JP2014167166A5 JP2014025560A JP2014025560A JP2014167166A5 JP 2014167166 A5 JP2014167166 A5 JP 2014167166A5 JP 2014025560 A JP2014025560 A JP 2014025560A JP 2014025560 A JP2014025560 A JP 2014025560A JP 2014167166 A5 JP2014167166 A5 JP 2014167166A5
Authority
JP
Japan
Prior art keywords
total weight
amount
coating
modified mcraly
formulation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2014025560A
Other languages
English (en)
Japanese (ja)
Other versions
JP5722475B2 (ja
JP2014167166A (ja
Filing date
Publication date
Priority claimed from US13/767,486 external-priority patent/US8697250B1/en
Application filed filed Critical
Publication of JP2014167166A publication Critical patent/JP2014167166A/ja
Publication of JP2014167166A5 publication Critical patent/JP2014167166A5/ja
Application granted granted Critical
Publication of JP5722475B2 publication Critical patent/JP5722475B2/ja
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

JP2014025560A 2013-02-14 2014-02-13 特定の酸化物配合物に対するバリヤーとして作用する高水準のセラミックを装填した改質MCrAlY組成物の選択酸化 Active JP5722475B2 (ja)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
US13/767,486 US8697250B1 (en) 2013-02-14 2013-02-14 Selective oxidation of a modified MCrAlY composition loaded with high levels of ceramic acting as a barrier to specific oxide formations
US13/767,486 2013-02-14

Publications (3)

Publication Number Publication Date
JP2014167166A JP2014167166A (ja) 2014-09-11
JP2014167166A5 true JP2014167166A5 (enExample) 2015-02-19
JP5722475B2 JP5722475B2 (ja) 2015-05-20

Family

ID=50101787

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2014025560A Active JP5722475B2 (ja) 2013-02-14 2014-02-13 特定の酸化物配合物に対するバリヤーとして作用する高水準のセラミックを装填した改質MCrAlY組成物の選択酸化

Country Status (9)

Country Link
US (2) US8697250B1 (enExample)
EP (1) EP2767609B1 (enExample)
JP (1) JP5722475B2 (enExample)
KR (1) KR101553466B1 (enExample)
CN (1) CN103993215B (enExample)
BR (1) BR102014003157B1 (enExample)
CA (1) CA2842993C (enExample)
ES (1) ES2766799T3 (enExample)
MX (1) MX357408B (enExample)

Families Citing this family (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104451655B (zh) * 2013-09-13 2018-02-16 中国科学院金属研究所 抗高温材料用表面合金涂层复合材料、涂层及其制备方法
CN105529172B (zh) * 2014-09-30 2017-11-24 中国科学院宁波材料技术与工程研究所 一种用于钐钴磁体工件表面防护的方法
KR101626913B1 (ko) * 2014-12-03 2016-06-02 창원대학교 산학협력단 우수한 크리프 특성을 위한 텅스텐 함유 내열합금의 열기계적 가공방법 및 그에 의한 합금
CN114318203B (zh) * 2020-09-29 2023-11-17 宝武装备智能科技有限公司 耐高温抗积瘤复合梯度涂层及其制备方法

Family Cites Families (17)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
LU31550A1 (enExample) 1955-03-28
US2972550A (en) 1958-05-28 1961-02-21 Union Carbide Corp Flame plating using detonation reactants
US3864093A (en) 1972-11-17 1975-02-04 Union Carbide Corp High-temperature, wear-resistant coating
US4124737A (en) 1976-12-30 1978-11-07 Union Carbide Corporation High temperature wear resistant coating composition
JPS59153825A (ja) * 1983-02-18 1984-09-01 Nippon Steel Corp 耐ビルドアツプ性の優れたハ−スロ−ル
WO1987002389A2 (en) * 1985-10-18 1987-04-23 Union Carbide Corporation High volume fraction refractory oxide, thermal shock resistant coatings
US4822689A (en) 1985-10-18 1989-04-18 Union Carbide Corporation High volume fraction refractory oxide, thermal shock resistant coatings
US4902539A (en) 1987-10-21 1990-02-20 Union Carbide Corporation Fuel-oxidant mixture for detonation gun flame-plating
JPH03215622A (ja) * 1990-01-17 1991-09-20 Sumitomo Metal Ind Ltd ウォーキングビーム
ATE125577T1 (de) * 1990-10-11 1995-08-15 Praxair Technology Inc Beschichtete ofenrolle und verfahren zu ihrer herstellung.
CN1065570C (zh) * 1994-06-24 2001-05-09 普拉塞尔·S·T·技术有限公司 生产金属铬铝钇基涂层的方法和涂覆以热喷涂层的基体
TW493016B (en) * 1994-06-24 2002-07-01 Praxair Technology Inc A process for producing an oxide dispersed MCrAly-based coating
KR100547263B1 (ko) 1999-11-09 2006-02-01 제이에프이 스틸 가부시키가이샤 내빌드업성에 우수한 용사피복용 서멧분말과 용사피복롤
US7361386B2 (en) * 2002-07-22 2008-04-22 The Regents Of The University Of California Functional coatings for the reduction of oxygen permeation and stress and method of forming the same
US7378132B2 (en) 2004-12-14 2008-05-27 Honeywell International, Inc. Method for applying environmental-resistant MCrAlY coatings on gas turbine components
TW200718805A (en) 2005-11-07 2007-05-16 United Technologies Corp Coating methods and apparatus
US20120128525A1 (en) * 2010-11-24 2012-05-24 Kulkarni Anand A Metallic Bondcoat or Alloy with a High y/y' Transition Temperature and a Component

Similar Documents

Publication Publication Date Title
Pflumm et al. Oxidation protection of γ-TiAl-based alloys–A review
EP1953253B1 (en) Metal alloy compositions and articles comprising the same
EP1980634B1 (en) Metal alloy compositions and articles comprising the same
CN102421928A (zh) 对含2-35重量%Mn的扁钢制品进行热浸镀层的方法和扁钢制品
Chang et al. Study on the thermal erosion, wear and corrosion behaviors of TiAlN/oxynitriding duplex-treated AISI H13 alloy steel
JP2014167166A5 (enExample)
JP4786576B2 (ja) 耐テンパーカラー性に優れたステンレス鋼材およびその製造法
JP5722475B2 (ja) 特定の酸化物配合物に対するバリヤーとして作用する高水準のセラミックを装填した改質MCrAlY組成物の選択酸化
CN105209668A (zh) 改善高锰钢带的可焊性的方法和经涂覆的钢带
US8039116B2 (en) Nb-Si based alloys having an Al-containing coating, articles, and processes
BR112020008112B1 (pt) Substrato de aço revestido, método para a fabricação de um substrato de aço revestido e método para a fabricação de um produto de aço laminado a quente
Matsumoto et al. The effect of pre-oxidation atmosphere on the durability of EB-PVD thermal barrier coatings with CoNiCrAlY bond coats
CN103114267B (zh) 一种钢基体表面氧化铝涂层的制备方法
CA2700899A1 (en) Wear protection coating
Kitaoka et al. Control of polymorphism in Al2O3 scale formed by oxidation of alumina-forming alloys
JP7063996B2 (ja) 被覆鋼基材
JP7162663B2 (ja) 被覆鋼基材
WO2023277063A1 (ja) 炉内構造物の被覆材料および表面被覆方法ならびに炉内構造物
JP5752445B2 (ja) ハースロール
CN113891953A (zh) 防腐蚀的方法
JP4774786B2 (ja) 炉内構造物被覆用溶射被膜およびその形成方法
KR102078700B1 (ko) 고내식성 용융 알루미늄 도금 강판 제조 설비 중 포트롤 및 그 제조방법
JPWO2020245027A5 (enExample)
Promdirek et al. Improvement of slurry aluminide coating on ferritic stainless steel AISI430 for high-temperature oxidation resistance
JPS6260817A (ja) 金属材料の酸化防止加熱方法