げとして有機塗装処理を行っていた。ところが、
有機塗膜は、耐侯性に劣るという問題点があった。
【0004】
【発明が解決しようとする課題】上記問題点に対して、
耐侯性に優れる無機塗料の使用が考えられる。しかし、
多孔質無機質板の表面には孔や凹凸があるため、無機塗
料の塗布に先立って、多孔質無機質板の表面を平滑に仕
上げる必要がある。そこで、この発明は、基体表面を平
滑に仕上げて無機塗料の塗布を可能にすることにより、
耐侯性に優れた塗装仕上げ表面を有する多孔質無機質板
を提供することを課題とする。
【0005】
【課題を解決するための手段】この発明にかかる多孔質
無機質板は、基体表面に目止め処理による平滑仕上げが
なされ、その上に無機塗料による塗装仕上げがなされて
いる。この発明にかかる多孔質無機質板の基体として
は、たとえば、ALC等の気泡コンクリート板、発泡ガ
ラス板等が挙げられる。
【0006】目止め処理は、基体の表面に、まずフィラ
ー層を形成させ、その上に強化シーラーを塗装すること
により行う。フィラーとしては、たとえば、炭酸カルシ
ウム系、マイカ系、クレー系(粘土質系体質顔料)、硫
酸マグネシウム系のものが挙げられる。塗布量は2〜3
kg/m2 が望ましい。フィラー層を形成させることによ
って、基体表面が平滑となり、塗料の吸い込みも防止さ
れる。強化シーラーとしては、たとえば、アクリルウレ
タン系、アクリルシリコン系、フッソ系、ウレタン系の
もの等が挙げられる。塗布量は300±100g/m2
が望ましい。強化シーラー層の役割は、基体からのアル
カリ成分の溶出の防止、無機塗料との密着性の確保、基
体の寸法変化による無機塗料への応力の分散等である。
【0007】無機塗料としては、特に限定はされない
が、たとえば、 ケイ酸塩、リン酸塩、シリカゾルやアルカリシリケ
ート等の水溶性シリケート、アルミナゾル等の、架橋に
より硬化するもの、 ソルダーガラス等の溶融物の冷却により硬化するも
の、 アルキルシリケート、アルキルチタネート等の有機
側鎖の消失により硬化するもの、 金属アルコラートを主成分とする、常温ないし低温
加熱によって硬化するもの、 等が挙げられる。塗布量は30〜130g/m2 が望ま
しい。無機塗料の塗布後、遠赤外線加熱等により焼き付
けを行い、塗膜を形成させる。遠赤外線加熱は、たとえ
ば、50〜150℃で5〜6分行えばよい。
【0008】
【作用】基体表面に目止め処理をすることにより、孔や
凹凸のある多孔質基体の表面が平滑になって、無機塗料
を塗布することができる。
【0009】
【実施例】図1はこの発明にかかる多孔質無機質板の実
施例を模式的に表す。図中、1は多孔質無機基体、2は
フィラー層21と強化シーラー層22からなる平滑仕上
げ層、3は無機塗膜である。以下にこの多孔質無機質板
の作り方を説明する。多孔質無機基体の表面に、フィラ
ーを2.5Kg/m2 塗布し、さらに強化シーラーを30
0g/m2 塗布して目止め処理を行う。この上に金属ア
ルコラート系無機塗料を10g/m2 塗布し、100
℃、5分間の遠赤外線加熱により焼き付けを行って、無
機塗膜を形成させる。
【0010】
【発明の効果】この発明によれば、多孔質無機基体の表
面に目止め処理をすることにより、基体表面を平滑にし
ているため、無機塗料による塗装が可能となる。このた
め、耐侯性に優れる無機塗料を塗布することができ、多
孔質無機質板の耐侯性が向上する。
【図面の簡単な説明】
【図1】この発明にかかる多孔質無機質板の実施例を模
式的に表す断面図である。
【符号の説明】
1 多孔質無機基体 2 平滑仕上げ層 21 フィラー層 22 強化シーラー層 3 無機塗膜

Claims (1)

    (57)【特許請求の範囲】
  1. 【請求項1】 基体表面に目止め処理による平滑仕上げ
    がなされ、その上に無機塗料による塗装仕上げがなされ
    おり、 前記目止め処理が、多孔質無機質板表面にフィラー層を
    形成し、その上に強化シーラーを塗装することによりな
    されている 多孔質無機質板。
JP4262272A 1992-09-30 1992-09-30 多孔質無機質板 Expired - Lifetime JP2813514B2 (ja)