JP2023509638A5 - - Google Patents
Info
- Publication number
- JP2023509638A5 JP2023509638A5 JP2022540428A JP2022540428A JP2023509638A5 JP 2023509638 A5 JP2023509638 A5 JP 2023509638A5 JP 2022540428 A JP2022540428 A JP 2022540428A JP 2022540428 A JP2022540428 A JP 2022540428A JP 2023509638 A5 JP2023509638 A5 JP 2023509638A5
- Authority
- JP
- Japan
- Prior art keywords
- aluminum
- based material
- piece
- laser beam
- less
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Applications Claiming Priority (5)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| USPCT/US2019/068996 | 2019-12-30 | ||
| PCT/US2019/068996 WO2020142458A1 (en) | 2018-12-30 | 2019-12-30 | Methods and systems for welding copper and other metals using blue lasers |
| US202063008722P | 2020-04-11 | 2020-04-11 | |
| US63/008,722 | 2020-04-11 | ||
| PCT/US2020/067591 WO2021138510A1 (en) | 2019-12-30 | 2020-12-30 | Methods and systems for reducing hazardous byproduct from welding metals using lasers |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JP2023509638A JP2023509638A (ja) | 2023-03-09 |
| JP2023509638A5 true JP2023509638A5 (https=) | 2023-06-05 |
Family
ID=76687449
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2022540428A Pending JP2023509638A (ja) | 2019-12-30 | 2020-12-30 | レーザーを用いた金属溶接部からの有害な副生成物を低減させる方法およびシステム |
Country Status (6)
| Country | Link |
|---|---|
| EP (1) | EP4084925B1 (https=) |
| JP (1) | JP2023509638A (https=) |
| KR (1) | KR20220116275A (https=) |
| CN (1) | CN115210031A (https=) |
| CA (1) | CA3163159A1 (https=) |
| WO (1) | WO2021138510A1 (https=) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE102020210182B4 (de) * | 2020-08-11 | 2024-09-19 | Continental Autonomous Mobility Germany GmbH | Schweißverfahren, Druckgussformteil und Aktuatorgehäuse |
| IT202200016164A1 (it) * | 2022-07-29 | 2022-10-29 | Nuovo Pignone Tecnologie Srl | Metodo per la produzione di una girante chiusa |
| CN117871354B (zh) * | 2024-01-02 | 2024-07-16 | 中国矿业大学 | 一种基于双目散射图像的粉尘质量浓度及其分布测量装置 |
Family Cites Families (11)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4224499A (en) * | 1978-10-20 | 1980-09-23 | General Electric Company | Laser welding aluminum to copper |
| JP4555160B2 (ja) * | 2005-06-01 | 2010-09-29 | 株式会社神戸製鋼所 | アルミニウム材との異材溶接接合用鋼板および異材接合体 |
| US10562132B2 (en) | 2013-04-29 | 2020-02-18 | Nuburu, Inc. | Applications, methods and systems for materials processing with visible raman laser |
| US10971896B2 (en) | 2013-04-29 | 2021-04-06 | Nuburu, Inc. | Applications, methods and systems for a laser deliver addressable array |
| US11646549B2 (en) | 2014-08-27 | 2023-05-09 | Nuburu, Inc. | Multi kW class blue laser system |
| CN205764438U (zh) * | 2015-02-09 | 2016-12-07 | 司浦爱激光技术英国有限公司 | 激光焊缝和包括激光焊缝的物品 |
| KR20230090371A (ko) * | 2016-04-29 | 2023-06-21 | 누부루 인크. | 반도체 패키징, 자동차 전기 장치, 배터리 및 기타 부품에 대한 가시 레이저 용접 방법 |
| KR102473803B1 (ko) * | 2017-01-31 | 2022-12-02 | 누부루 인크. | 청색 레이저를 사용한 구리 용접 방법 및 시스템 |
| CN206747804U (zh) * | 2017-02-20 | 2017-12-15 | 广东海洋大学 | 一种铜铝异质金属的激光焊接装置 |
| WO2018157159A1 (en) * | 2017-02-27 | 2018-08-30 | Arconic Inc. | Aluminum alloy compositions, products and methods of making the same |
| CN113745973A (zh) | 2017-06-13 | 2021-12-03 | 努布鲁有限公司 | 高密集波长束组合激光系统 |
-
2020
- 2020-12-30 KR KR1020227024966A patent/KR20220116275A/ko active Pending
- 2020-12-30 WO PCT/US2020/067591 patent/WO2021138510A1/en not_active Ceased
- 2020-12-30 CN CN202080097762.1A patent/CN115210031A/zh active Pending
- 2020-12-30 JP JP2022540428A patent/JP2023509638A/ja active Pending
- 2020-12-30 CA CA3163159A patent/CA3163159A1/en active Pending
- 2020-12-30 EP EP20908467.2A patent/EP4084925B1/en active Active
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP3520952B1 (fr) | Dispositif de fabrication de flans soudés comprenant une source laser pour oter par fusion et vaporisation une couche a base aluminium et un dispositif de soudage | |
| Qin et al. | Effect of modified flux on MIG arc brazing-fusion welding of aluminum alloy to steel butt joint | |
| JP2020506808A5 (https=) | ||
| JP5725723B2 (ja) | 高出力レーザビーム溶接及びそのアセンブリ | |
| JP2023509638A5 (https=) | ||
| Kim et al. | Relationship between the weldability and the process parameters for laser-TIG hybrid welding of galvanized steel sheets | |
| JP6719345B2 (ja) | アルミニウム接合体の製造方法 | |
| JP3767375B2 (ja) | 亜鉛系めっき鋼板の重ね溶接方法及び溶接結合薄板 | |
| JP6638529B2 (ja) | Ni基合金系溶接材料を用いたレーザー・アークハイブリッド溶接法による溶接継ぎ手及びその作製方法 | |
| CN112207443B (zh) | 激光电弧复合焊接装置 | |
| JP2011115836A (ja) | 金属メッキ板のレーザー溶接方法 | |
| JP7416999B2 (ja) | レーザ・アークハイブリッド溶接装置 | |
| WO2017099004A1 (ja) | 突合せ溶接方法 | |
| JP2713000B2 (ja) | 制振鋼板のレーザ溶接方法 | |
| JP2009045628A (ja) | 鋼板のレーザ溶接方法 | |
| JPH04138889A (ja) | レーザ加工用ヘッド装置 | |
| JPH07323386A (ja) | レーザ溶接方法 | |
| Alfieri et al. | Porosity evolution in aluminum alloy 2024 bop and butt defocused welding by Yb-YAG disk laser | |
| JP3205449B2 (ja) | レーザー溶接用フィラワイヤ | |
| Miyazaki et al. | Welding techniques for tailored blanks | |
| JP7712245B2 (ja) | 板材、接合体、板材の接合方法及び板材の製造方法 | |
| JP3182603B2 (ja) | アルミニウム合金の接合方法及びアルミニウム合金製真空容器 | |
| JP3229110B2 (ja) | アルミニウム合金の接合方法 | |
| Caiazzo et al. | Bead characterization of disk-laser butt welding of thin AA 2024 sheets | |
| JP7160090B2 (ja) | 金属材料の複合溶接方法および金属材料の突合せ溶接部材 |